Part-66 Module 6 Practice Test

EASA Part-66 Module 6 - Materials and Hardware

Part-66 Module 6 overview

  • 200 practice questions
  • 32 flashcards
  • 9 study guide topics
  • 40 key terms

What you'll study

  • Aircraft Materials - Ferrous11%
  • Aircraft Materials - Non-Ferrous11%
  • Aircraft Materials - Composite and Non-Metallic11%
  • Corrosion11%
  • Fasteners11%
  • Pipes and Unions11%
  • Springs, Bearings and Transmissions11%
  • Control Cables11%
  • Electrical Cables and Connectors12%

Part-66 Module 6 - Materials and Hardware is one of the knowledge modules that make up the aircraft maintenance licence (AML) syllabus under the EU Part-66 framework. It is aimed at trainee and practising certifying staff - typically candidates working toward a B1 (mechanical) or B2 (avionics) licence, either through a Part-147 approved basic training course or through self-study followed by examinations at the competent authority. The module tests the practical materials knowledge a certifying engineer needs on the hangar floor: the properties and identification of ferrous, non-ferrous and composite/non-metallic materials, the recognition and treatment of the various forms of corrosion, and the hardware that holds an aircraft together - fasteners, pipes and unions, springs, bearings, transmissions, control cables, and electrical cables and connectors. Each of those areas is examined at a level of detail closer to trade practice than to pure metallurgy, so questions tend to be about selection, inspection, defect recognition and correct fitment rather than theory. Because the module is broad and largely descriptive, preparation should combine a structured pass through the nine subject areas with plenty of recall practice on terminology, material codes, fastener types and inspection criteria. Candidates should confirm the examination parameters - question count, time allowed and pass mark - with their training organisation or national competent authority before booking, as these are set at national level and are not stated in the sources used for this page.

Common mistakes

Classifying 304 stainless steel as magnetic and hardenable by heat treatment.

Candidates assume every steel is magnetic and can be hardened, so they transfer carbon-steel behaviour onto austenitic stainless.

What to do instead

Learn the family rule: 300-series is austenitic, non-magnetic and hardened only by work hardening; 400-series ferritic/martensitic is magnetic and martensitic grades respond to heat treatment.

Choosing 7075-T6 as the correct material for a welded aircraft structure.

A 'highest strength equals best choice' heuristic overrides knowledge of weldability limits.

What to do instead

Memorise the weldability split: 6061 is the common weldable heat-treatable alloy, while 2024 and especially 7075 are generally not fusion welded; match alloy to joining method, not just strength.

Selecting dye penetrant inspection to find delamination inside a CFRP laminate.

Candidates carry metal NDT habits across to composites without checking whether the defect reaches the surface.

What to do instead

Use methods that see internal structure: tap testing, ultrasonic inspection or radiography for delamination and disbonds; penetrant only reveals surface-breaking defects in non-porous materials.

Stating that the steel member corrodes when aluminium and steel are joined in a wet environment.

Candidates remember that aluminium corrodes easily but do not apply the galvanic series to decide which metal is anodic.

What to do instead

Apply the rule that the less noble (anodic) metal is consumed: aluminium is anodic to steel, so the aluminium side corrodes; quote the series order before choosing the victim.

Selecting a bolt whose threads fall inside the shear plane of the joint.

Candidates size the bolt by overall length instead of by grip length relative to material thickness.

What to do instead

Use grip length equal to the total thickness of the parts being joined, keep threads out of the bearing/shear plane, and allow no more than about three threads exposed beyond the nut.

Identifying 37 degrees as the automotive flare angle and 45 degrees as the aircraft angle.

The two common flare standards are memorised as a pair but swapped under exam pressure.

What to do instead

Anchor it with the fittings: AN/JIC aircraft flares are 37 degrees, SAE automotive flares are 45 degrees, and the two must never be intermixed.

Claiming a compression spring may be stretched to restore or increase its free length.

Candidates treat springs as ductile wire that can be re-formed without consequence.

What to do instead

Recognise that stretching beyond the elastic limit produces permanent set and changes rate and load; reject or replace springs that are overstressed, and check free length and rate rather than reforming them.

Choosing a cylindrical roller bearing to carry a pure axial thrust load.

The simplification that roller bearings carry heavy loads is applied without checking the direction of load.

What to do instead

Match bearing type to load direction: cylindrical rollers are radial-only, while thrust ball, tapered roller or spherical roller bearings are used where axial loads must be carried.

Approving a knot or a U-bolt clamp as a repair for a broken aircraft control cable.

Everyday hardware intuition suggests clamping or knotting is an acceptable field fix.

What to do instead

State that control cables are joined only by properly swaged terminals or splices; knots, cable clamps and soldered joints are prohibited, and inspection looks for broken wires, corrosion and correct tension.

Stating that a larger AWG number indicates a thicker electrical wire.

The gauge scale runs opposite to intuitive size numbering, so candidates invert it.

What to do instead

Remember that increasing AWG number means decreasing conductor cross-section; use the wire gauge table and current rating rather than judging size from the number alone.

Exam requirements can change. Confirm current details with the exam provider.

Part-66 Module 6 practice

200 questions. Each one lists the choices, the correct answer, and an explanation. With JavaScript, this list opens one question at a time. The checker at the top of this page saves progress in this browser when it is available.

  1. Question 1Aircraft Materials - Ferrous

    In plain carbon steel, increasing the carbon content up to about 0.8% generally results in:

    1. Lower hardness but noticeably better weldability
    2. Improved ductility and impact toughness together with lower tensile strength
    3. Higher hardness and tensile strength, lower ductility Correct answer.
    4. No significant change in the mechanical properties

    Explanation

    Carbon is the principal hardening element in plain carbon steel; as the carbon content rises towards the eutectoid composition of about 0.8%, hardness and tensile strength increase. The same rise in carbon restricts slip, so ductility and impact toughness fall. Above roughly 0.8% the steel becomes progressively more brittle without a useful gain in strength.

  2. Question 2Aircraft Materials - Ferrous

    When eutectoid plain carbon steel (about 0.8% carbon) is cooled slowly from the austenitic range, the resulting structure consists mainly of:

    1. Pearlite Correct answer.
    2. Austenite and cementite
    3. Ferrite only
    4. Martensite

    Explanation

    Slow cooling allows carbon to diffuse, so the austenite transforms into pearlite, an alternating lamellar mixture of ferrite and cementite. Ferrite alone would require a very low carbon content, and martensite only forms on rapid quenching. Austenite is not retained at room temperature after slow cooling.

  3. Question 3Aircraft Materials - Ferrous

    Cementite, or iron carbide (Fe3C), in steel is best described as:

    1. Having the same properties as ferrite
    2. A solid solution of carbon in gamma iron
    3. Soft and highly ductile
    4. Hard and brittle Correct answer.

    Explanation

    Cementite is an intermetallic compound of iron and carbon that is very hard and very brittle. It contributes wear resistance but, in large amounts or coarse form, reduces toughness. A solid solution of carbon in gamma iron is austenite, not cementite.

  4. Question 4Aircraft Materials - Ferrous

    After a steel component has been hardened by quenching, tempering is carried out mainly to:

    1. Soften the component completely so that it can be machined
    2. Increase the carbon content of the surface layer
    3. Refine the grain size before the hardening operation
    4. Relieve internal stresses and reduce brittleness Correct answer.

    Explanation

    As-quenched martensite is very hard but brittle and contains high internal stresses. Tempering, a controlled reheating below the critical range, allows some carbon to precipitate and relieves those stresses while retaining useful hardness. The amount of tempering determines the final balance of hardness and toughness.

  5. Question 5Aircraft Materials - Ferrous

    Martensite forms when austenite is quenched rapidly because:

    1. The steel recrystallises directly into fine pearlite colonies
    2. Carbon is trapped in a supersaturated body-centred tetragonal lattice Correct answer.
    3. Carbon diffuses out of solution to form coarse carbide plates at the grain boundaries
    4. Ferrite and cementite separate into alternate lamellae

    Explanation

    Rapid cooling suppresses the diffusion of carbon, so the face-centred cubic austenite transforms by a shear mechanism into a body-centred tetragonal structure supersaturated with carbon. This distorted lattice is what makes martensite hard and brittle. Any process in which carbon can diffuse would give pearlite or other softer products instead.

  6. Question 6Aircraft Materials - Ferrous

    Case carburising is normally applied to:

    1. Low carbon steel in order to give a hard wear-resistant surface Correct answer.
    2. Austenitic stainless steel in order to improve corrosion resistance
    3. High carbon tool steel in order to toughen the core
    4. Grey cast iron in order to reduce machining costs

    Explanation

    Carburising diffuses carbon into the surface of a low carbon steel, which is then quenched so that the enriched surface becomes hard martensite while the unaffected core stays tough. A high carbon steel would not need extra carbon and would be too brittle throughout. The process is a surface treatment and does not change corrosion behaviour appreciably.

  7. Question 7Aircraft Materials - Ferrous

    Compared with carburising, the nitriding process:

    1. Can only be applied to high carbon steels
    2. Produces a deeper case in a much shorter time
    3. Uses a lower temperature and requires no quenching Correct answer.
    4. Requires a rapid water quench immediately after treatment

    Explanation

    Nitriding introduces nitrogen into the surface, usually from ammonia gas, at around 500 °C, which is below the critical range. Because no austenite is formed, no quench is needed and distortion is very small. The case produced is thinner but extremely hard and wear resistant.

  8. Question 8Aircraft Materials - Ferrous

    Which statement about austenitic stainless steels is correct?

    1. They are non-magnetic and not hardened by heat treatment Correct answer.
    2. They are strongly magnetic and can be hardened by quenching
    3. They are hardened mainly by precipitation of carbides
    4. They contain less than 10.5% chromium

    Explanation

    Austenitic stainless steels, of the 18/8 family, keep a face-centred cubic structure at room temperature and are therefore essentially non-magnetic. Because no martensite can form on quenching, they cannot be hardened by heat treatment and are strengthened only by cold working. Their chromium content is well above the 10.5% minimum needed for stainless behaviour.

  9. Question 9Aircraft Materials - Ferrous

    The designation 18/8 stainless steel indicates a content of:

    1. 18% nickel and 8% chromium
    2. 18% chromium and 8% nickel Correct answer.
    3. 18% chromium and 8% carbon
    4. 18% carbon and 8% chromium

    Explanation

    In the traditional 18/8 notation the first figure is the chromium percentage and the second is the nickel percentage. Chromium provides the passive surface film and nickel stabilises the austenitic structure. Such a steel therefore contains about 18% chromium and 8% nickel with a carbon content of only a few hundredths of a percent.

  10. Question 10Aircraft Materials - Ferrous

    Martensitic stainless steels can be hardened by heat treatment because they:

    1. Are fully austenitic at room temperature
    2. Contain nickel as the main alloying element
    3. Depend on nitrogen for their strength
    4. Have a higher carbon content together with 12-18% chromium Correct answer.

    Explanation

    Martensitic grades contain enough carbon, typically 0.1% to about 1%, for austenite to transform to martensite on quenching, while 12-18% chromium gives moderate corrosion resistance. They are magnetic and are used where hardness and wear resistance matter more than corrosion resistance. Nickel-rich grades, by contrast, stay austenitic and cannot be hardened this way.

  11. Question 11Aircraft Materials - Ferrous

    An austenitic stainless steel that has been held in the 450-850 °C range may later suffer intergranular corrosion because:

    1. The passive oxide layer becomes thicker and then cracks
    2. The structure transforms locally into martensite at the grain boundaries
    3. Nickel diffuses to the surface and oxidises rapidly
    4. Chromium carbides precipitate at the grain boundaries Correct answer.

    Explanation

    In this temperature range carbon diffuses to the grain boundaries and precipitates as chromium carbides, which removes chromium from the adjacent metal. The depleted zones then fall below the level needed to maintain a passive film and corrode preferentially. This effect is called sensitisation and is avoided by using low carbon or stabilised grades.

  12. Question 12Aircraft Materials - Ferrous

    In grey cast iron, the carbon is mainly present as:

    1. Spheroidal nodules of graphite
    2. Graphite flakes Correct answer.
    3. Carbon dissolved in solid solution in ferrite
    4. Combined carbon in the form of cementite

    Explanation

    Slow cooling of grey cast iron allows the carbon to separate as graphite flakes, which give the characteristic grey fracture and provide good damping and machinability. White cast iron, by contrast, retains its carbon combined as cementite because it cools too quickly for graphite to form. Nodular graphite is found in spheroidal graphite iron, not in ordinary grey iron.

  13. Question 13Aircraft Materials - Ferrous

    Malleable cast iron is produced by:

    1. Quenching grey cast iron from above its critical temperature
    2. Adding magnesium to the molten iron just before casting
    3. Heat treating white cast iron so that the cementite decomposes Correct answer.
    4. Rolling and forging grey cast iron at high temperature

    Explanation

    Malleable iron is made by casting white iron, in which all the carbon is combined as cementite, and then giving it a long annealing treatment. This breaks the cementite down into temper carbon, giving a ductile material that can be bent without fracturing. Adding magnesium instead produces spheroidal graphite iron, a different material.

  14. Question 14Aircraft Materials - Ferrous

    Which property is typical of wrought iron?

    1. It is used mainly for casting gearbox housings
    2. Very high hardness combined with poor ductility
    3. A carbon content of about 2%
    4. A low carbon content with fibrous slag inclusions Correct answer.

    Explanation

    Wrought iron is a very low carbon ferrous material containing characteristic threads of slag rolled into the metal. These inclusions give it good ductility, toughness and resistance to corrosion, and it can be forged and welded readily. It is not a casting material and does not contain the high carbon levels found in cast iron.

  15. Question 15Aircraft Materials - Ferrous

    In the AISI/SAE designation 4130, the figures '41' indicate:

    1. A chromium-molybdenum steel Correct answer.
    2. A carbon content of 0.41%
    3. A chromium content of 4.1%
    4. A nickel-chromium steel

    Explanation

    In the four-digit system the first two digits identify the alloy type, with 41 denoting a chromium-molybdenum (chrome-moly) steel. The last two digits give the carbon content in hundredths of a percent, so 4130 contains about 0.30% carbon. Such steels are widely used for welded tubular structures such as aircraft engine mounts.

  16. Question 16Aircraft Materials - Ferrous

    Normalising of steel consists of:

    1. Heating above the critical range and cooling in still air Correct answer.
    2. Cold working followed by a low temperature soak
    3. Heating below the critical range and quenching in oil
    4. Heating above the critical range and cooling slowly in the furnace

    Explanation

    Normalising heats the steel above its upper critical temperature to form austenite and then cools it in still air. The moderate cooling rate gives a finer, more uniform grain structure than annealing, with slightly higher strength. Furnace cooling is annealing and produces a softer structure.

  17. Question 17Aircraft Materials - Ferrous

    The main purpose of fully annealing a steel component is to:

    1. Introduce compressive stresses at the surface
    2. Produce a hard martensitic structure throughout
    3. Increase its surface hardness for wear resistance
    4. Soften it and relieve internal stresses Correct answer.

    Explanation

    Full annealing heats the steel above the critical range and cools it very slowly, usually in the furnace, producing a soft, stress-free structure with good machinability. The slow cooling gives coarse pearlite rather than martensite. Hardening treatments require rapid cooling instead.

  18. Question 18Aircraft Materials - Ferrous

    Spheroidising heat treatment is used mainly to:

    1. Increase the corrosion resistance of the surface
    2. Improve the machinability of high carbon steels Correct answer.
    3. Give the steel maximum hardness for cutting tools
    4. Produce a very fine grain size before forging

    Explanation

    Spheroidising holds the steel just below the critical range for a long time so that the lamellar carbide turns into small rounded globules. This globular structure is soft and machines much more readily, particularly in high carbon and tool steels. It is a softening treatment, not a hardening one.

  19. Question 19Aircraft Materials - Ferrous

    The Brinell hardness test uses:

    1. A diamond cone under a 150 kg load
    2. A hardened ball under a heavy load Correct answer.
    3. A swinging pendulum dropped onto the surface
    4. A sharp pyramidal diamond under a light load

    Explanation

    The Brinell test presses a hardened steel or tungsten carbide ball of standard diameter into the surface under a heavy load, typically 500 to 3000 kg. The diameter of the resulting impression is measured and converted to a hardness number. A diamond cone is used in the Rockwell C test and a pyramid in the Vickers test.

  20. Question 20Aircraft Materials - Ferrous

    Decarburisation of the surface of a steel part during heat treatment will:

    1. Reduce surface hardness and fatigue strength Correct answer.
    2. Improve the corrosion resistance of the part
    3. Have no measurable effect on the mechanical properties
    4. Increase surface hardness and wear resistance

    Explanation

    Decarburisation occurs when carbon is lost from the surface by reaction with the surrounding atmosphere at high temperature. The depleted surface layer is softer and weaker, and it lowers fatigue resistance because cracks initiate easily there. It is controlled by using a protective atmosphere or by removing the affected layer afterwards.

  21. Question 21Aircraft Materials - Ferrous

    Stainless steel resists corrosion because chromium:

    1. Prevents any oxygen from reaching the surface
    2. Makes the steel fully austenitic at all temperatures
    3. Forms a thin self-repairing passive oxide film Correct answer.
    4. Raises the carbon content of the surface layer

    Explanation

    Chromium in excess of about 10.5% allows a very thin, adherent chromium-rich oxide film to form on the surface. This passive film is stable and reforms quickly if damaged, isolating the metal from the environment. It is the film, not the bulk metal, that provides the protection.

  22. Question 22Aircraft Materials - Ferrous

    Manganese is added to steel mainly to:

    1. Give the steel a non-magnetic structure
    2. Improve hardenability and act as a deoxidiser Correct answer.
    3. Raise the resistance to seawater corrosion
    4. Increase the carbon content of the melt

    Explanation

    Manganese combines with sulphur to prevent hot shortness and acts as a deoxidiser during melting, and in amounts around 1-2% it also improves hardenability and strength. It is present in almost all steels for these reasons. It does not raise the carbon content or provide corrosion resistance.

  23. Question 23Aircraft Materials - Non-Ferrous

    In an aluminium alloy designation, what does the temper letter 'T6' indicate?

    1. Annealed to its softest possible condition
    2. As fabricated, with no further treatment
    3. Solution heat treated, then artificially aged Correct answer.
    4. Strain hardened, then partially annealed

    Explanation

    The 'T' prefix denotes a temper produced by thermal treatment, and the digit 6 specifically means the metal was solution heat treated and then artificially aged, sometimes after a small amount of cold work. This is the temper normally used for high-strength alloys such as 7075 and 2014. Other prefixes cover entirely different conditions: O for annealed, H for strain hardened and F for as fabricated.

  24. Question 24Aircraft Materials - Non-Ferrous

    What is the purpose of the thin pure aluminium surface layer on Alclad sheet?

    1. To protect the core by sacrificial action Correct answer.
    2. To raise the tensile strength of the sheet
    3. To lower the weight of the finished panel
    4. To allow the sheet to be welded more easily

    Explanation

    The cladding is anodic to the alloy core, so it corrodes preferentially and protects the core from attack, including at cut edges where it is smeared over the exposed core. It also provides a good key for paint. It contributes no strength and slightly increases weight.

  25. Question 25Aircraft Materials - Non-Ferrous

    Which element is the principal alloying addition in aluminium alloy 2024?

    1. Zinc
    2. Silicon
    3. Copper Correct answer.
    4. Magnesium

    Explanation

    2024 is an aluminium-copper alloy, containing roughly 4.4 per cent copper together with smaller amounts of magnesium and manganese, and it is heat treatable to high strength. Its copper content also makes it less corrosion resistant than pure aluminium, which is why it is often supplied clad.

  26. Question 26Aircraft Materials - Non-Ferrous

    Which property of magnesium alloys demands particular care during repair and overhaul?

    1. They are strongly magnetic at high temperature
    2. They have a very high melting point
    3. They are highly resistant to all common chemicals
    4. They are flammable and burn with intense heat Correct answer.

    Explanation

    Magnesium in thin sections, and especially as machining swarf or dust, ignites readily and burns with a very hot, bright flame. Water and carbon dioxide react with burning magnesium, so special dry powders are used to extinguish it. Repair areas are also kept free of contamination from other metals to limit galvanic corrosion.

  27. Question 27Aircraft Materials - Non-Ferrous

    The very high strength of aluminium alloy 7075-T6 derives mainly from the presence of:

    1. Zinc Correct answer.
    2. Copper
    3. Manganese
    4. Titanium

    Explanation

    7075 belongs to the Al-Zn-Mg-Cu family, in which zinc is the dominant addition and provides the greatest response to precipitation hardening. It is one of the strongest aluminium alloys used in aircraft structures but has poor corrosion resistance unless protected.

  28. Question 28Aircraft Materials - Non-Ferrous

    Solution heat treatment of a wrought aluminium alloy such as 2024 is normally carried out at approximately:

    1. 650 °C
    2. 350 °C
    3. 500 °C Correct answer.
    4. 250 °C

    Explanation

    The alloying elements must be taken into solid solution, which for 2024 requires roughly 495 to 505 °C, close to but safely below the temperature at which the grain-boundary eutectic would melt. Temperature control is critical because overheating causes incipient melting and irreparable damage. Quenching follows immediately after soaking.

  29. Question 29Aircraft Materials - Non-Ferrous

    Which of these aluminium alloys normally needs artificial ageing, rather than natural ageing, to reach full strength?

    1. 7075 aluminium-zinc-magnesium-copper alloy Correct answer.
    2. 1050A commercially pure aluminium
    3. 3003 aluminium-manganese alloy
    4. 5052 aluminium-magnesium alloy

    Explanation

    7075 does not harden sufficiently at room temperature and must be given a controlled furnace ageing treatment at elevated temperature to precipitate the strengthening phases. Alloys such as 2024 harden largely by natural ageing at room temperature over several days. Alloys of the 1xxx, 3xxx and 5xxx series are not heat treatable at all and gain strength only by cold work.

  30. Question 30Aircraft Materials - Non-Ferrous

    The oxide film produced on aluminium by sulphuric acid anodising is best described as:

    1. Metallic and soluble in water
    2. Electrically conductive and soft
    3. Porous and an electrical insulator Correct answer.
    4. Magnetic and used for crack detection

    Explanation

    Anodising grows a hard oxide layer that is porous at the surface, so it can be dyed and then sealed, and it provides an excellent paint base. Because it is a ceramic oxide it is an electrical insulator, which is why anodised parts need special treatment where electrical bonding is required.

  31. Question 31Aircraft Materials - Non-Ferrous

    Rivets marked 'AD' (2117-T4) can be driven straight from the stores because:

    1. They must be solution treated just before driving
    2. They must be heated to a red heat before driving
    3. They must be refrigerated until they are driven
    4. They need no further heat treatment before driving Correct answer.

    Explanation

    2117 is a low-copper alloy supplied already solution treated and naturally aged, soft enough to be upset cold yet strong enough in service, so no further treatment is needed. This makes it the standard 'field rivet' for general structural repair. Rivets that must be kept in the quenched condition are stored in a refrigerator instead.

  32. Question 32Aircraft Materials - Non-Ferrous

    Titanium alloys are extensively used in aero-engine compressors because they:

    1. Combine high strength with good heat resistance Correct answer.
    2. Are the cheapest of the structural metals
    3. Have the highest thermal conductivity of any metal
    4. Can be easily soft soldered to aluminium

    Explanation

    Titanium offers an excellent strength-to-weight ratio and retains useful strength at temperatures where aluminium would soften, together with good resistance to corrosion and oxidation. That combination makes it ideal for compressor blades and discs and for hot airframe areas near engines. It is, however, expensive and difficult to machine.

  33. Question 33Aircraft Materials - Non-Ferrous

    Monel is an alloy of:

    1. Nickel and copper Correct answer.
    2. Copper and tin
    3. Aluminium and silicon
    4. Copper and zinc

    Explanation

    Monel contains roughly two-thirds nickel with the balance mainly copper, giving very good resistance to corrosion and to moderately high temperatures. It is used for firewalls, exhaust components and marine fittings. It is considerably stronger and harder than the copper alloys it is often compared with.

  34. Question 34Aircraft Materials - Non-Ferrous

    Brass is an alloy of copper with:

    1. Zinc Correct answer.
    2. Tin
    3. Aluminium
    4. Nickel

    Explanation

    Brass is copper alloyed principally with zinc; varying the zinc content changes colour, strength and ductility. It is used for fittings, bushes and pipework where good corrosion resistance and easy machining are needed. Adding further elements such as aluminium or tin produces the special brasses.

  35. Question 35Aircraft Materials - Non-Ferrous

    Bronze is traditionally an alloy of copper with:

    1. Lead
    2. Magnesium
    3. Tin Correct answer.
    4. Zinc

    Explanation

    The classic bronze is copper alloyed with tin, producing a hard bearing material with good corrosion resistance. Modern bronzes may use aluminium, silicon or beryllium instead of tin to obtain particular properties such as higher strength or non-sparking behaviour.

  36. Question 36Aircraft Materials - Non-Ferrous

    Compared with aluminium alloys, magnesium alloys have:

    1. An identical density but better weldability
    2. A higher melting point and better ductility
    3. A higher density but lower strength
    4. A lower density but poorer corrosion resistance Correct answer.

    Explanation

    Magnesium has a density of about 1.74 g/cm³ against 2.7 g/cm³ for aluminium, making it the lightest structural metal in common aircraft use. Its drawback is chemical activity: it corrodes readily and needs thorough surface protection and careful isolation from other metals.

  37. Question 37Aircraft Materials - Non-Ferrous

    Intergranular corrosion in a 2024 component is most likely to be caused by:

    1. An anodic film that is thinner than specified
    2. Mechanical polishing of the external surface
    3. Long exposure to ultraviolet light in service
    4. Improper heat treatment at the grain boundaries Correct answer.

    Explanation

    Incorrect solution treatment or quenching can leave a continuous network of anodic precipitate along the grain boundaries, which then corrodes preferentially and eats the metal away along narrow paths. The correct heat treatment keeps the precipitate finely distributed within the grains instead. Cladding and good surface protection further reduce the risk.

  38. Question 38Aircraft Materials - Non-Ferrous

    Exfoliation corrosion of aluminium alloy plate is characterised by:

    1. Small pits of uniform depth over the whole surface
    2. A white powder deposit on the upper surfaces only
    3. Cracking that follows the direction of applied stress
    4. Flaking of the metal in layers parallel to the surface Correct answer.

    Explanation

    Exfoliation follows the elongated grain structure of rolled or extruded material, so the corrosion products lift successive layers and the metal appears to flake or swell. It is a severe form of intergranular attack and causes a significant loss of section thickness. It is often found at edges, fastener holes and faying surfaces.

  39. Question 39Aircraft Materials - Non-Ferrous

    The cladding on Alclad sheet consists of:

    1. A low-alloy or pure aluminium layer bonded to the core Correct answer.
    2. An electroplated cadmium layer applied after rolling
    3. A paint film applied at the rolling mill
    4. A sprayed zinc coating applied after forming

    Explanation

    Alclad is produced by roll-bonding a thin layer of commercially pure aluminium or a low-alloy aluminium onto one or both faces of the alloy core during manufacture. The layer is metallurgically bonded, not applied later, and it protects the core galvanically. Care is needed in service so that deep scratches do not expose the core.

  40. Question 40Aircraft Materials - Non-Ferrous

    Why must a solution-treated aluminium alloy be quenched rapidly?

    1. To increase the grain size of the material
    2. To keep the alloying elements in supersaturated solution Correct answer.
    3. To allow coarse particles of alloying elements to form
    4. To relieve the internal stresses from rolling

    Explanation

    Rapid cooling suppresses the precipitation of alloying elements, so they remain trapped in a supersaturated solid solution at room temperature. That unstable condition is what allows the subsequent ageing treatment to produce fine, uniformly distributed precipitates and hence high strength. Slow cooling would instead produce coarse particles and a weaker, corrosion-prone structure.

  41. Question 41Aircraft Materials - Non-Ferrous

    Compared with conventional aluminium alloys, aluminium-lithium alloys offer:

    1. Better electrical conductivity and lower cost
    2. Lower density and higher stiffness Correct answer.
    3. Improved corrosion resistance and easier welding
    4. Higher density and improved fatigue strength

    Explanation

    Lithium is the lightest metallic element, so each per cent added reduces the density of aluminium appreciably while also raising the elastic modulus. This makes Al-Li alloys attractive for weight-critical structure. Their disadvantages include higher cost and greater sensitivity to damage and to certain joining processes.

  42. Question 42Aircraft Materials - Non-Ferrous

    Which non-ferrous metal is most widely used for aircraft electrical cables?

    1. Copper Correct answer.
    2. Titanium
    3. Magnesium
    4. Aluminium

    Explanation

    Copper combines low electrical resistance with good ductility and reliable crimped terminations, which is why it is the standard conductor material. Aluminium is lighter but has higher resistance and poorer termination behaviour and is used mainly for large power feeders where weight saving justifies it.

  43. Question 43Aircraft Materials - Non-Ferrous

    Nickel-based superalloys such as the Nimonic series are selected for turbine blades because they:

    1. Retain strength at high temperature and resist creep Correct answer.
    2. Have a very high coefficient of thermal expansion
    3. Have the lowest density of the heat-resistant metals
    4. Are easily formed cold into complex shapes

    Explanation

    Nickel superalloys keep useful strength and creep resistance at temperatures where aluminium and even steel would fail, which is essential in the turbine section. They are usually vacuum cast or machined because they are difficult to form. Their relatively low, controlled thermal expansion is a further advantage in close-tolerance assemblies.

  44. Question 44Aircraft Materials - Non-Ferrous

    In the alloy Ti-6Al-4V, the role of vanadium is to:

    1. Act only as a grain refiner in the melt
    2. Improve machinability by forming graphite
    3. Stabilise the beta phase and aid heat treatment Correct answer.
    4. Raise the density to that of steel

    Explanation

    Aluminium is an alpha-phase stabiliser while vanadium stabilises the beta phase, so the two together give a balanced alpha-beta alloy that responds well to heat treatment and has good strength. Ti-6Al-4V is the most widely used titanium alloy in airframes and engines. Its density remains about 4.4 g/cm³, well below that of steel.

  45. Question 45Aircraft Materials - Composite and Non-Metallic

    Which statement best defines a structural composite material as used in aircraft construction?

    1. A metal alloy containing more than one element
    2. Two or more distinct materials combined with a recognisable interface Correct answer.
    3. A single material with a homogeneous internal structure
    4. A plastic that has been given a thin metallic coating

    Explanation

    A composite consists of two or more distinct constituents, normally a reinforcement such as fibres and a matrix such as resin, which remain separately identifiable at their interface. The combination produces properties that neither constituent could provide alone.

  46. Question 46Aircraft Materials - Composite and Non-Metallic

    Why can a cured thermosetting resin not be softened and re-formed by reheating?

    1. Its polymer chains are permanently cross-linked Correct answer.
    2. Its fibres prevent any movement of the resin
    3. It contains no polymer chains at all
    4. Its chains are held only by weak secondary forces

    Explanation

    Thermosetting resins cure by a chemical reaction that builds a three-dimensional network of covalent cross-links between the polymer chains. Once formed, this network cannot be broken by heat, so the material chars or degrades rather than softening.

  47. Question 47Aircraft Materials - Composite and Non-Metallic

    Which property is characteristic of a thermoplastic matrix composite?

    1. It needs a hardener added before use
    2. It cures by an irreversible chemical reaction
    3. It softens on heating and hardens again on cooling Correct answer.
    4. It cannot be re-formed after shaping

    Explanation

    Thermoplastic polymers are not cross-linked, so raising the temperature allows the chains to move and the material to soften; cooling restores rigidity. The process can be repeated, which allows re-forming and welding.

  48. Question 48Aircraft Materials - Composite and Non-Metallic

    Which type of glass fibre is the general-purpose reinforcement most widely used in aircraft composite laminates?

    1. E-glass, used for general structural and electrical-grade laminates Correct answer.
    2. S-glass, used where cost is secondary to strength
    3. C-glass, used mainly for chemical resistance
    4. A-glass, used where alkali resistance is required

    Explanation

    E-glass is the standard general-purpose grade, combining adequate strength and stiffness with moderate cost and good electrical insulation properties. The other grades are selected for specific characteristics and are produced in much smaller quantities.

  49. Question 49Aircraft Materials - Composite and Non-Metallic

    What property does aramid fibre reinforcement give to a composite?

    1. High stiffness combined with high density
    2. Very high compressive strength
    3. High tensile strength with good impact resistance Correct answer.
    4. Very high electrical conductivity

    Explanation

    Aramid fibres have high specific tensile strength and excellent energy absorption, which is why they are used for impact-prone and ballistic-resistant parts. They are notably weak in compression and are electrically insulating.

  50. Question 50Aircraft Materials - Composite and Non-Metallic

    Why must carbon fibre composite be electrically isolated from aluminium structure?

    1. Aluminium expands more than carbon fibre when heated
    2. Carbon fibre melts at a lower temperature than aluminium
    3. Carbon and aluminium form a galvanic cell when wet Correct answer.
    4. Carbon fibre releases corrosive acids when wetted

    Explanation

    Carbon is cathodic relative to aluminium, so when moisture provides an electrolyte path the aluminium becomes the anode and corrodes rapidly. Isolation with sealant, glass cloth or protective coatings prevents the couple from forming.

  51. Question 51Aircraft Materials - Composite and Non-Metallic

    In a fibre-reinforced composite, what is the primary role of the matrix?

    1. To carry all the tensile load along the fibre direction
    2. To bind the fibres together and transfer load between them Correct answer.
    3. To act as a release film during the curing cycle
    4. To provide the highest stiffness obtainable in the laminate

    Explanation

    The matrix holds the fibres in their designed positions, protects them from abrasion and environment, and transfers load from fibre to fibre through shear. The fibres themselves provide the main strength and stiffness.

  52. Question 52Aircraft Materials - Composite and Non-Metallic

    Within practical design limits, increasing the fibre volume fraction of a laminate generally does what?

    1. It lowers the strength but raises the toughness
    2. It raises strength and stiffness along the fibre direction Correct answer.
    3. It raises the elongation to failure of the laminate
    4. It removes the need for a controlled cure cycle

    Explanation

    Because the fibres are the load-bearing constituent, a higher proportion of fibre in the same volume increases both the strength and the stiffness in the fibre direction. There is a practical limit, since too little resin leaves voids and dry areas.

  53. Question 53Aircraft Materials - Composite and Non-Metallic

    Uncured pre-preg is normally kept in a freezer because low temperature does what?

    1. It increases the tackiness of the resin
    2. It stops the backing film from sticking
    3. It removes moisture from the fibres
    4. It slows the resin's advance towards cure Correct answer.

    Explanation

    Pre-preg resin is already mixed with its curing agent and slowly reacts at room temperature. Cold storage suppresses that reaction so the material stays within its specified handling and out-time limits.

  54. Question 54Aircraft Materials - Composite and Non-Metallic

    In a sandwich panel, what is the main function of the honeycomb core?

    1. To carry the bending tensile loads in the panel
    2. To protect the facing skins from lightning strikes
    3. To provide the smooth outer aerodynamic surface
    4. To separate the faces and carry shear between them Correct answer.

    Explanation

    The core holds the two facings apart, which gives the panel its bending stiffness, and it transmits shear between the facings. The facings carry the bending tensile and compressive stresses.

  55. Question 55Aircraft Materials - Composite and Non-Metallic

    Why is the hot/wet condition important when assessing composite aircraft structure?

    1. Moisture raises conductivity of carbon fibres
    2. Water freezes in the fibres and splits them
    3. Absorbed moisture plus heat lowers resin strength Correct answer.
    4. Water dissolves fibre sizing and removes the fibres

    Explanation

    Resins absorb moisture from the atmosphere, and at elevated temperature this plasticises the matrix and lowers its glass transition temperature. Properties that depend on the resin, such as compression and interlaminar shear strength, are therefore reduced.

  56. Question 56Aircraft Materials - Composite and Non-Metallic

    Which feature protects a carbon fibre composite wing skin against a lightning strike?

    1. A bonded metallic mesh in the outer plies Correct answer.
    2. An extra glass ply inside the core
    3. Aluminium rivets along the trailing edge
    4. A coat of polyurethane paint on the surface

    Explanation

    A conductive mesh or expanded foil is bonded into the outermost plies so that strike current spreads over the surface and is conducted away instead of vaporising the resin. The paint alone cannot carry the current.

  57. Question 57Aircraft Materials - Composite and Non-Metallic

    When drilling a carbon fibre laminate, which practice helps to prevent delamination at the exit face?

    1. Supporting the exit face and using a low feed rate Correct answer.
    2. Using a blunt drill so fibres are pushed aside
    3. Drilling dry without any dust extraction
    4. Increasing feed rate and speed to the maximum

    Explanation

    Delamination occurs when the drill pushes unsupported plies away from the laminate as it breaks through. A backing plate supports the exit face, and a low feed with a sharp carbide drill limits the push-out force.

  58. Question 58Aircraft Materials - Composite and Non-Metallic

    Which method is most suitable for detecting delamination between plies in a composite panel?

    1. A rebound hardness test on the skin
    2. A dye penetrant test on the painted skin
    3. Magnetic particle inspection of the surface
    4. An ultrasonic scan through the thickness Correct answer.

    Explanation

    Ultrasonic inspection sends sound through the laminate and detects echoes from internal interfaces, so voids and disbonds between plies show up clearly. It is the standard method for internal defects in composites.

  59. Question 59Aircraft Materials - Composite and Non-Metallic

    Why are individual plies laid at different orientations in a laminate?

    1. To make release from the mould easier
    2. To reduce the total weight of the finished part
    3. To allow the part to be cured at a lower temperature
    4. To give the laminate strength in more than one direction Correct answer.

    Explanation

    A unidirectional ply is strong along the fibres but weak across them, so plies are stacked at angles such as 0, 45 and 90 degrees. The resulting laminate carries load in several directions and balances the in-plane stiffness.

  60. Question 60Aircraft Materials - Composite and Non-Metallic

    Which cleaning method is acceptable for an acrylic aircraft window?

    1. Scrubbing with a dry nylon brush
    2. Polishing with an abrasive paste until dry
    3. Washing with mild soap and water, then rinsing Correct answer.
    4. Wiping with MEK to remove grease and paint

    Explanation

    Acrylic softens and crazes when attacked by solvents, so only mild soap solution and plenty of water should be used, followed by thorough rinsing and gentle drying. Solvents and dry abrasion both damage the surface.

  61. Question 61Aircraft Materials - Composite and Non-Metallic

    Which material is typically used as a fuel tank sealant on aircraft structure?

    1. Two-part polysulphide compound Correct answer.
    2. Silicone rubber gasket sheet
    3. Acrylic adhesive film
    4. Epoxy laminating resin

    Explanation

    Polysulphide sealants cure to a flexible rubber that adheres well to metal and composite and resists jet fuel, which is why they are specified for integral fuel tank sealing. They are mixed in the specified ratio and applied within their pot life.

  62. Question 62Aircraft Materials - Composite and Non-Metallic

    What happens if extra hardener beyond the specified ratio is added to a two-part epoxy?

    1. The heat resistance of the finished part improves
    2. Unreacted hardener remains and degrades the cured resin Correct answer.
    3. The resin will not cure at all
    4. The cure speeds up without changing the cured resin

    Explanation

    The mixing ratio is stoichiometric, so each hardener molecule must find a resin molecule to react with. Excess hardener cannot be consumed and stays in the cured material as a plasticising or corrosive residue, lowering strength and heat resistance.

  63. Question 63Aircraft Materials - Composite and Non-Metallic

    Why is aramid fibre seldom used as the main load-bearing ply in compression-critical laminates?

    1. It cannot be bonded to epoxy resin systems
    2. It is much weaker in compression than in tension Correct answer.
    3. It has very low resistance to impact damage
    4. It absorbs water and swells more than other fibres

    Explanation

    Aramid filaments are anisotropic and tend to fibrillate and buckle under compressive load, so compressive strength may be only a fraction of the tensile value. Carbon fibre is normally chosen where compressive loading dominates.

  64. Question 64Aircraft Materials - Composite and Non-Metallic

    Why does barely visible impact damage present a particular concern in carbon fibre laminates?

    1. The resin in the impact area continues to cure and becomes brittle
    2. The damaged region always loses its electrical bonding to the structure
    3. The fibres melt locally and leave a soft area that can be felt
    4. Internal delamination may reduce strength with little visible damage Correct answer.

    Explanation

    Low-energy impacts can separate plies internally while the outer skin springs back and looks almost undamaged. The resulting loss of stiffness and strength is not obvious from a visual walk-round, so scheduled inspections use tap testing or ultrasonics.

  65. Question 65Aircraft Materials - Composite and Non-Metallic

    What is the main purpose of vacuum bagging during the cure of a composite lay-up?

    1. To compact the plies and remove trapped air Correct answer.
    2. To cool the laminate quickly after the exotherm
    3. To draw resin out until the laminate is dry
    4. To align the fibres with the vacuum direction

    Explanation

    The bag applies uniform atmospheric pressure over the lay-up, consolidating the plies, seating them against the mould and extracting air and volatiles through the bleeder. This reduces voids and controls the fibre volume fraction.

  66. Question 66Aircraft Materials - Composite and Non-Metallic

    Why can residual stresses build up within a laminate during and after curing?

    1. The vacuum bag compresses the plies unevenly
    2. Trapped air expands as the laminate cools
    3. Resin shrinks on cure and contracts more than the fibres Correct answer.
    4. The fibres dissolve partly in the resin when hot

    Explanation

    The resin cross-links with a chemical shrinkage and also has a much larger coefficient of thermal expansion than the fibres. As the laminate cools from cure temperature the fibres restrain the resin, leaving locked-in stresses that can cause warping or matrix cracking.

  67. Question 67Corrosion

    Which combination of conditions is necessary for galvanic corrosion to occur?

    1. Two dissimilar metals in electrical contact bridged by an electrolyte Correct answer.
    2. Two similar metals joined together and fully sealed from any moisture
    3. A metal under sustained tensile load in a completely inert atmosphere
    4. A single metal exposed to dry air at elevated temperature for a long period

    Explanation

    Galvanic corrosion is an electrochemical process that needs an anode, a cathode (supplied by two dissimilar metals), an electrical path between them and an electrolyte to carry ions. Removing any one of these four elements stops the cell from working.

  68. Question 68Corrosion

    When two different metals are joined and wetted by an electrolyte, which metal is attacked?

    1. The more noble metal, because it attracts electrons from the other
    2. The more active metal, which becomes the anode Correct answer.
    3. The harder of the two metals, regardless of its position in the series
    4. Both metals at exactly the same rate at all times

    Explanation

    The metal higher in the galvanic series (more negative potential) becomes the anode and loses metal ions into the electrolyte, while the more noble metal becomes the cathode and is protected. The potential difference between the two drives the current.

  69. Question 69Corrosion

    What does an anodizing treatment produce on an aluminium alloy surface?

    1. A zinc layer applied by electroplating
    2. A thin adherent oxide film that protects the metal Correct answer.
    3. A soft wax film renewed at each annual inspection
    4. A cadmium layer acting as a sacrificial anode

    Explanation

    Anodizing makes the part the anode in an electrolytic bath so that the natural oxide is thickened into a hard, adherent and electrically resistive film. The film also provides a good key for paint and primer.

  70. Question 70Corrosion

    Why are aircraft washed regularly with fresh water, particularly after flying at low level over the sea?

    1. To keep the paint glossy and so reduce aerodynamic drag
    2. To remove static electricity from the airframe skin
    3. To remove salt deposits that promote corrosion Correct answer.
    4. To cool the structure after high-speed flight

    Explanation

    Salt is hygroscopic and, once deposited, holds moisture on the surface and forms a strong electrolyte that breaks down protective films. Regular rinsing with fresh water removes the salt before significant attack can start.

  71. Question 71Corrosion

    Stress corrosion cracking requires which combination of conditions?

    1. A single overload applied once to a part free from any corrosion
    2. A sustained tensile stress and a specific corrosive environment Correct answer.
    3. Compressive stress only, combined with a strong alkaline cleaner
    4. A cyclic load applied in dry, clean air at room temperature

    Explanation

    Stress corrosion cracking is a time-dependent failure that needs both a tensile stress, whether applied or residual, and an environment to which that particular alloy is susceptible. Either factor alone is usually harmless, but together they allow fine cracks to propagate.

  72. Question 72Corrosion

    Why must mercury and mercury compounds be kept away from aluminium structures?

    1. They make the aluminium strongly magnetic
    2. They amalgamate the metal and break down its oxide film Correct answer.
    3. They weaken nearby steel fittings by embrittlement
    4. They soften the surrounding paint and primer film

    Explanation

    Mercury amalgamates aluminium and destroys the protective oxide layer, so attack can spread rapidly and penetrate the structure within hours. Strict tool control and spill procedures are used to prevent any contact.

  73. Question 73Corrosion

    Pitting corrosion is best described as:

    1. Localised attack that forms small deep cavities in the surface Correct answer.
    2. A general thinning of the metal along the grain boundaries
    3. Uniform metal loss spread evenly over the whole surface
    4. Swelling of the metal caused by trapped corrosion products

    Explanation

    Pitting begins where the passive film breaks down locally, typically under chloride deposits, and produces narrow cavities that can perforate a skin while total metal loss remains small. It is therefore easily missed during a general visual check.

  74. Question 74Corrosion

    Filiform corrosion is normally found:

    1. Under organic coatings on aluminium as thread-like filaments Correct answer.
    2. On bare steel exposed to continuous immersion in sea water
    3. Along the grain boundaries of forged steel landing gear parts
    4. Inside fuel tanks where water has collected at the bottom

    Explanation

    Filiform attack develops beneath paint films in warm, humid conditions and tracks across the surface as fine filaments following the coating. The metal loss is superficial but the coating is undermined and its protection is lost.

  75. Question 75Corrosion

    Exfoliation corrosion typically appears as:

    1. Dark staining on stainless steel that has been welded
    2. Chalky white deposits around steel rivets
    3. A fine grey powder on the surface of a magnesium casting
    4. Layered flaking and lifting of the metal surface along grain boundaries Correct answer.

    Explanation

    Exfoliation is a form of intergranular attack in wrought products with elongated grains; the corrosion products are bulkier than the metal they replace and force successive layers apart. It appears as flaking, blistering or a laminated edge on sheet and extrusions.

  76. Question 76Corrosion

    Crevice corrosion is most likely to start where:

    1. Stagnant electrolyte is trapped in a narrow gap between parts Correct answer.
    2. A component is stored in dry air at constant temperature
    3. A part is fully immersed in flowing, well-aerated water
    4. Two dissimilar metals are kept apart by an insulating layer

    Explanation

    Inside a narrow gap oxygen cannot be replenished, so the shielded area becomes anodic to the surrounding well-aerated surface and is attacked. Gasket faces, lap joints and areas under dirt deposits are typical sites.

  77. Question 77Corrosion

    Fretting corrosion is caused by:

    1. Continuous immersion of two metals in sea water
    2. High temperature oxidation of bare steel
    3. Small oscillating movement between two surfaces in contact Correct answer.
    4. A direct current leaking through a bonded joint

    Explanation

    Fretting occurs at clamped joints subject to vibration, where tiny relative movements repeatedly break the oxide and expose fresh metal that then oxidises. The result is dark debris between the faces and often the early initiation of fatigue cracks.

  78. Question 78Corrosion

    How does Alclad sheet protect the aluminium alloy core?

    1. Zinc anodes are embedded in the sheet during manufacture
    2. A paint film is baked on at the rolling mill
    3. Pure aluminium is rolled onto each face as a cladding Correct answer.
    4. The core is sealed inside a stainless steel envelope

    Explanation

    The cladding is commercially pure aluminium, which is anodic to the alloy core, so it corrodes preferentially and also acts as a barrier. Even where the cladding is scratched, the exposed core is protected galvanically by the surrounding pure metal.

  79. Question 79Corrosion

    A zinc block bolted in contact with a steel structure acts as:

    1. A cathode, so that the zinc is protected from attack
    2. A sacrificial anode, which corrodes in place of the steel Correct answer.
    3. A catalyst that slows down the formation of rust
    4. An insulator, which stops any current flowing

    Explanation

    Zinc is more active than steel, so in the galvanic couple it becomes the anode and is consumed while the steel is cathodically protected. The block is renewed periodically before it is completely used up.

  80. Question 80Corrosion

    The corrosion resistance of stainless steel depends on:

    1. Regular application of a sacrificial anti-corrosion oil
    2. Its naturally low chromium content and high carbon content
    3. A thin chromium oxide film that forms on the surface Correct answer.
    4. A thick layer of zinc applied during manufacture

    Explanation

    Chromium in the alloy oxidises to form a thin, self-healing passive layer that separates the metal from the environment. If this film is destroyed and cannot re-form, for example in stagnant chloride conditions, the steel becomes susceptible to attack.

  81. Question 81Corrosion

    After a lead-acid battery electrolyte spill on an aluminium alloy structure, the area should be:

    1. Neutralised with baking soda solution and flushed with water Correct answer.
    2. Flushed with a strong caustic soda solution
    3. Wiped with an oily rag and left to dry in the sun
    4. Covered with a fresh coat of primer without cleaning

    Explanation

    Acid residues must first be neutralised with a mild alkali such as sodium bicarbonate and then removed with plenty of clean water. Any acid left in joints continues to attack the metal and the protective coatings.

  82. Question 82Corrosion

    Why are strong alkaline paint strippers unsuitable for aluminium alloy parts?

    1. They leave a magnetic deposit on the alloy surface
    2. They have no effect on paint and only damage steel
    3. Alkalis attack aluminium rapidly and dissolve the metal Correct answer.
    4. They evaporate too quickly to soften the paint film

    Explanation

    Aluminium oxide is amphoteric, so it is attacked by both strong acids and strong alkalis. An alkaline stripper can pit or dissolve the skin, so only strippers approved for aluminium are used.

  83. Question 83Corrosion

    What is the main purpose of applying a corrosion preventive compound to faying surfaces during assembly?

    1. To conduct electrical current between the joined parts
    2. To lubricate the bolts so that they can be torqued easily
    3. To act as a thread locking device on the fasteners
    4. To exclude moisture and oxygen from the joint interface Correct answer.

    Explanation

    Faying surfaces form tight, poorly ventilated joints where moisture can be trapped and crevice or galvanic attack can begin. A compound film keeps the electrolyte out of the interface and so preserves the protection of the mating surfaces.

  84. Question 84Corrosion

    When corrosion is removed by blending, the depth of metal removed should normally not exceed:

    1. The full thickness once the area is repainted
    2. Any depth, provided the surface is left smooth
    3. 10% of the thickness, unless the manual allows more Correct answer.
    4. 50% of the original material thickness

    Explanation

    Blending must stay within the limits published in the structural repair manual because removing metal reduces the load-carrying capacity of the part. The blended area must also be left smooth and be re-protected afterwards.

  85. Question 85Corrosion

    A small stainless steel bracket is bolted directly to a large aluminium alloy panel with no isolation. Which outcome is most likely?

    1. The aluminium will be severely attacked near the bracket Correct answer.
    2. The stainless steel will corrode rapidly because it is the smaller part
    3. Corrosion will be spread evenly across the aluminium panel
    4. Neither metal will corrode because both are passive

    Explanation

    Aluminium is anodic to stainless steel, so it becomes the anode of the couple. A small anode feeding a large cathode gives a high current density at the anode, which concentrates deep localised attack in the aluminium immediately around the fastener.

  86. Question 86Corrosion

    Austenitic stainless steel slowly cooled through the 450-850 °C range may later fail by intergranular corrosion because:

    1. The passive film grows too thick and spalls off
    2. Chromium carbides precipitate at the grain boundaries Correct answer.
    3. Copper diffuses to the boundaries and forms a couple
    4. The steel absorbs hydrogen and becomes brittle

    Explanation

    Chromium carbide precipitation removes chromium from the metal immediately adjacent to the grain boundaries, leaving narrow chromium-depleted zones that cannot re-passivate. These zones then corrode preferentially, a condition known as sensitisation.

  87. Question 87Corrosion

    Why are high-strength steel parts baked soon after cadmium plating or acid pickling?

    1. To drive out absorbed hydrogen that causes brittleness Correct answer.
    2. To harden the surface by a controlled diffusion process
    3. To relieve grinding stresses left by the finishing operation
    4. To melt the cadmium so that it fills surface cracks

    Explanation

    Acid pickling and electroplating generate atomic hydrogen that diffuses into the steel and can cause delayed brittle fracture in high-strength alloys. A controlled low temperature bake removes the hydrogen before it can do harm.

  88. Question 88Corrosion

    A component is fatigue tested in a corrosive environment. Compared with dry air, what is expected?

    1. Cracks start earlier and the fatigue limit disappears Correct answer.
    2. The fatigue life is unchanged because corrosion and fatigue act separately
    3. Cracks grow more slowly because the crack tip is blunted by corrosion
    4. The fatigue life increases because the surface is work hardened

    Explanation

    Corrosion pits act as stress raisers and the environment accelerates crack growth at the tip, so many alloys lose their endurance limit and life is reduced. Surface protection is therefore a fatigue-life issue, not only a cosmetic one.

  89. Question 89Fasteners

    On a screw thread, the term 'pitch' is defined as the:

    1. distance a nut moves along the bolt in one complete turn
    2. distance between corresponding points on adjacent threads Correct answer.
    3. angle between the thread flank and the axis of the screw
    4. difference between the major and minor diameters

    Explanation

    Pitch is the axial distance from a point on one thread to the corresponding point on the next thread. The distance travelled in one full turn is the lead, which equals the pitch only on a single-start thread. Flank angle and the difference between major and minor diameters describe other thread features.

  90. Question 90Fasteners

    The grip length of an aircraft bolt is measured from the:

    1. underside of the head to the start of the thread Correct answer.
    2. end of the threaded portion to the end of the shank
    3. underside of the head to the end of the bolt
    4. top of the head to the end of the bolt

    Explanation

    Grip length is the thickness of material the bolt can clamp, so it is measured from the underside of the head to the first thread. The bolt is selected so that the unthreaded shank lies within the joint and only a short length of thread is exposed beyond the nut.

  91. Question 91Fasteners

    A solid rivet with a small dimple formed in the centre of its manufactured head is identified as:

    1. a 2117-T3 alloy rivet (AD) Correct answer.
    2. a 5056 alloy rivet (B)
    3. a monel rivet (M)
    4. a 2024-T4 alloy rivet (D)

    Explanation

    2117-T3 rivets, coded AD, carry a single dimple in the centre of the head so the alloy can be recognised after the packaging has been discarded. Other alloys use different head markings or are not marked at all.

  92. Question 92Fasteners

    A cross-recess (Phillips) screw is preferred over a slotted screw in aircraft structures because it:

    1. is available in a wider range of corrosion-resistant materials
    2. may be removed with an ordinary flat-blade screwdriver
    3. can be tightened to a higher torque than any other screw type
    4. allows the driver to self-centre and limits head damage Correct answer.

    Explanation

    The tapered cross recess guides the driver into the centre of the head and cams the bit out before the recess is badly damaged. This makes it more suitable than a slotted head where controlled tightening matters. The torque capability is still limited by the recess size.

  93. Question 93Fasteners

    A Dzus fastener is a type of:

    1. high-tensile bolt used in shear joints
    2. quarter-turn quick-release fastener with a wire spring Correct answer.
    3. blind rivet installed from one side of the structure
    4. self-locking nut with a nylon insert

    Explanation

    A Dzus fastener is a quarter-turn stud that engages a spring wire to secure access panels and cowlings. The stud turns through about 90 degrees and is retained in the panel by a grommet and spring.

  94. Question 94Fasteners

    An all-metal self-locking nut provides its locking action by:

    1. distorted threads in the upper part of the nut Correct answer.
    2. a nylon collar that grips the bolt threads
    3. a cotter pin passing through the nut and bolt
    4. a spring washer trapped under the nut

    Explanation

    All-metal locknuts have the threads in the top portion deliberately distorted or made out of round so they interfere with the bolt thread and resist loosening. The nylon-insert type achieves the same result with a fibre collar rather than deformed threads.

  95. Question 95Fasteners

    The main purpose of a plain washer fitted under a nut is to:

    1. prevent the nut from turning once tightened
    2. compensate for a bolt that is too long for the grip
    3. spread the load and protect the part surface Correct answer.
    4. provide a seal against fluid leakage

    Explanation

    A plain washer distributes the clamping load over a larger area and protects the surface finish of the part from the rotating nut. It has no locking action and no sealing function; a stack of washers must not be used to make a short-grip bolt fit.

  96. Question 96Fasteners

    An aircraft bolt is to be torqued to a specified tension. If the threads are lubricated instead of being dry, the applied torque must be:

    1. reduced, because less torque is absorbed by friction Correct answer.
    2. the same, because torque values are independent of friction
    3. increased, because the lubricant cushions the threads
    4. increased, because the nut must overcome the film of lubricant

    Explanation

    The torque applied to a bolt is shared between producing tension and overcoming friction in the threads and under the nut. Lubrication lowers that friction, so less torque is needed to reach the same preload. Using dry-thread torque figures on lubricated threads would over-tension and possibly yield the bolt.

  97. Question 97Fasteners

    When installing lockwire between two bolts, the wire should be routed so that:

    1. the wire passes around the shank of each bolt below the head
    2. the wire crosses over the top of each bolt head
    3. the wire is twisted in both left- and right-hand directions
    4. bolt loosening pulls the wire in the tightening direction Correct answer.

    Explanation

    Lockwire is fitted so that any tendency of a fastener to loosen puts the wire in tension and pulls it in the tightening direction. The wire should be new, evenly twisted and routed without slack so it cannot work loose.

  98. Question 98Fasteners

    In a riveted sheet repair, the minimum edge distance from the centre of a rivet to the edge of the sheet is normally:

    1. 6 diameters of the rivet
    2. 4 diameters of the rivet
    3. 2 diameters of the rivet Correct answer.
    4. 1 diameter of the rivet

    Explanation

    Edge distance is measured from the centre of the hole to the edge of the material and should be at least two rivet diameters to prevent the sheet tearing out under load. Pitch along the row is governed by a separate rule of roughly four to six diameters.

  99. Question 99Fasteners

    The rivet pitch in a typical aircraft skin lap joint should normally lie between:

    1. 1D and 2D
    2. 2D and 3D
    3. 4D and 6D Correct answer.
    4. 8D and 10D

    Explanation

    Pitch is the distance between adjacent rivets in the same row and is normally kept between four and six rivet diameters. Rivets spaced too closely weaken the sheet, while excessive spacing allows the sheets to separate between fasteners.

  100. Question 100Fasteners

    A Hi-Lok fastener is installed by:

    1. driving the pin with a rivet gun while holding a bucking bar
    2. torquing the collar with a calibrated torque wrench to a stated value
    3. turning the pin with a screwdriver until the collar bottoms
    4. holding the pin with a hex key while the collar shears off Correct answer.

    Explanation

    The Hi-Lok pin is held with a hex key while the threaded collar is run down until its frangible section shears at the designed preload. The sheared collar is the positive indication that the correct torque has been reached, so no torque wrench is required.

  101. Question 101Fasteners

    In a blind rivet, the mandrel serves to:

    1. seal the hole against leakage after the rivet is set
    2. act as a permanent locking pin through the rivet head
    3. centre the rivet gun and prevent damage to the head
    4. upset the rivet body and break off at a set load Correct answer.

    Explanation

    The mandrel is pulled by the setting tool, expanding or upsetting the rivet tail against the far side of the structure, then it fractures at a necked point at a predetermined load. The broken stub is discarded, leaving the set rivet in place.

  102. Question 102Fasteners

    Where the internal thread in a cast component has been damaged, the approved repair is normally to:

    1. drill out the hole and fit an oversized screw without an insert
    2. build up the thread with solder and re-tap it
    3. fit a self-tapping screw in place of the original fastener
    4. install a thread insert of the original thread size Correct answer.

    Explanation

    A thread insert such as a Heli-Coil restores the original internal thread size in a damaged casting and is a standard approved repair. Any oversize repair must be specifically approved and would require an oversize fastener, not simply a larger screw driven into the hole.

  103. Question 103Fasteners

    When installing a bolt in a shear joint, the:

    1. threads should be located in the shear plane to improve grip
    2. bolt may be any length provided a washer is added
    3. nut should be fitted under the head of the bolt
    4. shank, not the threads, should lie in the shear plane Correct answer.

    Explanation

    The unthreaded shank has the full cross-section and bears on the hole wall, so it must lie in the shear plane with the threads outside the joint. Threads in the shear plane reduce bearing area and fatigue life, and the correct bolt length is chosen rather than being made up with washers.

  104. Question 104Fasteners

    A nylon-insert self-locking nut should be rejected if:

    1. it can be turned on the bolt thread by finger pressure Correct answer.
    2. the nylon insert is a light colour
    3. its colour has darkened through age
    4. it has been removed from a bolt with a socket

    Explanation

    The locking action depends on the insert being an interference fit on the bolt thread. If the nut spins on the thread under finger pressure after removal, the insert has worn and the nut must be replaced. Normal removal with a socket does not by itself condemn the nut.

  105. Question 105Fasteners

    When fitting a cotter pin to a castellated nut, the pin should be:

    1. fitted with only one leg bent, so the other can be removed easily
    2. fitted so that the legs project straight out from the nut
    3. reused only if the legs are still straight and unbroken
    4. a new pin, head seated in the slot and legs bent back Correct answer.

    Explanation

    A new cotter pin is used each time, with its head seated in the slot of the nut and the legs bent back tightly around the bolt end so the pin cannot work out. The nut is then adjusted so that a slot lines up with the hole rather than being backed off.

  106. Question 106Fasteners

    The correct method of safetying an aircraft control turnbuckle is to:

    1. peen the ends of the barrel over the fittings
    2. run lockwire through the barrel hole and secure it to both end fittings Correct answer.
    3. tighten the barrel until the end fittings cannot move
    4. fit a split pin through the turnbuckle barrel

    Explanation

    A turnbuckle is normally safetied with lockwire passed through the hole in the barrel and wrapped around both terminal fittings, or with an approved turnbuckle clip. This prevents the barrel from rotating and altering the control cable tension.

  107. Question 107Fasteners

    Unless the maintenance manual states otherwise, a specified torque value is applied to the:

    1. washer, using a torque screwdriver
    2. threads, measured by the number of exposed threads
    3. nut, while the bolt head is prevented from turning Correct answer.
    4. head of the bolt, with the nut held

    Explanation

    Torque is normally applied to the nut while the bolt head is held steady, so that the shank is not twisted and the friction under the head is properly accounted for. Where the manual specifies torquing the head instead, that instruction takes precedence.

  108. Question 108Fasteners

    Monel rivets are commonly selected for use:

    1. where the rivet must be softened before driving
    2. in stainless steel structures where aluminium rivets would corrode Correct answer.
    3. in soft aluminium alloy sheet where high strength is not required
    4. in magnesium alloy structures to save weight

    Explanation

    Monel is a nickel-copper alloy with good strength and corrosion resistance, and it is chosen where it is compatible with stainless or other corrosion-resisting parts. Aluminium alloy rivets in contact with stainless steel would set up galvanic corrosion.

  109. Question 109Fasteners

    After driving a solid rivet, the shop head should be approximately:

    1. 1.5 times the rivet diameter wide and 0.5 times high Correct answer.
    2. 2 times the rivet diameter wide and 1.5 times high
    3. 0.75 times the rivet diameter wide and 0.25 times high
    4. 1 times the rivet diameter wide and 1 times high

    Explanation

    The driven head should be about one and a half diameters in width and half a diameter in height. An undersized head lacks strength, while an oversized or flattened head indicates over-driving and possible damage to the surrounding sheet.

  110. Question 110Fasteners

    An interference-fit fastener improves the fatigue life of a joint mainly because it:

    1. leaves residual compressive stress around the hole, reducing fatigue Correct answer.
    2. allows the bolt to be removed without disturbing the hole
    3. seals the joint against fuel leakage
    4. increases the clamping force of the nut for a given torque

    Explanation

    Filling the hole with an interference fit, or using a tapered shank, leaves residual compressive stress in the material around the hole. This reduces the alternating tensile stress at the hole edge and delays the initiation of fatigue cracks.

  111. Question 111Pipes and Unions

    What is the included angle of the flare used on standard aircraft flared tube fittings?

    1. 45°
    2. 30°
    3. 37° Correct answer.
    4. 60°

    Explanation

    Aircraft flared tube fittings of the AN/MS type use a 37° flare that seats against a matching 37° cone machined in the fitting body. The 45° flare belongs to the SAE automotive standard and does not match an aircraft cone.

  112. Question 112Pipes and Unions

    What is the function of a straight union in a fluid line?

    1. It joins two tubes of the same diameter in a straight run Correct answer.
    2. It connects a tube to a threaded port in a component
    3. It allows a line to pass through a structural bulkhead
    4. It joins two tubes of different diameters

    Explanation

    A straight union has two identical tube ends, so it can only join two lines of the same size running in the same direction, with the seal made at each flare or sleeve. Different functions require a reducing union, a bulkhead fitting or a component port fitting.

  113. Question 113Pipes and Unions

    How does a bulkhead union secure and seal a line where it passes through a structural panel?

    1. It seals a tube directly into a threaded port in a component
    2. It lets the line be disconnected by hand without tools
    3. Its threaded body passes through the panel and is clamped by a nut on each side, with a tube connection at each end Correct answer.
    4. It joins two tubes of different diameters on one side of the panel

    Explanation

    A bulkhead fitting has an elongated threaded body that passes through the hole in the structure, and a nut on each side clamps it in place. The tube connections are made at both ends of the body, so the fluid path stays sealed as it crosses the panel.

  114. Question 114Pipes and Unions

    How is the seal produced in a flareless (swaged-sleeve) tube fitting?

    1. A rubber washer is compressed by the nut
    2. The tube is brazed into the fitting body
    3. A sleeve is swaged onto the tube so that it both seals and grips Correct answer.
    4. An O-ring on the tube end provides the seal

    Explanation

    In a flareless fitting the tube is not flared; instead a hardened sleeve is crushed onto the outside of the tube as the nut is tightened. The swaged sleeve provides both the fluid seal and the mechanical grip that resists pull-out.

  115. Question 115Pipes and Unions

    How are pipe and tube sizes designated?

    1. Pipe is sized by wall thickness alone
    2. Pipe is sized by outside diameter, tube by nominal bore
    3. Pipe is sized by nominal bore, tube by outside diameter and wall thickness Correct answer.
    4. Both pipe and tube are sized by outside diameter only

    Explanation

    Pipe is designated by its nominal bore, which is only approximately related to the actual bore, with the wall given by the schedule. Tubing is designated by its actual outside diameter and wall thickness, which is why tubing dimensions can be used directly for fitting selection.

  116. Question 116Pipes and Unions

    Which practice prevents a flexible hose from being twisted during installation?

    1. Marking a line along the hose and checking that it stays straight while the nut is tightened Correct answer.
    2. Stretching the hose to remove all slack before tightening
    3. Holding the hose with pliers while the nut is turned
    4. Rotating the hose body itself to tighten the end fitting

    Explanation

    A line marked along the hose before installation shows whether the hose has rotated as the nut is tightened. Twisting a hose shortens its life because the reinforcement wires are stressed and the hose tends to kink or lift off its supports when pressurized.

  117. Question 117Pipes and Unions

    Which tubing material is normally selected for a line routed in a high-temperature zone such as near an engine exhaust?

    1. Aluminium alloy 1100
    2. Nylon
    3. Corrosion-resistant steel Correct answer.
    4. Copper

    Explanation

    Corrosion-resistant steel tubing retains useful strength and resists oxidation at the elevated temperatures found near engines and exhausts. Aluminium loses strength rapidly when hot, and copper and nylon are not suitable for high-temperature aircraft fluid lines.

  118. Question 118Pipes and Unions

    What is the function of a tee fitting in a fluid system?

    1. To allow a line to pass through a bulkhead
    2. To connect two tubes of different diameters
    3. To divide a flow into two branches or to combine two branches into one Correct answer.
    4. To blank off an unused port

    Explanation

    A tee has three tube ends: one run continues straight through while the branch turns off at right angles. It therefore splits a single flow into two, or merges two flows into one, depending on the direction of flow.

  119. Question 119Pipes and Unions

    Which preparation is essential before a tube end is flared?

    1. The tube must be filled with hydraulic fluid to prevent collapse
    2. The end must be threaded to hold the nut
    3. The end must be bent through 90° to support the flare
    4. The end must be cut square, deburred and set to the correct height above the flaring block Correct answer.

    Explanation

    A square, burr-free cut and the correct amount of tube protruding above the flaring block are needed to produce a concentric flare of the right size. Too little protrusion gives an undersized flare that will not seal, while too much gives an oversized, thin flare.

  120. Question 120Pipes and Unions

    Why must a tube not be bent to a radius smaller than the recommended minimum?

    1. The tube absorbs moisture through the bend
    2. The tube becomes stronger and harder to flare afterwards
    3. The wall thins on the outside of the bend and may wrinkle on the inside Correct answer.
    4. The fluid flow is unaffected and only the appearance changes

    Explanation

    Bending stretches the outer wall and compresses the inner wall, so an excessively tight bend thins the outside and can wrinkle or collapse the inside. Both effects weaken the tube and restrict flow, which is why manufacturers publish a minimum bend radius for each tube size and condition.

  121. Question 121Pipes and Unions

    How tight should a cushioned clamp be on a rigid fluid line?

    1. Fitted only at the two ends of the run, with no intermediate support
    2. Loose enough that the tube can slide freely in the clamp
    3. As tight as possible so that all vibration is eliminated
    4. Firmly enough to stop chafing and movement without crushing or deforming the tube Correct answer.

    Explanation

    A clamp must hold the line against vibration and chafing without squeezing the tube out of round, since a deformed tube restricts flow and creates a stress point. Intermediate supports are also needed so that the tube does not sag or vibrate over long runs.

  122. Question 122Pipes and Unions

    What should be done where an aluminium tube is clamped directly to steel structure?

    1. The aluminium tube should be replaced with a copper tube
    2. The clamp should be tightened very firmly to exclude all moisture
    3. No action is needed, because aluminium and steel are compatible
    4. A protective sleeve or insulating clamp should be fitted between the tube and the structure Correct answer.

    Explanation

    Aluminium and steel form a galvanic couple, and moisture trapped at the contact point causes the aluminium to corrode rapidly. A plastic sleeve, insulated clamp or protective tape separates the metals and removes the electrical path needed for galvanic attack.

  123. Question 123Pipes and Unions

    How should a flexible hose be installed between two components?

    1. Under tension so that it cannot whip
    2. With slight slack so that pressure expansion, movement and vibration do not pull on the end fittings Correct answer.
    3. Stretched tight so that the run looks neat
    4. With at least one full loop to absorb movement

    Explanation

    A hose changes length slightly under pressure and must accommodate relative movement between the components it connects. A little slack absorbs this without putting tension on the end fittings, whereas a taut hose pulls on its attachments and shortens its service life.

  124. Question 124Pipes and Unions

    Why must the identification marking on a flexible hose assembly stay legible?

    1. So that the hose can be identified as the highest-pressure line in the system
    2. Because the marking gives the torque value for the end fittings
    3. So that the manufacture date and specification can be checked against its shelf and service life limits Correct answer.
    4. Because the marking shows the direction of flow through the hose

    Explanation

    Hose assemblies carry a marking that identifies the specification and the date of manufacture, which are the basis for shelf life and service life limits. If the marking is lost, the assembly cannot be shown to be within its limits and must be replaced.

  125. Question 125Pipes and Unions

    How do tapered pipe threads achieve a seal?

    1. They are parallel threads that rely on an O-ring
    2. They are tapered and seal by the wedging action of the threads, assisted by a suitable sealing compound Correct answer.
    3. They seal by a flare formed at the end of the pipe
    4. They seal only by a copper washer under the hexagon

    Explanation

    In a tapered thread the crests of the male and female threads interfere progressively as the joint is made up, closing the leak path; a compatible sealing compound fills any remaining spiral gap. The compound must be applied so that excess cannot enter and contaminate the system.

  126. Question 126Pipes and Unions

    What is the consequence of overtightening a flare nut on a tube fitting?

    1. The flow through the fitting is restricted by the tighter joint
    2. The tube is pulled out of the fitting
    3. The flare angle is increased towards 45°
    4. The nut or the flare can be cracked or distorted, causing a leak Correct answer.

    Explanation

    The flare nut is tightened until the flare is seated and gripped, and further tightening only adds stress. Excess torque can split the nut, crack the flare or brinell the seating cone, and any of these produces a leak that cannot be cured by more tightening.

  127. Question 127Pipes and Unions

    Why must burrs be removed from the inside of a cut tube end?

    1. Burrs help the flare to grip the fitting cone
    2. Burrs have no effect on a low-pressure line
    3. Burrs restrict the flow path and can break away as particles that contaminate the system Correct answer.
    4. Burrs increase the effective wall thickness at the flare

    Explanation

    A burr left on the bore reduces the flow area and is only weakly attached, so it can break off and travel downstream into valves, pumps or filters. Deburring also removes sharp edges that could start a crack at the flare.

  128. Question 128Pipes and Unions

    How must a flexible hose be protected when it is routed through a designated fire zone?

    1. It must be left bare so that leaks can be seen easily
    2. It must be fitted with a fire-resistant protective sleeve Correct answer.
    3. It must be wrapped in electrical insulating tape
    4. It must be replaced with a rigid aluminium tube

    Explanation

    Hoses in fire zones are required to survive a fire long enough to keep the system functioning, so a fire-resistant sleeve is fitted over the hose. The sleeve also gives some protection against chafing and abrasion.

  129. Question 129Pipes and Unions

    A repaired hydraulic line leaks at the flare although the nut is correctly torqued and the flare itself is undamaged. What is the most likely cause?

    1. The tube has been flared to 45° instead of the 37° required by the fitting Correct answer.
    2. The nut was lubricated before assembly
    3. The tube wall is thicker than the fitting was designed for
    4. The tube was bent too close to the flare

    Explanation

    A 45° flare contacts a 37° cone only on a narrow line near the rim, so the joint cannot seal however much the nut is tightened. The mismatch is common when an automotive flaring tool is used by mistake, and the remedy is to cut off the flare and re-flare to 37°.

  130. Question 130Pipes and Unions

    Why is a tube bent slightly beyond the required angle when a hand tube bender is used?

    1. To work-harden the bend so that it holds its shape permanently
    2. To allow for the tube stretching as it is pushed through the bender
    3. To make the bend radius larger than the tool mark
    4. To compensate for the tube springing back elastically when the bending force is released Correct answer.

    Explanation

    Metal tubing recovers elastically when the bending load is removed, so the finished angle is always less than the angle to which the tool was driven. Overbending by the amount of springback gives the required final angle, which is checked against a template.

  131. Question 131Pipes and Unions

    What must be done to the sleeve before a flareless tube fitting is finally assembled?

    1. It must be preset onto the tube with the correct tool and checked for correct position Correct answer.
    2. It must be flared to 37° to match the fitting cone
    3. It must be heated and shrunk onto the tube
    4. It must be left loose so that it centres itself during tightening

    Explanation

    In a flareless fitting the sleeve must be swaged onto the tube in a controlled presetting operation, using the specified tooling, so that it grips at the correct point on the tube. The preset position is verified with a gauge or by the specified protrusion before the final assembly is torqued.

  132. Question 132Pipes and Unions

    A flexible hose fails by fatigue cracking of the braid right at the end fitting. Which installation fault is the most likely cause?

    1. The hose was fitted with a fire-resistant sleeve
    2. The hose was bent sharply immediately at the fitting instead of leaving a straight section Correct answer.
    3. The hose was held by cushioned clamps along its length
    4. The hose was slightly longer than the gap between the components

    Explanation

    A hose must leave the end fitting in a straight line for a short distance, because a bend starting at the nipple concentrates flexing stress on a few braid wires and they fatigue and break. An elbow fitting or a longer hose is used so that the bend occurs away from the fitting.

  133. Question 133Springs, Bearings and Transmissions

    A spring that is designed to be shortened along its axis by an applied force is called a:

    1. Extension spring
    2. Compression spring Correct answer.
    3. Leaf spring
    4. Torsion spring

    Explanation

    Springs are classified by the way they are loaded. A compression spring is designed to be pushed together along its axis, and it pushes back against that force.

  134. Question 134Springs, Bearings and Transmissions

    In a ball bearing, each ball contacts the raceway:

    1. At a single point Correct answer.
    2. Over the full ball surface
    3. Along two parallel lines
    4. Along a line

    Explanation

    A sphere touching a curved groove makes theoretical contact at one point, which is why ball bearings suit light-to-moderate loads at high speed. Roller bearings, by contrast, spread the load over a line of contact.

  135. Question 135Springs, Bearings and Transmissions

    The primary function of the lubricant in an anti-friction bearing is to:

    1. Separate the rolling elements from the raceways Correct answer.
    2. Raise the load rating quoted by the manufacturer
    3. Increase the radial internal clearance of the bearing
    4. Remove the need for any seals

    Explanation

    Lubricant forms a film that keeps the rolling elements and raceways apart, so metal-to-metal contact, friction and wear are minimised. It also carries away heat and helps exclude dirt and moisture.

  136. Question 136Springs, Bearings and Transmissions

    Spur gears transmit motion between shafts that are:

    1. At any angle to each other
    2. At right angles with non-intersecting axes
    3. Parallel to each other Correct answer.
    4. At right angles with intersecting axes

    Explanation

    Spur gear teeth are cut parallel to the shaft axis, so the gears mesh only when their shafts are parallel. Right-angle drives need bevel, worm or similar gearing.

  137. Question 137Springs, Bearings and Transmissions

    In a flat belt drive, slip between the belt and the pulley becomes significant when:

    1. The pulley diameter is increased
    2. A wider belt of the same material is fitted
    3. Belt tension is increased above its normal value
    4. Belt tension falls and the driven load rises Correct answer.

    Explanation

    A flat belt relies on friction created by tension, so the drive can only transmit as much torque as friction supports. If the load torque exceeds that limit, or tension is lost, the belt slips on the pulley.

  138. Question 138Springs, Bearings and Transmissions

    Compared with a ball bearing of similar size, a plain bush bearing offers:

    1. Quiet running with good shock load capacity Correct answer.
    2. Much lower starting friction than a ball bearing
    3. No lubrication of any kind is required
    4. A higher limiting speed than a ball bearing

    Explanation

    A plain bearing has no rolling elements, so it runs quietly and its conforming surface spreads shock loads over a large area. Its drawback is higher starting friction and a need for a continuous oil film.

  139. Question 139Springs, Bearings and Transmissions

    A universal joint in a shaft drive allows:

    1. Telescopic length compensation only
    2. Torque transmission between misaligned shafts Correct answer.
    3. Torque transmission only when shafts are aligned
    4. Conversion of rotary motion into linear motion

    Explanation

    A universal joint is a flexible coupling that transmits torque while the two shafts are at an angle to each other. This is why it is used in control runs and accessory drives where alignment changes.

  140. Question 140Springs, Bearings and Transmissions

    A spring with a rate of 40 N/mm is compressed by 15 mm. The force it exerts is:

    1. 55 N
    2. 600 N Correct answer.
    3. 2.7 N
    4. 150 N

    Explanation

    For an elastic spring, force equals spring rate multiplied by deflection, so 40 N/mm x 15 mm = 600 N. The rate is the force required to produce unit deflection.

  141. Question 141Springs, Bearings and Transmissions

    A Belleville washer is used principally to:

    1. Retain a bearing radially in its housing
    2. Isolate torsional vibration in a rotating shaft
    3. Act as a long-stroke compression spring
    4. Give a high preload in a short space Correct answer.

    Explanation

    A Belleville washer is a dished disc spring that produces a large force for a very small deflection. This makes it ideal for applying preload where axial space is limited, such as bearing and joint assemblies.

  142. Question 142Springs, Bearings and Transmissions

    A torsion spring is loaded:

    1. By radial expansion of its coils
    2. By bending of the wire between supports
    3. By twisting about its own axis Correct answer.
    4. By axial compression between its ends

    Explanation

    A torsion spring stores energy when its coils are wound tighter or unwound, with the end legs reacting against the load. The wire is therefore loaded in torsion rather than in simple tension or compression.

  143. Question 143Springs, Bearings and Transmissions

    Tapered roller bearings are particularly suited to carrying:

    1. Combined radial and axial loads Correct answer.
    2. Angular misalignment between the shafts
    3. Pure radial loads at very high speed
    4. Applications that need no lubrication

    Explanation

    The conical geometry of a tapered roller bearing lets it react both radial and thrust loads along its axis of contact. Bearings are usually mounted in opposed pairs so that thrust can be taken in either direction.

  144. Question 144Springs, Bearings and Transmissions

    A thrust bearing is designed primarily to carry:

    1. Moment loads only
    2. Axial load along the shaft Correct answer.
    3. Combined radial and moment loads
    4. Radial load only

    Explanation

    A thrust bearing reacts forces acting along the axis of the shaft, such as the thrust produced by a propeller or a helical gear. Radial loads are carried by separate radial bearings.

  145. Question 145Springs, Bearings and Transmissions

    A gear train has a 20-tooth driver and a 60-tooth driven gear. The output is:

    1. One third speed, triple torque Correct answer.
    2. One third speed, one third torque
    3. Three times speed, one third torque
    4. Three times speed, triple torque

    Explanation

    Speed ratio equals the number of driver teeth divided by the number of driven teeth, so 20/60 gives one third of the input speed. Ignoring losses, torque rises by the inverse ratio, so it is multiplied by three.

  146. Question 146Springs, Bearings and Transmissions

    Bevel gears are used to transmit drive:

    1. Between non-intersecting shafts at 90 degrees
    2. Between intersecting shafts at 90 degrees Correct answer.
    3. From rotary motion to reciprocating motion
    4. Between parallel shafts

    Explanation

    Bevel gears have teeth cut on conical pitch surfaces, so their axes intersect, normally at a right angle. Non-intersecting right-angle drives need worm or crossed-helical gearing instead.

  147. Question 147Springs, Bearings and Transmissions

    A single-start worm and wheel combination gives:

    1. A high reduction that is usually self-locking Correct answer.
    2. Drive between parallel shafts
    3. A reversible drive with low friction losses
    4. A very low reduction ratio with high efficiency

    Explanation

    One turn of a single-start worm advances the wheel by only one tooth, so very large reductions are obtained from a compact unit. The sliding action gives high friction, which is why such drives are often self-locking.

  148. Question 148Springs, Bearings and Transmissions

    A V-belt can transmit more power than a flat belt of the same width because:

    1. It is made from a stronger material
    2. Wedge action in the groove increases grip Correct answer.
    3. It needs larger diameter pulleys
    4. It relies on tension alone for grip

    Explanation

    The tapered sides of a V-belt press against the flanks of the pulley groove, and this wedge effect multiplies the available friction for a given belt tension. A flat belt relies only on the friction of one flat surface.

  149. Question 149Springs, Bearings and Transmissions

    Splines machined on a shaft are used to:

    1. Seal the gap between shaft and housing
    2. Centre a bearing radially on the shaft
    3. Retain the shaft axially against thrust
    4. Transmit torque while allowing axial sliding Correct answer.

    Explanation

    Splines are axial teeth that engage matching internal teeth, so they carry torque positively while the mating part can slide along the shaft. This is common in gearbox and accessory drives where the length must vary.

  150. Question 150Springs, Bearings and Transmissions

    Compared with a belt drive, a chain drive:

    1. Requires no lubrication
    2. Permits slip under overload
    3. Gives an exact speed ratio without slip Correct answer.
    4. Runs more quietly at high speed

    Explanation

    A chain engages sprocket teeth, so it is a positive drive that cannot slip and holds an exact ratio. Belts depend on friction and can slip when overloaded.

  151. Question 151Springs, Bearings and Transmissions

    Preloading a pair of opposed tapered roller bearings:

    1. Always reduces bearing life
    2. Removes internal clearance and increases stiffness Correct answer.
    3. Has no effect on shaft rigidity
    4. Increases internal clearance and reduces stiffness

    Explanation

    Preload holds the rolling elements firmly against their races, eliminating internal clearance so the shaft is located more rigidly under load. Within the manufacturer's limits this improves stiffness and run-out accuracy without shortening life.

  152. Question 152Springs, Bearings and Transmissions

    Excessive backlash in a gear train will most likely cause:

    1. Increased load carrying capacity
    2. Overheating of the bearings only
    3. Tooth interference and seizure
    4. Impact loading and noise on reversal Correct answer.

    Explanation

    Backlash is the clearance between meshing teeth; if it is too large, the driven gear accelerates across the gap whenever the load reverses, producing shock loads and noise. Too little backlash causes interference, heating and seizure.

  153. Question 153Springs, Bearings and Transmissions

    The helical teeth of a helical gear produce, in addition to radial load:

    1. No additional load at all
    2. An axial thrust needing a thrust bearing Correct answer.
    3. A tangential load only
    4. A bending moment on the shaft only

    Explanation

    Because helical teeth are cut at an angle, the tooth force has a component along the shaft axis as well as the tangential driving force. Bearings must therefore be arranged to react this thrust, or the helix angle must be opposed by a double helical design.

  154. Question 154Springs, Bearings and Transmissions

    Surge in an engine valve spring occurs when:

    1. The spring is compressed past its solid length
    2. The spring is over-lubricated in service
    3. The spring's natural frequency matches the load frequency Correct answer.
    4. The wire diameter is too large for the coil

    Explanation

    A coil spring behaves like a spring-mass system with its own natural frequency. If the frequency of the applied load matches it, waves of compression travel up and down the coils and the valve motion becomes erratic.

  155. Question 155Control Cables

    Which control cable construction is most suitable for a run that must pass around several pulleys?

    1. A single solid wire of large diameter
    2. 7 x 7, made of medium wires
    3. 7 x 19, made of many small wires Correct answer.
    4. 1 x 19, made of large wires

    Explanation

    Flexibility in a cable comes from having many small wires, so a 7 x 19 cable (seven strands of nineteen wires) bends easily around pulleys and tolerates repeated flexing without fatigue. Constructions with fewer, larger wires are stiffer and suited to straighter runs.

  156. Question 156Control Cables

    Where maximum stiffness and abrasion resistance are needed in a straight non-moving installation, the cable normally chosen is:

    1. 1 x 19 stranded cable Correct answer.
    2. 7 x 19 stranded cable
    3. 6 x 7 stranded cable
    4. 7 x 7 stranded cable

    Explanation

    A 1 x 19 cable is made of a few large wires, giving the greatest stiffness and the best resistance to external abrasion, which suits straight runs such as ties and bracing where no bending is required. Cables with more strands trade stiffness for flexibility.

  157. Question 157Control Cables

    The purpose of a turnbuckle in a cable control system is to:

    1. absorb vibration in the cable run
    2. increase the mechanical advantage of the control
    3. adjust cable length and hence tension Correct answer.
    4. provide a means of disconnecting the cable quickly

    Explanation

    A turnbuckle has left- and right-hand threads so that rotating the barrel shortens or lengthens the run, which sets the cable tension. It is an adjustment device, not a means of altering mechanical advantage or damping vibration.

  158. Question 158Control Cables

    The function of a thimble in a cable eye terminal is to:

    1. protect the eye from wear at the bolt Correct answer.
    2. seal the terminal against moisture ingress
    3. provide a fine tension adjustment
    4. grip the cable strands firmly

    Explanation

    The thimble is a grooved metal liner that spreads the load and keeps the cable from rubbing directly on the attachment bolt or pin. It does not grip the strands or provide adjustment.

  159. Question 159Control Cables

    In a cable control system, a pulley is used to:

    1. absorb the stretch in a new cable
    2. increase the tension in the cable run
    3. change the direction of the cable run Correct answer.
    4. stop the cable from chafing on structure

    Explanation

    A pulley redirects a cable run with low friction, allowing the control to be routed from the cockpit to the surface. It does not change tension and is not a substitute for a fairlead.

  160. Question 160Control Cables

    A fairlead is fitted in a cable system to:

    1. allow the cable to pass round a corner with low friction
    2. maintain a constant tension in the run
    3. guide the cable and prevent it rubbing on structure Correct answer.
    4. support the weight of the cable between supports

    Explanation

    A fairlead is a simple guide, often a block or bush with a smooth bore, that keeps a long cable run aligned and clear of structure so it cannot chafe. It does not carry load like a pulley or control tension.

  161. Question 161Control Cables

    After a turnbuckle has been adjusted to give the correct cable tension, it must be:

    1. positively locked to prevent rotation Correct answer.
    2. left unlocked so that tension can self-adjust
    3. backed off half a turn to relieve the stress
    4. welded to the adjacent cable terminal

    Explanation

    A turnbuckle that is free to rotate will allow the cable tension to change in service, so it must be locked after adjustment with its check nuts, a locking clip or safety wire as specified. Backing it off would remove the adjustment just made.

  162. Question 162Control Cables

    When checking cable tension with a tensiometer, the reading must be corrected for:

    1. the age of the cable only
    2. the number of pulleys in the run
    3. the length of the cable run only
    4. temperature and cable diameter Correct answer.

    Explanation

    A tensiometer reading depends on the diameter of the cable being deflected and on the ambient temperature, because the rigging chart tension is quoted at a reference temperature. The charts supplied with the instrument give the correction to apply.

  163. Question 163Control Cables

    A control cable that is tensioned too low will most likely cause:

    1. stiffness of the control around neutral
    2. excessive load on the pulley bearings
    3. overloading of the turnbuckle threads
    4. lost motion at the surface and cable whip Correct answer.

    Explanation

    With insufficient tension the cable sags and can whip, and part of the control input is used up in taking up the slack, giving lost motion at the surface and imprecise control. High bearing loads and stiffness are symptoms of excessive tension.

  164. Question 164Control Cables

    Excessive cable tension is undesirable mainly because it:

    1. loads pulleys, bearings and attachments heavily Correct answer.
    2. allows the cable to ride out of the pulley grooves
    3. reduces the friction in the system
    4. causes lost motion in the control run

    Explanation

    Over-tensioning raises the steady loads carried by pulleys, their bearings, bell cranks and attachment brackets, and it also increases friction in the run. Lost motion and cables leaving pulley grooves are symptoms of tension that is too low.

  165. Question 165Control Cables

    Rigging pins are used during the rigging of a flight control system to:

    1. lock a control surface during maintenance
    2. measure the travel of the control surface
    3. limit the maximum deflection of the stick
    4. hold the control system in the neutral position Correct answer.

    Explanation

    Rigging pins fit through alignment holes in the control mechanism and hold the system at a known neutral datum while cables are tensioned and linkages adjusted. Surface travel is then measured against that datum with a protractor or travel board.

  166. Question 166Control Cables

    The function of a cable tension regulator in a control system is to:

    1. keep tension constant when temperature changes Correct answer.
    2. release the cable if a control surface becomes jammed
    3. limit the peak tension reached under high control loads
    4. amplify the pilot's input before it reaches the surface

    Explanation

    A tension regulator is a spring-loaded device that takes up slack or pays out cable as the airframe and cable expand and contract at different rates, so the rigging tension stays essentially constant. It is not a jam release or a load limiter.

  167. Question 167Control Cables

    After a terminal has been swaged onto a control cable, the assembly must be:

    1. tested at its full breaking load before fitment
    2. annealed to relieve stress in the swage
    3. painted to seal the swage against moisture
    4. proof loaded to a set percentage of cable strength Correct answer.

    Explanation

    Swaged assemblies are proof loaded to a specified proportion of the rated cable strength so that any defective swage is revealed before the cable enters service. Loading to the full breaking load would damage a sound assembly.

  168. Question 168Control Cables

    A control cable with a kink or a birdcaged section must be:

    1. spliced at the damaged area
    2. marked and re-inspected at the next check
    3. stretched straight and returned to service
    4. replaced with a new cable Correct answer.

    Explanation

    A kink or birdcage means the strands have been permanently distorted and some wires are already overstressed, so the cable has lost strength and cannot be straightened back into service. Control cables are not repaired by splicing; the affected cable is replaced.

  169. Question 169Control Cables

    Uneven wear on one side of a cable where it passes over a pulley usually indicates:

    1. poor pulley alignment with the cable run Correct answer.
    2. excessive lubrication of the pulley
    3. the cable is of an incorrect construction type
    4. cable tension is too low

    Explanation

    A cable should run centrally in the pulley groove with the pulley plane aligned to the run; if the pulley is out of line the cable bears on one flange and the wires wear on one side only. The alignment and the free rotation of the pulley should be checked.

  170. Question 170Control Cables

    A cable guard fitted close to a pulley is intended to:

    1. take the load off the pulley bearing
    2. prevent the cable from being over-tensioned
    3. lubricate the cable as it passes over the pulley
    4. keep the cable in its groove if it goes slack Correct answer.

    Explanation

    A guard is a close-fitting device that stops a slack or whipping cable from jumping out of the pulley groove and jamming or chafing. It has no effect on tension or bearing load.

  171. Question 171Control Cables

    When no tensiometer is available, cable tension may be estimated by:

    1. deflecting the cable and measuring the force used Correct answer.
    2. measuring the cable diameter with a micrometer
    3. checking free play at the control column
    4. counting the threads exposed on the turnbuckle

    Explanation

    The deflection method applies a measured force at the mid-point of a known span and compares the deflection obtained with the manufacturer's chart, which gives the equivalent tension. Thread count and diameter do not indicate tension.

  172. Question 172Control Cables

    A push-pull rod is preferred to a cable where the control:

    1. must carry tension and compression in a straight line Correct answer.
    2. is required to be as light as possible
    3. must pass around several pulleys
    4. must be routed around several pulleys in a confined bay

    Explanation

    A rigid rod can transmit both a pull and a push, so it is used for straight-line runs between bell cranks and surfaces without needing a return cable. It cannot negotiate bends, which is where a cable and pulleys are needed.

  173. Question 173Control Cables

    On most aircraft, the primary stops that limit the travel of a flight control surface are located:

    1. at the quadrant or bell crank in the system Correct answer.
    2. at the control surface horn or hinge bracket
    3. on the pulley brackets along the cable run
    4. in the cockpit on the control column or yoke

    Explanation

    Travel is limited by stops in the control system itself, normally at the quadrant or bell crank, so that the surface never carries the stop loads through its hinges. Stops at the surface, where fitted, serve only as secondary limits.

  174. Question 174Control Cables

    A control cable correctly tensioned on a warm day may become slack when the aircraft is cold-soaked because:

    1. the steel cable expands more than the aluminium structure
    2. the turnbuckle threads contract and lose engagement
    3. the aluminium structure contracts more than the cable Correct answer.
    4. the cable stretches permanently at low temperature

    Explanation

    Aluminium has a higher coefficient of thermal expansion than steel, so as the airframe cools the structure between cable attachment points shrinks more than the cable does, and the tension falls. This is why rigging charts specify a reference temperature and why regulators are fitted.

  175. Question 175Control Cables

    After a new control cable has been in service for a short time, the tension may need re-adjusting because:

    1. the new cable beds in and stretches slightly Correct answer.
    2. the cable work-hardens and shortens in service
    3. the safety wire on the turnbuckle stretches
    4. the pulleys bed into their mounting brackets

    Explanation

    A new cable settles into its terminals and pulleys and the strands bed together, so the run lengthens slightly and tension drops. A re-check and adjustment after the initial period of service restores the rigging tension.

  176. Question 176Control Cables

    Aileron differential is rigged so that:

    1. the up aileron travels further than the down aileron Correct answer.
    2. both ailerons move through equal angles up and down
    3. the ailerons move in the same sense as the rudder
    4. the down aileron travels further to increase drag

    Explanation

    Making the up-going aileron deflect further than the down-going one reduces the extra lift and induced drag produced on the down-going wing, which reduces adverse yaw. Equal travel gives no such compensation.

  177. Question 177Electrical Cables and Connectors

    In the AWG system used for aircraft wiring, what happens to the conductor cross-sectional area as the gauge number increases from 12 to 20?

    1. It decreases Correct answer.
    2. It doubles for every six gauge numbers
    3. It stays the same for a given current rating
    4. It increases

    Explanation

    The AWG scale is inverse: a larger gauge number denotes a smaller conductor diameter and therefore a smaller cross-sectional area. Moving from 12 AWG to 20 AWG therefore gives a much thinner, lower-current-rated wire.

  178. Question 178Electrical Cables and Connectors

    Which wire insulation is normally chosen for a zone where the wiring must withstand continuous temperatures of about 260 degrees C?

    1. Polyethylene
    2. PTFE Correct answer.
    3. Neoprene
    4. PVC

    Explanation

    PTFE is a high-temperature insulation rated to roughly 260 degrees C and is also resistant to aircraft fluids and fuels. PVC, polyethylene and neoprene are all limited to much lower continuous temperatures.

  179. Question 179Electrical Cables and Connectors

    What is the purpose of the key and keyway arrangement on a circular electrical connector?

    1. To lock the coupling ring in the tightened position
    2. To provide the electrical bond between the shell halves
    3. To retain the contacts in the insert
    4. To prevent mismating Correct answer.

    Explanation

    Keys and keyways give each connector pair a unique clocking so that a plug can only be mated with the correct receptacle and only in the correct orientation. Coupling is retained by threads or a bayonet detent, bonding is made by shell-to-shell contact, and contacts are held by retention clips.

  180. Question 180Electrical Cables and Connectors

    Why are electrical wire bundles supported by clamps at regular intervals along aircraft structure?

    1. To prevent chafing and to limit vibration fatigue Correct answer.
    2. To increase the current-carrying capacity of the wires
    3. To keep the bundle straight for easier identification only
    4. To provide a return path for the electrical current

    Explanation

    Regular support stops the bundle rubbing against structure and stops flexing at terminations, which would otherwise fatigue the conductor strands and insulation. Excessive spacing allows the bundle to sag, chafe and vibrate.

  181. Question 181Electrical Cables and Connectors

    Which two factors determine the correct crimp terminal for a particular connection?

    1. Circuit voltage and frequency
    2. Wire gauge and terminal stud size Correct answer.
    3. Wire colour and insulation type
    4. Current rating and bundle factor

    Explanation

    The terminal barrel must suit the conductor gauge so that the crimp is gas-tight, and the terminal tongue must suit the stud or screw it is bolted to. Insulation colour, circuit voltage and bundling do not size the terminal.

  182. Question 182Electrical Cables and Connectors

    What information is normally given by the identification marking on an aircraft wire?

    1. The circuit identification and wire number Correct answer.
    2. The resistance per metre of the conductor
    3. The insulation material and colour code only
    4. The length of the wire run and its date of manufacture

    Explanation

    Wire markings carry the circuit function or system code and a unique wire number so that the wire can be traced in the wiring diagrams and physically located in the harness. They do not normally record material, length or resistance.

  183. Question 183Electrical Cables and Connectors

    What is the main purpose of the braided shield around a signal cable in an aircraft?

    1. To provide a fire-resistant barrier
    2. To limit electromagnetic interference Correct answer.
    3. To carry the return current for the circuit
    4. To increase the mechanical strength of the conductor

    Explanation

    A shield confines the electromagnetic field of the signal inside the cable and keeps external fields out, reducing both radiation and pick-up. It is not intended to carry return current, to strengthen the conductor or to act as a fire barrier.

  184. Question 184Electrical Cables and Connectors

    A 10 A load is supplied through a cable whose two conductors together have a resistance of 0.05 ohm. What voltage drop appears at the load?

    1. 0.10 V
    2. 0.5 V Correct answer.
    3. 0.05 V
    4. 2.0 V

    Explanation

    Voltage drop equals current multiplied by the total loop resistance of the cable, so 10 A x 0.05 ohm = 0.5 V. This value must be subtracted from the supply voltage when checking that the equipment still receives its minimum voltage.

  185. Question 185Electrical Cables and Connectors

    Why is the current rating of a wire lower when it forms part of a densely packed harness than when it runs alone in free air?

    1. Because neighbouring wires reduce the heat dissipation Correct answer.
    2. Because the clamp pressure raises the insulation temperature rating
    3. Because the bundling increases the conductor resistance
    4. Because the voltage drop of each wire adds to that of the others

    Explanation

    In a bundle, the heat produced by adjacent wires raises the ambient temperature around each conductor, so less heat can be lost for a given conductor temperature rise. Manufacturers publish bundle derating factors for this reason.

  186. Question 186Electrical Cables and Connectors

    A wire bundle 20 mm in diameter is routed around a structural corner. Using the usual general guidance, what is the minimum bend radius?

    1. 200 mm Correct answer.
    2. 40 mm
    3. 500 mm
    4. 20 mm

    Explanation

    Common practice is that the bend radius of a wire bundle should be not less than ten times the bundle diameter, giving 200 mm for a 20 mm bundle. Tighter bends can damage insulation and put strain on the conductors.

  187. Question 187Electrical Cables and Connectors

    Where a power feeder and a low-level signal cable must run in the same area, what practice limits induced noise?

    1. Run them in separate bundles and cross at right angles Correct answer.
    2. Twist the power feeder around the signal cable
    3. Earth both cable shields to the same single pin
    4. Tie both cables into the same bundle using the same clamps

    Explanation

    Physical separation reduces capacitive and inductive coupling, and crossing at right angles minimises the length over which the fields can interact. Sharing a bundle or twisting the two together maximises coupling.

  188. Question 188Electrical Cables and Connectors

    How should a contact be installed into a rear-release connector?

    1. Push it in with pliers until it clicks
    2. Screw it clockwise until it bottoms
    3. Solder it into the insert
    4. Use the correct insertion tool Correct answer.

    Explanation

    Rear-release contacts are pushed in with the specified plastic or metal insertion tool, which guides the contact and allows the retention clip to engage without damage. Improper tooling deforms the clip or the insert and leads to contact push-out.

  189. Question 189Electrical Cables and Connectors

    After crimping a terminal onto a wire, where should you look to confirm the conductor is fully seated in the barrel?

    1. Through the inspection hole in the barrel Correct answer.
    2. At the colour band on the insulation
    3. At the bend radius of the wire
    4. Under the heat-shrink sleeve after shrinking

    Explanation

    The inspection hole lets you see the end of the conductor in the crimp barrel, proving it is fully inserted and that the crimp is in the correct zone. Once heat-shrink is fitted the joint can no longer be inspected.

  190. Question 190Electrical Cables and Connectors

    Which practice is correct when installing a coaxial cable?

    1. Keep within the minimum bend radius and do not crush it Correct answer.
    2. Coil the spare length into a tight loop to save space
    3. Flatten it against the structure with a cable tie
    4. Cut the braid back as far as possible to reduce capacitance

    Explanation

    Coaxial cable relies on a concentric geometry, so tight bends or crushing change the impedance and cause reflections and losses. The manufacturer's minimum bend radius must be respected and the cable secured without deforming the dielectric.

  191. Question 191Electrical Cables and Connectors

    Why is a cable clamped to structure close to a connector backshell?

    1. To keep the connector insert dry
    2. To increase the current rating of the wires
    3. To stop the crimps carrying the termination load Correct answer.
    4. To keep the connector shell at the same potential

    Explanation

    Clamping near the connector transfers the weight and vibration loads of the harness into the structure, so the contact crimps and backshell are not loaded in tension. This is the purpose of strain relief or a clamp within a short distance of the connector.

  192. Question 192Electrical Cables and Connectors

    What is the correct basis for selecting a heat-shrink sleeve to seal a splice on a 12 AWG wire?

    1. The expanded size must be larger than the wire, whatever the recovered size
    2. The sleeve must be long enough to cover the whole harness
    3. The sleeve must match the colour of the wire insulation
    4. The recovered diameter must be smaller than the smallest part it covers Correct answer.

    Explanation

    A heat-shrink sleeve must expand enough to pass over the splice and then recover to a diameter smaller than the smallest component it covers, so that it grips and seals. It must also be rated for the temperature and fluid environment of the zone.

  193. Question 193Electrical Cables and Connectors

    Why is an approved corrosion-inhibiting compound applied to a connector exposed to the atmosphere?

    1. To displace moisture and protect the contacts from corrosion Correct answer.
    2. To provide the electrical bonding path between shell halves
    3. To lubricate the coupling threads so they can be over-tightened
    4. To increase the conductivity of the contact plating

    Explanation

    The compound wets the surfaces and displaces water, forming a barrier that prevents corrosion of the contact plating and shell. It is not a conductive filler and does not replace correct torque or shell bonding.

  194. Question 194Electrical Cables and Connectors

    Which statement about splicing aircraft wires is correct?

    1. Splices are preferred to continuous wires wherever possible
    2. Splices must be positioned at the mid-point between two clamps
    3. Uninsulated solder splices are acceptable in unpressurised zones
    4. Only where approved, using an approved splice Correct answer.

    Explanation

    Splicing is permitted only where the maintenance manual or approved data allows it, must use an approved splice type, and the number of splices per wire is kept to a minimum. Continuous wire is always preferred where it can be installed.

  195. Question 195Electrical Cables and Connectors

    What does an insulation resistance test of a cable measure?

    1. The end-to-end resistance of the conductor
    2. The contact resistance of a mated connector pair
    3. The capacitance of the cable per metre
    4. The resistance between the conductor and ground Correct answer.

    Explanation

    An insulation resistance test applies a high test voltage between the conductor and ground, or between adjacent conductors, to check that the insulation is sound. The conductor is disconnected from equipment so that only the insulation path is measured.

  196. Question 196Electrical Cables and Connectors

    Why must a wire's current rating be reduced when the aircraft operates at high altitude?

    1. The wire expands and the crimp loosens
    2. The conductor resistance rises sharply with altitude
    3. Thinner air carries heat away less effectively Correct answer.
    4. The dielectric strength of the insulation falls to zero above 10 000 ft

    Explanation

    At altitude the reduced air density lowers convective cooling, so for the same current the conductor reaches a higher temperature. Ratings must therefore be derated to keep the insulation within its permitted temperature.

  197. Question 197Electrical Cables and Connectors

    A connector is fitted with size 20 contacts. Which wire gauge range is appropriate?

    1. 8 to 10 AWG
    2. 12 to 14 AWG
    3. 26 to 30 AWG
    4. 20 to 24 AWG Correct answer.

    Explanation

    The contact size denotes the barrel size, and a size 20 contact accepts wires in the 20 to 24 AWG range. Using a wire outside that range gives a poor crimp and poor retention.

  198. Question 198Electrical Cables and Connectors

    Why is the shield of a twisted pair carrying a low-level signal usually grounded at one end only?

    1. To increase the characteristic impedance of the pair
    2. To allow the shield to carry the signal return current
    3. To prevent circulating shield currents inducing noise Correct answer.
    4. To reduce the weight of the harness

    Explanation

    Grounding both ends of a shield creates a loop in which structural currents can flow, and those currents induce noise in the signal pair. A single-point ground still provides the electrostatic shielding without the circulating current.

  199. Question 199Electrical Cables and Connectors

    Why are wire bundles routed with a specified clearance from hydraulic and fuel lines?

    1. To allow the fluid lines to be removed without disconnecting the wiring
    2. So a leak cannot soak the harness and create a fire hazard Correct answer.
    3. To avoid the magnetic field of the fluid affecting the signals
    4. To keep the wires cool enough to carry full rated current

    Explanation

    Separation ensures that a leaking or broken fluid line cannot spray or soak a wire bundle, which could lead to arcing, insulation degradation or fire. It also protects the wiring from heat and from fluid attack.

  200. Question 200Electrical Cables and Connectors

    Why must the shell of a connector mounted on composite structure be bonded to aircraft earth?

    1. To provide a return path for the shield current only
    2. To ensure the contacts stay engaged under vibration
    3. To give a low-impedance earth path so the shell does not float Correct answer.
    4. To stop the connector insert from absorbing moisture

    Explanation

    Composite structure does not provide a conductive path, so an unbonded shell can float and act as an antenna or hold a hazardous potential, for example after a lightning strike. A low-impedance bond ties the shell and its shield terminations to the aircraft earth network.

Part-66 Module 6 flashcards

32 cards. Read the term and the definition here. The deck at the top of this page is optional.

Austenitic stainless steel
Non-magnetic chromium-nickel steels that cannot be hardened by heat treatment, only by cold work, and are susceptible to intergranular corrosion after heating between 425 and 870 °C.
Sensitisation of stainless steel
Chromium carbide precipitation at grain boundaries when austenitic stainless steel is held at 425–870 °C, depleting chromium locally and causing intergranular corrosion; stabilised grades 321 and 347 resist it.
Tempering
Reheating hardened steel to below the lower critical temperature to relieve internal stress and reduce brittleness, trading some hardness and strength for improved toughness and ductility.
2024 aluminium alloy
Copper-bearing aluminium alloy with high strength and fatigue resistance but poor corrosion resistance, usually clad with pure aluminium (Alclad) when used for aircraft skins.
7075 aluminium alloy
Zinc-magnesium-copper alloy, one of the highest-strength aluminium alloys, used for highly stressed structures; it is notch sensitive and prone to exfoliation and stress corrosion, so it is always protected.
Solution heat treatment
Heating an alloy to a temperature that dissolves the alloying elements into solid solution, then quenching rapidly to retain a supersaturated solid solution before ageing.
Delamination
Separation between plies of a laminated composite, typically caused by impact, voids or poor cure; detected by tap testing or ultrasonic inspection and seriously reducing compressive strength.
Aramid fibre
Para-aramid (Kevlar) fibre with high tensile strength and impact resistance but low compressive strength; it absorbs moisture and fuzzes when cut or machined.
Lightning strike protection
Fine aluminium or copper mesh, or a conductive filled coating, embedded in the outer ply of a composite structure to conduct lightning current and prevent resin damage.
Galvanic corrosion
Corrosion caused by electrical contact between dissimilar metals in the presence of an electrolyte, in which the more anodic metal corrodes, accelerated by a large cathode-to-anode area ratio.
Stress corrosion cracking
Cracking produced by the combined action of tensile stress and a specific corrosive environment, often along grain boundaries; seen in high-strength aluminium and stainless steels.
Exfoliation corrosion
Corrosion that spreads along grain boundaries parallel to the surface, forcing layers of metal apart; typical of 7075 aluminium and prevented by cladding and protective finishes.
Grip length
The thickness of material a fastener clamps, measured from under the head to the start of the thread; it must be selected so the nut engages the correct number of full threads.
Edge distance
The distance from the centre of a fastener hole to the nearest edge of the part, normally at least two hole diameters to prevent tear-out under load.
Hi-Lok fastener
Two-piece fastener with a threaded pin and a frangible-collar nut; the collar shears at a designed torque so a consistent preload is obtained without a torque wrench.
Flareless fitting
Tube fitting in which a ferrule is swaged onto the tube by the nut, requiring no flaring; used in high-pressure hydraulic systems and reassembled only a limited number of times.
37-degree flared tube
Standard aircraft rigid tube end where the tube is flared at 37 degrees to mate with a flared fitting cone; the flare must be smooth, concentric and free of cracks.
Flexible hose
Hose of rubber or PTFE with braided reinforcement, used where vibration or relative movement prevents rigid tubing; it must be supported and installed within its minimum bend radius.
Spring rate
The load required to deflect a spring by unit distance; for a helical spring k = Gd⁴/(8D³N), so the rate falls as the number of active coils increases.
Shot peening
Bombarding a spring surface with small media to induce compressive residual stress, improving fatigue life by counteracting the tensile stress at the surface.
Spring set (scragging)
Preloading a spring beyond its working stress to produce controlled permanent deformation, stabilising its free length so that it does not change in service.
Brinelling
Permanent indentation of a bearing raceway caused by static overload or by impact while the bearing is stationary, producing vibration and early failure once rotation begins.
Tapered roller bearing
Bearing with conical rollers and raceways that carries combined radial and thrust load in one direction; mounted in opposed pairs and requiring preload or clearance adjustment.
Backlash
The clearance between mating gear teeth that allows lubrication and thermal expansion; too little causes overheating and seizure, too much causes impact noise and wear.
Swaged cable terminal
End fitting attached to a control cable by cold pressing with a specified tool and die; the completed assembly is gauge-checked and proof-loaded and inspected for wire slippage.
Turnbuckle
Threaded barrel connecting two cable terminals, one with a right-hand and one with a left-hand thread, used to adjust control cable tension and rigging.
Cable proof load
A specified tensile load applied to a completed cable assembly to verify terminal security, applied before installation and below the design breaking load.
7x19 cable
Stranded control cable made of seven strands of nineteen wires each, giving high flexibility for runs passing over pulleys, unlike the stiffer 1x19 construction.
Wire gauge (AWG)
Numbering system in which a smaller AWG number denotes a larger conductor cross-section, with lower resistance and higher current-carrying capacity.
Crimped terminal
Electrical connection made by mechanically deforming a terminal onto a conductor with a calibrated tool; reliability depends on correct tool and die selection and a pull test.
Coaxial cable
Cable with a central conductor surrounded by dielectric, a braided shield and an outer jacket, carrying high-frequency signals while shielding them from electromagnetic interference.
Bonding
Electrically connecting aircraft structure and components to provide a low-resistance return path for current, preventing static build-up, arcing and interference.

Part-66 Module 6 study guide

Aircraft Materials - Ferrous

Core concepts

Ferrous airframe materials fall into three families: low-alloy steels such as 4130 chromium-molybdenum; corrosion-resistant steels, including the austenitic 300 series (302, 304, 321, 347), the martensitic 400 series (410, 440C) and precipitation-hardening grades such as 17-4PH; and maraging steels for highly stressed landing-gear parts.

Learn the heat-treatment vocabulary precisely. Annealing softens and relieves internal stress; normalising refines grain structure; hardening is austenitise-then-quench; tempering follows hardening to trade hardness for toughness. Case hardening gives a hard wear surface over a tough core: carburising diffuses carbon into low-carbon steel and requires a quench, while nitriding diffuses nitrogen at a lower temperature and needs no quench.

Traps in questions

Austenitic stainless steels cannot be hardened by heat treatment at all - only by cold working - and in the annealed condition they are essentially non-magnetic. Martensitic 400-series steels are magnetic and hardenable. Nitrided surfaces must not be ground or machined afterwards, because the thin case is the entire benefit. Quenching a high-strength forging to "fix" a defect destroys its temper. Never confuse hardening temperature with tempering temperature; a part overheated during tempering has lost strength permanently.

Worked example

A fastener is strongly attracted to a magnet, shows light surface rust after a damp winter and is specified as heat-treatable. Rule out 304 stainless immediately: it would be non-magnetic and non-hardenable. The material is a 400-series stainless or a low-alloy steel. Confirm from approved data - never by the magnet alone.

Aircraft Materials - Non-Ferrous

Core concepts

Aluminium alloys are the backbone of the airframe. 2024 (copper) has good strength and fatigue resistance but poor corrosion resistance, so sheet is usually Alclad - clad with a thin layer of pure aluminium that protects the core galvanically. 7075 (zinc) is the strongest common alloy and the least corrosion resistant. 6061 (magnesium-silicon) is weldable and corrosion resistant; 5052 is a good general-purpose sheet alloy. Tempers matter: O is annealed, T3 solution-treated and cold worked, T4 solution-treated and naturally aged, T6 solution-treated and artificially aged. Solution treatment is around 500 C followed by a quench; artificial ageing is done at a much lower temperature, and that ageing temperature is the ceiling for later paint-baking or repair heating.

Magnesium alloys are light but corrode readily and can burn; they need chromate-type protective treatments and isolation from other metals. Titanium has excellent strength-to-weight, poor thermal conductivity, galls easily and absorbs oxygen if heated in air, so welding needs inert-gas shielding. Copper alloys (brass, bronze) serve as bushes and fittings.

Traps in questions

Assuming stronger is always better: 7075-T6 is strong but less tough and less corrosion resistant than 2024-T3, which is why cladding and protection matter. Thinking anodising adds strength - it only builds a brittle oxide layer for corrosion resistance and paint adhesion. Confusing Alclad (pure aluminium) with plating.

Rule of thumb

2024 - copper, strong, needs cladding; 7075 - zinc, strongest, needs protection; 6061 - weldable, corrosion resistant. Never heat a heat-treated part above its artificial ageing temperature.

Aircraft Materials - Composite and Non-Metallic

Core concepts

A composite is reinforcement plus matrix. Reinforcements are glass (cheap, insulating, radar-transparent, moderate strength), aramid such as Kevlar (tough, good in tension, poor in compression, absorbs moisture) and carbon (stiffest and strongest, electrically conductive, brittle in impact). Matrices are usually epoxy, with phenolic used where low smoke and toxicity matter and polyester in light structures.

Know the lay-up language: warp and weft directions, bias, ply orientation, quasi-isotropic stacking, and sandwich construction with honeycomb (Nomex or aluminium) or foam cores. Understand pot life versus cure time, exotherm in thick laminates, vacuum bagging and autoclave cure, and the moisture absorption that demands dry storage of prepreg.

Traps in questions

Composites do not yield. There is no visible bending before failure, and a low-energy impact can leave barely a mark while halving residual strength - that is barely visible impact damage. Delamination and disbond are internal and need tap testing or NDT. Carbon fibre is conductive, forms a galvanic couple with aluminium and needs isolation and lightning-strike protection on outer skins. Drilling composites with a blunt or wrong-geometry bit causes delamination. Aramid is difficult to cut and machine. Glass is the choice for radomes because it is transparent to radar.

Worked example

A wing skin shows a small paint crack after a dropped tool. It is carbon/epoxy sandwich. Do not simply fill and paint: coin-tap the area for a change in sound indicating disbond, then compare the finding with the manufacturer's damage-tolerance limits before any repair decision.

Rule of thumb

If the fibre is cut, the strength is gone - never judge composite damage by appearance alone.

Corrosion

Core concepts

Corrosion needs an anode, a cathode, an electrolyte and a metallic path. Remove any one and the cell stops. Know the forms: general or surface attack; galvanic between dissimilar metals; pitting in passive metals such as stainless and aluminium; crevice attack in trapped moisture; intergranular and exfoliation in high-strength aluminium extrusions; filiform under paint; fretting at joint interfaces; stress corrosion cracking under sustained tensile stress plus a specific environment; and corrosion fatigue.

Prevention: protective finishes, primers and paints, sealants and wet assembly, drainage paths, plated or isolated fasteners, wash-downs and scheduled inspections. The anodic index ranks metals; the further apart two metals are, the faster the anodic one is consumed. Area matters enormously: a small anode joined to a large cathode corrodes very quickly.

Traps in questions

Aluminium is anodic to steel and sacrifices itself; magnesium is anodic to everything common. Mercury, chlorinated solvents and some fire extinguishants attack aluminium. Stainless is not immune - in chlorides it pits and suffers stress corrosion cracking. Stress corrosion needs a sustained tensile stress, so a part that corrodes only when loaded points to SCC. Exfoliation is typical of extruded 2024 and 7075. Fretting appears as dark powder at joints.

Rule of thumb

Keep the anodic index difference below about 0.25 V in a salt or humid environment and below about 0.50 V elsewhere, and never allow a small anode against a large cathode.

Worked example

A steel bolt in an aluminium plate in a wet bay corrodes the plate, not the bolt: aluminium is anodic and becomes the sacrificial anode, and because the anodic area is small the attack is rapid and localised.

Fasteners

Core concepts

Know the families: AN, MS and NAS bolts, machine screws, self-locking nuts (nylon insert and all-metal), castle nuts with cotter pins, shear nuts, and washers (AN960 flat, AN970 large area). Grip length must suit the joint; identification is by head marking and specification. Torque produces preload, and preload - not torque - holds the joint. Lubricated threads reach the same preload at a lower torque than dry threads, so always use the torque figure for the stated condition.

Rivets: 1100 (A, plain head), 2017-T3 (D, raised dot), 2024-T4 (DD, raised double dash), 2117-T4 (AD, dimple) and 5056 (B, raised cross). Blind rivets, Hi-Loks and lockbolts are used where access is one-sided.

Traps in questions

Threads must not lie in the bearing (shear) plane of the joint - a maximum of about one thread is tolerated. Do not over-torque to "make it safe". Self-locking nuts have limited re-use. Lockwire must be routed so that it pulls the fastener in the tightening direction, with a neat pigtail. Rivet spacing and edge distance are habitually tested: pitch about 3 to 4 diameters, edge distance at least 2 diameters, and the rivet diameter at least three times the thickness of the thickest sheet.

Rule of thumb

Edge distance 2D, pitch 3-4D, rivet diameter at least 3t, no thread in the shear plane.

Pipes and Unions

Core concepts

Rigid fluid lines use aluminium alloy tubing (3003 or 5052-O for low pressure, 6061-T6 for higher pressure), corrosion-resistant steel (304, 321) or titanium where temperature or pressure demands it. End fittings are either flared or flareless. The aviation flare is 37 degrees, formed with a proper flaring tool and checked for cracks, eccentricity and correct diameter. Flareless fittings use a ferrule that bites into the tube when the nut is torqued; once swaged the ferrule must not be re-used.

Flexible hoses range from low-pressure rubber to PTFE-lined, braided high-pressure assemblies, with defined minimum bend radii, a shelf life and a date of manufacture. Route lines with slack for expansion, clipped at approved intervals, clear of hot areas and structure, and never used to pull two components into alignment.

Traps in questions

A 45-degree automotive flare is not interchangeable with a 37-degree AN flare. A cracked or distorted flare must be cut off and re-made, never straightened. Do not reuse flareless ferrules or olive-type fittings. Aluminium tubing is not for high-pressure hydraulic systems. Hoses must not be twisted during installation - twist shortens life - and must not be bent tighter than the stated radius.

Rule of thumb

Keep bends to at least three tube diameters radius with no wrinkling or flattening, and support the line so it carries no weight and no vibration-induced stress.

Worked example

A leaking flare on a 3/8 in aluminium line is found to be oval. The correct action is to cut back past the damaged section, re-anneal if required, re-flare to 37 degrees, inspect, and pressure-test - not to tighten further.

Springs, Bearings and Transmissions

Springs

Core concepts

Spring types are helical compression, helical extension, torsion, leaf, Belleville (disc), wave and spiral. The controlling parameters are spring rate (load per unit deflection), preload or installed length, solid height for compression springs, and stress at the working deflection. Hooke's law applies within the elastic range: deflection is proportional to load, so doubling the load doubles the deflection until solid height or yield.

Manufacture and treatment matter for questions: springs are stress-relieved after coiling, and shot peening raises fatigue life by putting the surface into compression. Extension spring hooks and the inside of coils are stress raisers where cracks start. Springs are identified by part number and sometimes by colour coding, but colour alone means nothing without the approved chart.

Traps in questions

Never heat a spring to straighten or re-temper it, and never stretch an extension spring to increase its free length - both destroy the heat treatment. Electroplating can cause hydrogen embrittlement, so plated springs need a post-plating bake. A spring that has taken a set or lost tension is replaced, not adjusted. Do not cut coils to shorten a spring.

Rule of thumb

Rate k = load divided by deflection. Two identical springs in parallel give twice the rate; in series they give half the rate.

Worked example

An extension spring of rate 10 N/mm is installed with a 20 mm preload stretch. It carries 200 N working load: total extension = (200/10) = 20 mm plus the 20 mm preload = 40 mm, and the hook stress must be checked at that length.

Bearings and Transmissions

Core concepts

Bearings are plain (bush), rolling (ball, cylindrical roller, needle, tapered roller, spherical) or thrust types. Designation and clearance codes tell you the fit and internal clearance. The interference fit goes on the rotating race - normally the inner race on a rotating shaft - so the race cannot creep. Fit bearings by pressing on the race being fitted, or by controlled heating (typically not above about 120 C), never by hammering on the cage or balls. Sealed and shielded bearings differ: shields retain grease and keep out dirt but are not watertight.

Transmissions: spur gears are simple and noisy, helical gears run quietly with axial thrust, bevel gears turn the drive through an angle, worm drives give high reduction, and epicyclic (planetary) sets give large ratios in a small space. Backlash is the clearance between meshing teeth and must be within limits - too little causes overheating and seizure, too much causes impact loading.

Traps in questions

False brinelling arises from vibration in transit or storage, not from overload; true brinelling is from excessive static load. Pressing on the wrong race damages the bearing. Tapered roller bearings are adjusted by preload, not left slack.

Rule of thumb

Gear ratio = driven teeth divided by driving teeth; torque is multiplied by the same ratio while speed is divided by it.

Control Cables

Core concepts

Aircraft control cables are preformed, stranded constructions - mainly 7x7 (stiffer, more abrasion resistant) and 7x19 (more flexible, used round small pulleys). Terminals are swaged (Nicopress type), spliced, ball-ended or threaded, and each has its own proof load and inspection criteria. Turnbuckles provide rigging adjustment, with locking clips and safety wire, and a specified minimum thread engagement in the barrel.

Rigging tension is measured with a tensiometer and corrected to the reference temperature in the maintenance manual. Cables contract as they cool, so tension rises in a cold soak and falls when hot - a cable rigged correctly in a warm hangar can be dangerously tight at altitude in winter. Pulleys must be the correct size and in line, fairleads and pressure seals must not chafe, and the cable must not rub on structure.

Traps in questions

Turnbuckle terminals must never be backed out so far that the inspection hole is uncovered. Never solder a structural cable terminal. Broken-wire limits apply per strand and over a stated length - and corrosion inside a swaged terminal is a frequent hidden failure. Bird-caging means the strands have opened and the cable is unserviceable. Cables must not be used to spring components into alignment.

Rule of thumb

Inspect at every pulley, fairlead and terminal, check tension at the reference temperature, and replace any cable with a bird-caged, kinked or corroded section.

Electrical Cables and Connectors

Core concepts

Aircraft wire is selected by conductor size (AWG), strand count, insulation type and temperature rating, and by the current it must carry with acceptable voltage drop. Insulations include PVC, PTFE, ETFE/Tefzel, silicone and fibreglass; specifications such as MIL-W-22759 define the wire. Shielded and coaxial cables carry sensitive or high-frequency signals and need correct termination and grounding at the specified end only.

Connectors are circular or rectangular with pin and socket contacts, keyways to prevent mis-mating and positive contact retention. Crimping is the preferred termination, using the correct tool and a pull test; solder joints must be supported and never used as the mechanical joint. Bonding and grounding paths carry fault and static current and must be clean, protected and within resistance limits. Route bundles clear of fuel, oxygen and hydraulic lines, hot areas and control runs, supported at regular intervals and protected against chafing.

Traps in questions

Aluminium wire is prohibited in aircraft electrical systems. A bundle carrying many currents must be derated - bundled wires run hotter than single wires. Over-tightened clamps cut insulation; too small a bend radius damages conductors; wrong insertion tools spread or damage contacts. Mixing power and low-level signal wires in one bundle invites interference.

Rule of thumb

Allow a bend radius of at least ten times the bundle diameter, support the run at roughly 24 in intervals and near connectors, and leave a service loop at each termination.

Part-66 Module 6 cheat sheet

Quick reference

Aircraft Materials - Ferrous

  • SAE 4130 chromium-molybdenum low-alloy steel is the standard tube material for fuselage frames, engine mounts and landing gear; it is normally supplied normalised or normalised and stress-relieved.

  • Hardening steel requires heating above the upper critical temperature to form austenite, holding, then quenching in water, oil or air; tempering must follow immediately to restore toughness.

  • Austenitic stainless steels (301, 302, 304, 321, 347) are non-magnetic, cannot be hardened by heat treatment, and are strengthened only by cold working.

  • Grade 321 (titanium-stabilised) and 347 (niobium-stabilised) resist sensitisation and are preferred for exhaust systems and welded parts exposed to 425–870 °C.

  • Martensitic and ferritic stainless steels (410, 416, 440C) are magnetic and hardenable; 440C is used for bearings and high-hardness wear parts.

  • 17-4PH is a precipitation-hardening stainless steel: solution treated, machined, then aged (e.g. H900) to reach high strength with minimal distortion.

  • Main heat-treatment defects are decarburisation (loss of surface carbon) and quench cracking; hardness testing and magnetic-particle inspection reveal them.

  • Stainless steel must not be worked with carbon-steel tooling or wire brushes - embedded iron particles cause rust staining and galvanic attack on the surface.

Quick reference

Aircraft Materials - Non-Ferrous

  • 2024 (Al-Cu) offers high strength and fatigue resistance but poor corrosion resistance; airframe skins use Alclad 2024, which has a thin pure-aluminium cladding.

  • 7075 (Al-Zn-Mg-Cu) is the highest-strength common aircraft aluminium; it is notch-sensitive and prone to exfoliation and stress corrosion, so it is always protected.

  • 6061 (Al-Mg-Si) is weldable, corrosion resistant and heat treatable, used for tubing, fittings and moderately stressed structures.

  • Temper designations: O = annealed, H = strain hardened, T = heat treated; T3 = solution treated, cold worked and naturally aged; T6 = solution treated and artificially aged.

  • Magnesium alloys are the lightest structural metals but ignite readily; magnesium chips and dust are a fire hazard requiring dry powder or D-class extinguishing agents.

  • Ti-6Al-4V is an alpha-beta titanium alloy with a high strength-to-weight ratio and excellent corrosion resistance, used for engine parts, landing gear and fasteners.

  • Anodising grows a hard, corrosion-resistant oxide film on aluminium and provides a key for paint; it does not increase fatigue strength and thick coatings can reduce it.

  • Nickel-base alloys such as Inconel (heat resistant) and Monel (copper-nickel, seawater resistant) are used in exhaust systems and marine environments.

Quick reference

Aircraft Materials - Composite and Non-Metallic

  • Carbon-fibre/epoxy has the highest specific stiffness and strength but is brittle, electrically conductive and galvanically incompatible with aluminium, so isolation plies or sealant are used.

  • Aramid (Kevlar) has excellent tensile and impact properties but poor compressive strength and absorbs moisture; it fuzzes when machined and is hard to cut.

  • Glass fibre (E-glass, S-glass) is cheaper, electrically insulating and corrosion resistant; S-glass has higher strength where strength-to-weight matters.

  • Prepreg has a limited shelf life and out-life at room temperature; it is stored frozen and must be thawed in sealed bags to prevent condensation before lay-up.

  • Cure cycles control ramp rate, dwell temperature, pressure and vacuum; voids and porosity result from insufficient pressure or trapped volatiles.

  • Honeycomb cores give high stiffness-to-weight but can trap water; ingress is found by tap testing, X-ray or thermography and drained through weep holes.

  • Damage types include delamination, disbond, matrix cracking, fibre breakage, porosity and foreign objects; tap testing finds disbonds and ultrasonic C-scan finds internal defects.

  • Repairs use tapered scarf or stepped joints to restore the load path, and the repair ply orientation and stacking sequence must match the original layup.

Quick reference

Corrosion

  • A corrosion cell needs an anode, a cathode, an electrolyte and a metallic path; breaking any one of these (e.g. sealing faying surfaces) stops the attack.

  • Galvanic series from anodic to cathodic: magnesium, zinc, aluminium, cadmium, steel, lead, tin, brass, copper, passive stainless steel, titanium, graphite.

  • A small anode coupled to a large cathode is the worst case - a steel fastener in a large aluminium skin corrodes rapidly.

  • Pitting is localised breakdown of the passive film by chlorides; crevice corrosion occurs in stagnant trapped gaps such as under gaskets and clamps.

  • Intergranular and exfoliation corrosion follow grain boundaries; exfoliation lifts surface layers and is common in 7075 extruded and forged sections.

  • Stress corrosion cracking requires combined tensile stress and a specific corrosive environment; stress relief and protective finishes prevent it.

  • Fretting corrosion occurs at clamped joints under vibration, producing dark oxide debris (cocoa staining) that acts as a fatigue crack initiator.

  • Protection methods: cladding, anodising, chromate conversion coating, primer plus topcoat, sacrificial anodes, corrosion-inhibiting compound and faying-surface sealant.

Quick reference

Fasteners

  • AN bolt dash numbers give diameter in 1/16 in steps (AN3 = 3/16 in), with letter suffixes for drilled heads and thread length; head markings identify the manufacturer and type.

  • Grip length must match the clamped thickness so that no thread lies in the shear plane and the nut engages the specified number of full threads.

  • For riveted joints, edge distance should be at least 2D and pitch about 3D–4D; closer spacing risks tear-out and wider spacing reduces joint efficiency.

  • Solid rivet alloys: 2117-T4 (AD), 2017-T4 (D, refrigerated), 2024-T4 (DD), 7050 (E), 5056 (B); rivet strength must suit the material being joined.

  • Blind rivets (Cherrymax, Cherrylock, Avex) are used where only one side is accessible; hole size, grip range and stem break must match the rivet specification.

  • Hi-Lok and Hi-Shear fasteners use a collar that shears off at a preset torque, giving a controlled preload without using a torque wrench.

  • Torque figures apply to dry or lubricated threads and friction strongly affects the resulting preload; the nut is normally turned, not the bolt.

  • Safety wire must be routed so any tendency of the fastener to loosen pulls the wire tight, with 6–8 twists per inch and a 1/4 to 1/2 in pigtail.

Quick reference

Pipes and Unions

  • Rigid tubing materials: 6061-T6 aluminium for low-pressure systems, 304/321 corrosion-resistant steel for high pressure and heat, and titanium in some high-pressure circuits.

  • A 37° flared fitting requires a smooth, concentric, crack-free flare; over-tightening work-hardens the flare and leads to cracking in service.

  • Flareless (ferrule) fittings rely on a swaged ferrule biting the tube; they allow only a limited number of reassemblies and require the correct insertion depth.

  • Minimum bend radius is typically 2–3 times the tube diameter measured to the centreline; tighter bends cause ovality and wall thinning.

  • Tube support clamps are spaced per the maintenance manual, must not crush the tube, and use a rubber or plastic sleeve to prevent chafing and galvanic contact.

  • Flexible hose must be installed without twist, within its minimum bend radius, and supported at intervals; hose assemblies also carry a shelf life and installation date.

  • Hose assemblies are proof-pressure tested and marked with operating pressure, fluid type, date and part number; fire sleeves are fitted in designated fire zones.

  • Dissimilar metal tube and fitting combinations need a barrier (sealant, sleeve or insulating washer) to prevent galvanic corrosion at the joint.

Quick reference

Springs

  • Hooke's law applies within the elastic range; for a helical spring the rate is k = Gd⁴/(8D³N), where G is shear modulus, d wire diameter, D mean coil diameter and N the number of active coils.

  • Increasing wire diameter raises the rate by the fourth power; increasing coil diameter or the number of active coils lowers the rate.

  • Compression springs have open coils, tension springs have closed coils with hooks, torsion springs apply torque, and Belleville washers are disc springs giving high load in a short space.

  • Shot peening induces compressive residual stress at the spring surface and improves fatigue life; it must be done to the approved specification.

  • Scragging (presetting) removes residual set so the free length remains stable; a spring that has taken a permanent set in service is replaced, not re-used.

  • Common spring materials: music wire for small springs, chrome-vanadium and chrome-silicon for high-fatigue duty, 17-7PH stainless for corrosion and heat resistance.

  • End condition changes the number of active coils: plain, plain and ground, and squared and ground, the last being usual for compression springs.

  • Springs must not be stressed beyond their tested load and must be installed with the correct end orientation and without side loading or coil binding.

Quick reference

Bearings and Transmissions

  • Ball bearings carry radial loads plus moderate thrust; cylindrical rollers carry higher radial loads; tapered rollers carry combined radial and thrust loads in one direction.

  • Needle roller bearings fit a small radial envelope; thrust bearings carry axial load only and are usually paired with a radial bearing.

  • Bearing internal clearance allows thermal expansion; preloading opposed pairs removes clearance, increases stiffness and reduces vibration.

  • Failure modes: brinelling from static overload or impact, spalling from subsurface fatigue, fretting from micro-movement, and scoring from lubrication breakdown.

  • Correct fits are essential - an inner race spinning on a shaft wears the shaft; use the specified interference and heat for installation rather than impact force.

  • Gear types: spur for parallel shafts, helical for smoother quieter drive with thrust load, bevel for intersecting shafts, worm for high ratios, planetary for high torque density.

  • Gear ratio = teeth on driven gear ÷ teeth on driving gear; torque ratio is the inverse of the speed ratio.

  • Backlash is measured with a dial indicator at the pitch circle; belts and chains need correct tension and pulley or sprocket alignment.

Quick reference

Control Cables

  • Cable construction: 7x7 for general runs, 7x19 where maximum flexibility over pulleys is needed, 1x19 for stiff straight high-strength runs; construction and diameter are marked on the cable.

  • Swaged terminals (e.g. Nicopress) require the correct die, a go/no-go gauge check after swaging and a proof load test before installation.

  • Turnbuckles have one right-hand and one left-hand thread; a minimum number of threads must remain engaged at each end and the barrel must be safety-wired.

  • Pulleys must match the cable size and be fitted with guards to prevent the cable jumping out; fairleads guide cables through structure without chafing.

  • Cable tension is set with a tensiometer to the rigging figures and corrected for temperature, since tension changes with structure temperature.

  • Inspection looks for broken wires (limits per strand and per length), corrosion, kinks, flattening and pulley wear; a kinked or corroded cable is replaced, never repaired.

  • Cables must be lubricated with the specified cable lubricant and must not rub on structure, since chafing causes rapid wire wear and failure.

  • Constructional stretch settles after the first loadings, so rigging tensions are rechecked after initial flights or after cable replacement.

Quick reference

Electrical Cables and Connectors

  • In the AWG system a smaller number means a larger conductor; wire size is selected so that voltage drop at maximum current remains within the specified limit.

  • Insulation types include Tefzel (ECTFE), PTFE and polyimide (Kapton); polyimide is moisture sensitive and needs special handling and protection.

  • Crimped terminals are preferred to soldered joints in vibrating aircraft structures; use the correct tool and die, then inspect and pull-test the termination.

  • Connector families: keyed circular MS/EN connectors, D-sub miniature connectors for avionics and coaxial connectors for RF; pin numbering must match the wiring diagram.

  • Cable shielding (braid or foil) is grounded at the end(s) specified to control EMI; the shield must never be used as a current-carrying conductor.

  • Power and signal wiring is routed separately with the specified separation, supported by correct clamps and protected from chafing, heat and fluid.

  • Bonding resistance between structure and components is checked in milliohms with a bonding meter; a poor bond causes arcing, static build-up and interference.

  • Insulation resistance is measured with a megohmmeter at the specified test voltage and continuity with a low-resistance ohmmeter, never on a live circuit.

Part-66 Module 6 key terms

Annealing

A heat treatment that heats steel above its critical temperature, holds it there, then cools it very slowly, usually in the furnace. It softens the metal, relieves internal stresses and refines the grain structure.

Related: Case hardening (carburising), Martensitic stainless steel
Case hardening (carburising)

A process that adds carbon to the surface of low-carbon steel by heating it in a carbon-rich atmosphere, then quenching and tempering. The result is a hard, wear-resistant skin over a tough, shock-resistant core.

Related: Annealing, Martensitic stainless steel
Austenitic stainless steel

A chromium-nickel stainless steel, usually about 18% chromium and 8% nickel. It is non-magnetic, cannot be hardened by heat treatment, work-hardens rapidly and has excellent corrosion resistance. Types 304 and 316 are common.

Related: Martensitic stainless steel, Stress corrosion cracking
Martensitic stainless steel

A stainless steel with more carbon and little or no nickel, magnetic and hardenable by quenching and tempering. It gives high strength and wear resistance but poorer corrosion resistance, and is used for cutlery and some aircraft parts.

Related: Austenitic stainless steel, Case hardening (carburising)
2024 aluminium alloy

An aluminium-copper-magnesium alloy with high strength and good fatigue resistance, widely used for aircraft skins and structures. Its corrosion resistance is poor, so it is usually clad with pure aluminium (Alclad) or painted.

Related: 7075 aluminium alloy, Galvanic corrosion
7075 aluminium alloy

An aluminium-zinc-magnesium-copper alloy, one of the strongest wrought aluminium alloys, used for highly stressed parts such as wing spars and fittings. It has low corrosion resistance and is normally protected by cladding, anodising or paint.

Related: 2024 aluminium alloy, Galvanic corrosion
Titanium alloy

A light, very strong metal with outstanding corrosion resistance and good performance at elevated temperature. It is used for engine parts and highly loaded structures, but it is expensive, difficult to machine and its fine chips are a fire hazard.

Related: Magnesium alloy, Galvanic corrosion
Magnesium alloy

The lightest common structural metal, used for castings such as gearbox housings and wheels. It corrodes easily, needs protective treatment, and its turnings and dust can ignite and burn fiercely.

Related: Galvanic corrosion, Titanium alloy
Matrix (resin)

The plastic material, usually epoxy or polyester resin, that surrounds and bonds the reinforcing fibres in a composite. It carries load between fibres, protects them from moisture and damage, and holds the part's shape.

Related: Prepreg, Delamination
Prepreg

Composite material supplied as fibre cloth or tape already impregnated with a controlled amount of uncured resin. It must be stored cold, has a limited out-life, and is laid up and cured in an autoclave.

Related: Matrix (resin), Honeycomb core
Honeycomb core

A lightweight core of thin metal or composite sheet formed into hexagonal cells, bonded between two skins to make a sandwich panel. It gives very high stiffness and strength for very little weight, but trapped water can cause damage.

Related: Delamination, Prepreg
Delamination

Separation between the layers of a laminated composite, caused by impact, poor bonding, trapped moisture or manufacturing defects. It reduces strength and stiffness and is often found by tapping or ultrasonic inspection.

Related: Honeycomb core, Matrix (resin)
Galvanic corrosion

Corrosion that occurs when two different metals are in electrical contact in the presence of an electrolyte. The less noble metal becomes the anode and corrodes faster; the further apart the metals in the galvanic series, the worse it is.

Related: Sacrificial anode, Bonding
Sacrificial anode

A piece of less noble metal, such as zinc or magnesium, deliberately attached to a structure so that it corrodes instead of the protected metal. It is used in tanks, pipelines and immersed or buried parts.

Related: Galvanic corrosion
Stress corrosion cracking

Cracking of a metal caused by the combined effect of a sustained tensile stress and a corrosive environment, for example chlorides on stressed stainless steel. The cracks are often fine and hard to find, and failure can be sudden.

Related: Austenitic stainless steel, Galvanic corrosion
Fretting corrosion

Damage at the contact surfaces of two parts that rub slightly under load, such as riveted joints or bearing seats. It produces fine dark oxide debris, loosens the joint and can start fatigue cracks.

Related: Close-tolerance bolt, Galvanic corrosion
Grip length

The thickness of material that a bolt or rivet clamps together, measured under the head and not including washers. Choosing the correct grip length ensures the unthreaded shank, not the threads, lies in the shear plane.

Related: Close-tolerance bolt
Close-tolerance bolt

A bolt whose shank is machined to a tight tolerance so it fits closely in a reamed hole. It carries shear loads and prevents movement between the joined parts, giving a stronger, more fatigue-resistant joint.

Related: Grip length, Fretting corrosion
Lockwire

A stainless steel wire threaded through drilled heads or nuts and twisted in the tightening direction so vibration cannot loosen the fastener. It is used on critical fasteners where self-locking features alone are not enough.

Related: Self-locking nut
Self-locking nut

A nut with a built-in locking feature, such as a nylon insert or a deliberately deformed thread, that resists loosening under vibration. Its locking action must be checked, and it may only be reused a limited number of times.

Related: Lockwire
37-degree flare

The conical end formed on a rigid tube so that, when the B-nut is tightened, the flare is clamped against a matching cone on the fitting. This seals the joint without a separate sleeve and is standard on aircraft flared fluid lines.

Related: Flareless fitting, Bend radius
Flareless fitting

A tube fitting in which a separate ferrule (sleeve) is crushed onto the plain end of the tube by the nut, sealing and gripping it. No flaring is needed, but assembly and inspection need care.

Related: 37-degree flare, Bend radius
Bend radius

The smallest curve a tube or cable may be formed into without kinking, wrinkling or losing strength. Too sharp a bend restricts flow, stresses the material and can crack or flatten the bore.

Related: 37-degree flare, Fairlead
Hose ferrule

A metal sleeve, swaged or screwed onto the end of a flexible hose, that clamps the hose onto the insert fitting. It must match the hose and fitting type and be correctly crimped to prevent leaks or blow-off.

Related: Bend radius, 37-degree flare
Spring rate

The load needed to compress or extend a spring by a given distance, usually stated in newtons per millimetre. A higher rate means a stiffer spring; rate depends on wire diameter, coil diameter and number of coils.

Related: Compression spring, Torsion spring
Compression spring

A helical spring designed to resist a pushing force, shortening under load and returning to its free length when released. It is used in valves, controls and landing gear, and must not be compressed to solid height in service.

Related: Spring rate, Shot peening
Torsion spring

A spring that works by twisting, storing energy as its ends are rotated relative to each other. It is used for hinges, control surfaces and return mechanisms, and must be fitted so that it is loaded in the correct direction.

Related: Spring rate
Shot peening

A process that bombards a metal surface with small round particles to induce compressive stress in the surface layer. On springs and other highly stressed parts it greatly improves resistance to fatigue cracking.

Related: Compression spring
Tapered roller bearing

A bearing with conical rollers running between conical races, able to carry both radial and axial loads. It is used for wheels, gearboxes and shafts and is normally fitted as a matched pair with a set preload.

Related: Preload, Backlash
Preload

The deliberate axial force applied during assembly to a bearing, bolt or joint so the parts stay tight in service. Correct preload removes internal clearance, reduces vibration and stops rolling elements from skidding.

Related: Tapered roller bearing, Backlash
Backlash

The small amount of free movement between the teeth of two meshed gears, or between a shaft and its bearing, when they are not loaded. Too little causes overheating and wear; too much causes noise and lost motion.

Related: Preload, Tapered roller bearing
Plain bearing

A bearing with no rolling elements, just a sleeve or bush of bearing material running against a shaft and separated by a film of oil or grease. It is simple, quiet and cheap but needs reliable lubrication.

Related: Tapered roller bearing
Swaging

The process of compressing a metal sleeve onto a cable end to form a permanent eye or terminal. The correct die, insertion depth and proof load are essential, because a badly swaged terminal can pull off.

Related: Turnbuckle, Fairlead
Turnbuckle

An adjustable connector with left-hand and right-hand threads at its two ends, used to tighten and rig control cables. After adjustment it must be locked, and a minimum number of threads must stay engaged.

Related: Swaging, Fairlead
Bowden cable

A flexible cable running inside an outer conduit, used where the load path must curve, as in cockpit controls for vents or brakes. The conduit carries the reaction force, so the inner cable can work in both push and pull.

Related: Fairlead, Swaging
Fairlead

A guide, usually a grooved block or bush, that leads a cable or rod along the correct path and stops it rubbing on structure. Fairleads also keep a cable from jumping off its pulley.

Related: Bowden cable, Bend radius
AWG (American Wire Gauge)

A standard system for stating wire size in which the number decreases as the wire gets thicker. Each gauge has a defined cross-sectional area and current rating, and a replacement wire must be the same size or larger.

Related: Crimp terminal, Insulation resistance
Crimp terminal

An electrical terminal attached to a wire by mechanically compressing it with a tool rather than by soldering. A correct crimp needs the right tool, the right terminal for the wire size, and a pull check.

Related: AWG (American Wire Gauge), Bonding
Bonding

The electrical connection of metal parts of an aircraft to each other and to the structure, giving a low-resistance path. It prevents static build-up, provides a current return path and reduces radio interference and lightning damage.

Related: Insulation resistance, Galvanic corrosion
Insulation resistance

A measurement of how well the insulation of a wire, cable or connector resists leakage current, taken with a megohmmeter at a specified test voltage. A low reading indicates moisture, contamination or damaged insulation.

Related: Bonding, AWG (American Wire Gauge)

Part-66 Module 6 study plan

8 weeks · About 7 hours per week

Week 1

Electrical Cables and Connectors

  • Classify aircraft electrical wire by insulation type, temperature rating and current-carrying capability, and state where each is used.

  • Compare crimped, soldered and welded terminations and list the acceptance and rejection criteria for each.

  • Explain connector shell, insert, keying and contact-retention features and how they prevent mismating.

  • Describe shielding, bonding and grounding requirements for cable runs, and calculate allowable voltage drop for a given run length.

  • Diagnose typical in-service cable and connector faults: chafing, arc tracking, cold solder joint, over-crimped barrel, contact back-out.

Your checkpoint

A one-page cable-routing and connector inspection checklist plus a 20-item self-test scored at 100% on termination defect identification.

Week 2

Aircraft Materials - Ferrous

  • Distinguish mild steel, low-alloy steel and the stainless families by composition and typical aircraft application.

  • Explain annealing, normalising, hardening and tempering, and predict the effect of each on strength, hardness and ductility.

  • Interpret a steel specification callout and state the heat-treatment condition it implies and its handling constraints.

  • Identify nitriding, carburising and induction hardening, and select the appropriate one for a stated wear or fatigue requirement.

  • Describe inspection methods for heat-treatment defects and the hydrogen-embrittlement risk introduced by plating.

Your checkpoint

An 8-alloy by 5-attribute ferrous comparison matrix plus a 15-question quiz scored at 80% or better.

Week 3

Corrosion

  • Classify corrosion findings as galvanic, pitting, intergranular, exfoliation, crevice, stress-corrosion, fretting or filiform.

  • Predict which member of a dissimilar-metal couple becomes the anode, and select a mitigation that is valid for that couple and location.

  • Explain the electrochemical cell, naming the roles of electrolyte, potential difference and anode-to-cathode area ratio.

  • Locate the highest-risk inspection zones on an airframe and choose a detection method suited to each corrosion type.

  • Apply protective schemes in the correct sequence: surface conversion, primer, topcoat, sealant, sacrificial or barrier protection.

Your checkpoint

A fault-finding flow chart mapping 10 corrosion findings to probable cause, detection method and corrective action.

Week 4

Aircraft Materials - Non-Ferrous

  • Sort aluminium alloys into heat-treatable and non-heat-treatable series and state a typical use for each.

  • Explain the Alclad concept and its effect on corrosion resistance, strength and repairability.

  • Relate solution treatment, quenching, natural ageing and artificial ageing to the resulting mechanical properties.

  • Compare magnesium, titanium, copper and nickel alloys for aircraft use, including handling and machining hazards.

  • Decode temper designations and explain what each suffix tells the technician about condition.

Your checkpoint

A timed 30-question mixed mock covering 6.1, 6.2, 6.4 and 6.9, scored at 75% or better.

Week 5

Aircraft Materials - Composite and Non-Metallic

  • Identify reinforcement and fibre types and match each resin system to its service temperature and handling requirement.

  • Describe wet lay-up, prepreg and autoclave curing, and name the defects each process is prone to.

  • Differentiate laminate defects: void, delamination, disbond, fibre breakage, porosity and wrinkle.

  • Select an inspection technique (tap test, ultrasonic, radiography, visual) for a stated defect and state its limitations.

  • Describe the handling and installation constraints of transparencies, sealants and adhesives used on non-metallic structures.

Your checkpoint

A defect-diagnosis table covering 12 composite and non-metallic defects with inspection method and accept/reject reasoning.

Week 6

Fasteners

  • Identify thread forms, thread series and fit classes, and determine the correct grip length and grip range for a joint.

  • Select the correct fastener and locking device for a stated joint, access condition and vibration environment.

  • Describe installation and removal procedures for solid rivets, blind fasteners and proprietary structural fasteners.

  • Explain torque, preload and the effect of lubrication on applied torque, and compute a worked preload example.

  • Recognise failure modes: thread stripping, galling, hydrogen embrittlement and fatigue cracking from poorly prepared holes.

Your checkpoint

A 25-item fastener identification and selection quiz scored at 100%, supported by a torque/preload worked-example sheet.

Week 7

Pipes and Unions & Springs, Bearings and Transmissions

  • Differentiate rigid and flexible fluid lines, and identify fittings, unions, flares and their pressure and temperature limits.

  • Describe correct tube fabrication: bend radius limits, flaring, annealing before forming and B-nut torque practice.

  • Classify springs by type and explain rate, preload, set, and the effects of temperature and fatigue.

  • Classify bearings by load direction and describe inspection for brinelling, false brinelling, fretting and lubrication failure.

  • Describe gear types, ratio calculation, backlash and the inspection points for belt, chain and shaft drives.

Your checkpoint

Two one-page job aids - fluid-line fabrication, and a bearing/gear defect atlas - each validated by a 10-question quiz at 80% or better.

Week 8

Control Cables

  • Describe control-cable construction, swaged and spliced terminations, and the inspection technique for each.

  • State rejection criteria for broken wires, wear, corrosion, kinks, and pulley and fairlead deterioration.

  • Explain rigging, cable tension measurement and temperature compensation during rigging checks.

  • Re-attempt every previously missed question across all nine domains and close each identified gap.

  • Sit a full-length timed mock across all domains and analyse the result by domain.

Your checkpoint

A full 60-question timed mock scored at 80% or better overall with no single domain below 70%.

Milestones

Week 4: Explain a corrosion finding end-to-end (mechanism, detection, treatment) without notes, and score 75% or better on the mixed mock covering the four heaviest domains.

Week 6: Select and justify the correct fastener and locking device for five different joints with no errors, and score 100% on the fastener identification quiz.

Week 8: Complete the 60-question timed mock at 80% or better overall with a minimum of 70% in every one of the nine domains.

Part-66 Module 6 exam day

Your checklist

Valid photo ID

Bring the same identity document you used at registration (passport or national ID card). Confirm with the provider which forms of ID they accept and whether a second document is required.

Examination admission / booking confirmation

Printed or on-phone copy of your appointment confirmation, candidate number, or admission letter if your provider issues one. Check the exact arrival time and room on it.

Provider-approved calculator

Module 6 involves material properties, densities, and stress/load arithmetic. Confirm with the provider whether calculators are permitted and which models are banned (typically programmable or networked devices).

Nothing on your person that could be treated as unauthorised material

Leave notes, revision cards, smart watches, and phones in the locker or at home. Ask the invigilator where to store personal items before you sit down.

Stationery if allowed

Some centres supply everything; others allow only the pen/pencil they issue. Confirm with the provider whether you may bring pens, pencils, or an eraser.

Confirm the exam format and duration

Module 6 is normally a multiple-choice question paper delivered on paper or by computer. Confirm with the provider the number of questions, time allowed, and the pass mark before exam day so you can pace yourself.

Confirm the permitted reference material

Part-66 knowledge examinations are normally closed-book. Ask the provider explicitly whether any data sheets, formula sheets, or tables are supplied on the day.

Re-read your own summary of weak topics

One page only, reviewed the day before and then put away: material properties, corrosion types, fastener identification, and hardware marking conventions are the usual slip points in Module 6.

Plan the journey and arrive early

Aim to be at the centre well before the start time so that ID checks and seating do not eat into your exam time. Check local transport and parking in advance.

Know your provider's late-arrival and absence rules

Ask in advance what happens if you are delayed or fall ill, and whether a re-sit can be booked and at what cost.

Rest and eat sensibly beforehand

Avoid a last-minute cramming session the morning of the exam; a settled, alert candidate outperforms an exhausted one on recall-based multiple choice.

Read the candidate instructions sent by the provider

Providers issue a regulations or candidate handbook covering conduct, malpractice, and results. Read it in the final week rather than on the day.

Plan the day

72 hours before

Finish active revision: work through practice questions on materials, corrosion, fasteners, bearings, seals, and control cables. Stop learning new topics; consolidate what you already know.

72 hours before

Confirm the logistics: exact address, arrival time, room, ID requirements, and whether calculators or stationery are permitted. Contact the provider if anything is unclear.

72 hours before

Get three full nights of normal sleep. Do not trade sleep for extra revision in the last stretch.

24 hours before

Do one light review pass over your own summary sheet and the marking/identification conventions you find hardest. Then stop.

24 hours before

Prepare and lay out everything on the checklist: ID, confirmation, permitted calculator, transport tickets, and money for the journey.

24 hours before

Check travel plans against any disruption notices and set two alarms. Eat a normal meal and go to bed at your usual time.

Morning of

Eat breakfast, avoid heavy caffeine if you are not used to it, and leave with enough margin to arrive early.

Morning of

Do not open new material. At most, skim your one-page summary while travelling, then put it away before entering the centre.

On arrival

Present your ID, store personal items as instructed, listen to the invigilator's briefing, and check that your question paper or workstation is the correct module and version before starting.

During the test

Read the candidate instructions on the paper or screen. Note the number of questions and the time allowed, and work out roughly how long you can spend on each.

During the test

First pass: answer everything you are confident about. Second pass: return to the harder items and eliminate options where possible. Leave nothing blank unless the marking scheme penalises wrong answers, which you should confirm in the instructions.

During the test

Watch the clock at the halfway point and near the end, and reserve a few minutes to check that every question has a recorded answer and your candidate details are correct.

After the test

Hand in all materials as instructed, collect your belongings, and note the provider's stated timescale and process for results and any re-sit.

Rules to check

  • Bring the identity document specified by your provider and keep it on the desk throughout; you will normally be refused entry without acceptable photo ID.

  • Follow the invigilator's instructions at all times, including on where to place bags, phones, and outer clothing, and on when you may leave your seat.

  • Treat the examination as closed-book unless the provider has confirmed otherwise in writing; possession of unauthorised notes or devices is normally treated as malpractice.

  • Raise your hand and wait for the invigilator if you need to leave the room, feel unwell, or have a problem with your paper or workstation. Confirm the provider's rules on toilet breaks, as escorted breaks may be allowed but the clock usually keeps running.

  • Do not communicate with other candidates once the examination has begun, and do not attempt to copy from or share answers with anyone.

  • Record an answer for every question unless the provider's instructions state that incorrect answers are penalised; confirm this before you start.

  • If you believe a question is defective, note the question number and report it to the invigilator after the examination rather than guessing at what was intended.

  • Confirm with your provider the pass mark, the number of questions, and the rules on re-sits and result appeals; these are set by the examining organisation and the competent authority, not by general assumption.

Part-66 Module 6 FAQ

How many Part-66 Module 6 practice questions are available?

The practice set has 200 Part-66 Module 6 questions. Each one includes the choices, the correct answer, and an explanation, and the set is free to read with no signup.

How many Part-66 Module 6 flashcards are available?

The flashcard set has 32 Part-66 Module 6 cards. Each card shows the term and its definition.

Which topics does the Part-66 Module 6 study material cover?

The Part-66 Module 6 study material has 9 sections, including Aircraft Materials - Ferrous, Aircraft Materials - Non-Ferrous, and Aircraft Materials - Composite and Non-Metallic.

What format facts does the catalog list for the Part-66 Module 6 exam?

The catalog lists these item types: multiple choice for the Part-66 Module 6 exam.