CWI overview

  • 200 practice questions
  • 32 flashcards
  • 3 study guide topics
  • 38 key terms

What you'll study

  • Welding Fundamentals and Processes (Part A)33%
  • Practical Inspection and Nondestructive Examination (Part B)33%
  • Codes, Standards, and Acceptance Criteria (Part C)34%

The AWS Certified Welding Inspector (CWI) is one of the welding industry's most recognized professional credentials, issued by the American Welding Society to individuals who can demonstrate a working command of welding processes and of the standards that govern them. A CWI determines whether a weldment meets acceptance criteria, handles qualification records, oversees non-destructive testing, and confirms that proper materials are available during testing, which places the inspector at the center of fabrication quality control. The credential suits experienced welders, quality and fabrication personnel, and engineering or supervisory staff moving into inspection work. Candidates must document qualifying welding experience; those still short of that requirement can begin with the Certified Associate Welding Inspector (CAWI) credential. Exam content spans process fundamentals, practical inspection and nondestructive examination methods, and code application and acceptance criteria, with the authoritative outline and reference list published in the AWS Program Exam and Reference Guide. Preparation is flexible: AWS offers in-person seminars, online instructor-led training, self-paced online courses, and custom seminars built around an organization's needs, delivered at locations across the United States and through international training programs.

Common mistakes

Reading the digits of SMAW electrode classifications (e.g., E7018 vs E8018 vs E7024) by position but swapping what the third and fourth digits mean - treating the position digit as the coating/current-type digit and vice versa.

The string of digits is memorized as a chant during study instead of being decoded from the AWS filler metal specification, so under time pressure the middle digits blur together.

What to do instead

Build a one-page decoder card and force yourself to say it out loud for each electrode: E = electrode, first two digits = minimum tensile strength in ksi, third digit = usable position (1 = all position, 2 = flat and horizontal fillet, 3 = flat only), fourth digit = coating and current type (e.g., 8 = low-hydrogen, AC or DCEP). Drill 20 random classifications until decoding is automatic.

Computing heat input without the unit-conversion factor - e.g., multiplying amps by volts and dividing only by travel speed, or plugging travel speed in inches per minute but reporting the answer as if it were kJ/mm.

The formula is remembered as 'amps times volts over travel speed' with the 60 and the 1000 dropped, because the candidate never wrote out the units on both sides of the equation.

What to do instead

Write the full expression every time: heat input (kJ/in) = [60 × amperage × voltage] ÷ [1000 × travel speed in in/min]. Carry the units through the calculation and cancel them; then sanity-check the result against a known reference value (MIG welding at 200 A, 25 V, 10 in/min gives about 30 kJ/in).

Choosing a process or transfer mode by its general reputation ('spray is fastest', 'short circuit is for thin metal') without connecting it to the specific joint, position, thickness, or filler requirement described in the question.

Process knowledge was learned as isolated facts per chapter, so the candidate cannot match a process characteristic (spray transfer requires argon-rich gas and does not work out of position; short-circuit transfer is limited to thin material; FCAW self-shielded needs no external gas) to the constraint the question actually imposes.

What to do instead

For each of SMAW, GMAW (short-circuit, globular, spray, pulsed), FCAW (self-shielded vs gas-shielded), SAW, and GTAW, make a grid of position capability, thickness range, shielding medium, deposition rate, and typical defects. Answer process questions by eliminating options that violate a stated constraint rather than by picking the most familiar name.

Answering preheat questions by recalling a single thickness threshold or treating preheat as interchangeable with interpass temperature, instead of determining preheat from base metal chemistry (carbon equivalent), thickness, and hydrogen level of the process.

Preheat tables are memorized as isolated numbers and the underlying logic - that preheat and interpass control hydrogen-assisted cracking by slowing cooling rate - is never internalized.

What to do instead

Learn the causal chain: higher carbon equivalent or thicker section means faster heat extraction and greater hardenability, which raises cracking risk; low-hydrogen processes and higher preheat reduce it. Be able to state that preheat is the minimum temperature before welding while interpass is the maximum allowed between passes, and that both appear as essential variables on the WPS.

Using a fillet weld gauge or bridge cam gauge on the wrong scale or wrong feature - reading the leg when the question asks for throat, holding the gauge on a curved or misaligned surface so it rocks, or using a gauge whose face was never verified against a zero.

Instrument practice was read about rather than physically rehearsed, so the candidate does not have a habit of identifying which edge of the gauge contacts the weld face versus the plate.

What to do instead

Practice on a set of known-size fillet specimens until you can state before measuring which gauge and which scale you will use and why: leg length on the appropriate scale, throat as the theoretical 0.707 × leg for a equal-leg 45-degree fillet, with the gauge seated flat on both members. Verify your tools before the exam and keep the gauge perpendicular to the weld axis.

On penetrant and magnetic particle questions, judging indications without applying the technique controls - skipping dwell time, ignoring surface temperature limits, or on MT magnetizing parallel to the expected discontinuity instead of perpendicular to it.

The candidate focuses on 'did an indication show up' and treats the method as a yes/no test, forgetting that PT requires a properly cleaned surface and a dwell period within a temperature range (commonly about 50–125 °F), and that MT only detects discontinuities that intercept the magnetic flux at a significant angle.

What to do instead

Memorize the technique controls as a checklist for each method: surface prep, temperature range, dwell/development time, and field direction (perpendicular to the long axis of the expected flaw), plus AC for surface-breaking and DC for slightly subsurface indications with a yoke. Practice sorting indications into relevant, nonrelevant, and false before deciding accept or reject.

Taking a measurement or reading an indication and then guessing at acceptance ('that looks like a lot of undercut') instead of locating the written limit and comparing the measured value against it in the same step.

Practical inspection is treated as pure measurement, and memorized numbers are fuzzy, so the candidate either under-rejects or over-rejects on the basis of appearance.

What to do instead

Adopt a fixed two-step script for every practical item: measure, then cite. Record the number with units, state the applicable limit from the code table, and state the comparison explicitly ('2 mm undercut measured against a 1 mm allowable, therefore reject'). Use the same script in study so it becomes automatic in the exam.

Treating the open-book code portion as a reading test - starting at the table of contents and paging forward through the standard to answer each question, running out of time with questions unanswered.

Candidates assume the open-book format removes the need for memorization, so they never learn the structure of the code or build a navigation scheme before exam day.

What to do instead

Before the exam, tab the clauses and tables you will use most (scope, prequalification, visual acceptance criteria, NDE acceptance criteria, qualification of inspectors) and practice timed drills where you locate a specific clause or table in under 30 seconds using the index and tab set. Answer code questions by index lookup, never by sequential paging.

Applying the wrong acceptance criteria set - using visually inspected acceptance limits to judge an NDE indication, or applying statically loaded structure criteria to a cyclically loaded structure.

All acceptance numbers are stored as one undifferentiated list, and the candidate does not first establish which loading condition and which inspection method the question specifies.

What to do instead

Before touching any acceptance limit, write down the two qualifiers you identified from the question: inspection method and loading condition. Then open the specific table for that combination rather than the first acceptance table you find. Practice by sorting a mixed set of 25 acceptance questions into method and loading categories before answering any of them.

Confusing essential, nonessential, and supplementary essential variables on a WPS/PQR, and therefore failing to recognize when a change in the process, filler, position, thickness, or preheat requires requalification.

The variable categories are memorized as a list without the governing idea - that essential variables affect mechanical properties, nonessential ones do not, and supplementary essential ones matter only where notch toughness is required.

What to do instead

Learn the three-tier logic first, then attach examples to each tier (amperage and voltage are typically nonessential; filler classification and preheat are essential; impact testing requirements make variables such as heat input supplementary essential). Drill change scenarios and ask one question each time: does this change alter mechanical properties, and is toughness required?

Exam requirements can change. Confirm current details with the exam provider.

CWI practice

200 questions. Each one lists the choices, the correct answer, and an explanation. With JavaScript, this list opens one question at a time. The checker at the top of this page saves progress in this browser when it is available.

  1. Question 1Welding Fundamentals and Processes (Part A)

    In the SMAW electrode classification E7018, what does the number 70 represent?

    1. Typical deposition rate of 70 percent
    2. Minimum yield strength of 70,000 psi
    3. Minimum tensile strength of 70,000 psi Correct answer.
    4. Maximum carbon content of 0.70 percent

    Explanation

    The first two digits of an E70xx electrode give the minimum as-welded tensile strength in ksi, so E70 means 70,000 psi minimum tensile strength. Yield strength and composition are not encoded in those digits. The suffix digits describe position and coating/current.

  2. Question 2Welding Fundamentals and Processes (Part A)

    Which joint configuration places two members at approximately 90 degrees in the form of a T?

    1. Lap joint
    2. Corner joint
    3. T-joint Correct answer.
    4. Butt joint

    Explanation

    A T-joint has one member perpendicular to the face of the other, forming the stem and flange of a T. Butt joints align members end to end, lap joints overlap parallel surfaces, and corner joints meet at an edge.

  3. Question 3Welding Fundamentals and Processes (Part A)

    In the AWS position designation, a groove weld made in the horizontal position is identified as:

    1. 4G
    2. 3G
    3. 2G Correct answer.
    4. 1G

    Explanation

    AWS groove weld positions use 1G flat, 2G horizontal, 3G vertical, and 4G overhead. The horizontal position is therefore 2G.

  4. Question 4Welding Fundamentals and Processes (Part A)

    On a welding symbol, a weld placed on the same side as the reference line arrow is:

    1. Welded in the field
    2. Welded on the other side
    3. Welded all around
    4. Welded on the arrow side Correct answer.

    Explanation

    The side of the joint to which the arrow points is the arrow side; a symbol below the reference line denotes an arrow-side weld, while a symbol above denotes the other side.

  5. Question 5Welding Fundamentals and Processes (Part A)

    An E6013 electrode is designed to deposit weld metal with a minimum tensile strength of:

    1. 60,000 psi Correct answer.
    2. 13,000 psi
    3. 6,000 psi
    4. 70,000 psi

    Explanation

    The first two digits of the E60xx classification specify minimum tensile strength in ksi, so E6013 deposits at least 60,000 psi tensile strength. The 13 refers to position and coating/current, not strength.

  6. Question 6Welding Fundamentals and Processes (Part A)

    What is the primary purpose of preheating a thick carbon steel joint before welding?

    1. To slow cooling and reduce cracking risk Correct answer.
    2. To increase the welding current capacity
    3. To increase the travel speed of the welder
    4. To remove the need for post-weld inspection

    Explanation

    Preheating raises base metal temperature so the weld cools more slowly, which lowers hardness and helps hydrogen escape, reducing cracking. It does not change equipment capacity or eliminate inspection.

  7. Question 7Welding Fundamentals and Processes (Part A)

    Slag inclusion in a multipass SMAW weld is most often caused by:

    1. Too small a root gap
    2. Failure to remove slag between passes Correct answer.
    3. Excessive travel speed on the root pass
    4. Using DC current rather than AC current

    Explanation

    Slag trapped between passes occurs when the slag from the previous bead is not fully chipped and brushed away. Current type and root gap do not directly cause slag entrapment.

  8. Question 8Welding Fundamentals and Processes (Part A)

    In brazing, the filler metal melts at a temperature:

    1. Exactly at the melting temperature of the base metal
    2. At any temperature below 450 degrees F
    3. Above the melting temperature of the base metal
    4. Below the base metal melting point but above 840 F Correct answer.

    Explanation

    Brazing uses a filler that melts above 840 F (450 C) but below the melting point of the base metal. Soldering occurs below 840 F, and welding melts the base metal.

  9. Question 9Welding Fundamentals and Processes (Part A)

    Which GMAW metal transfer mode is characterized by low heat input and is commonly used on thin sheet with small-diameter wire?

    1. Short-circuit transfer Correct answer.
    2. Pulsed spray transfer mode
    3. Globular transfer mode
    4. Spray transfer mode

    Explanation

    Short-circuiting transfer alternates short circuits and arc re-establishment at low current, giving low heat input suitable for thin material. Spray and pulsed spray require higher currents and are used on thicker sections.

  10. Question 10Welding Fundamentals and Processes (Part A)

    Why must SAW flux be kept dry and stored according to the manufacturer's recommendations?

    1. Wet flux increases deposition efficiency
    2. Dry flux conducts current better
    3. Moisture in flux can cause hydrogen cracking Correct answer.
    4. Wet flux changes the electrode classification

    Explanation

    Moisture in flux breaks down in the arc to hydrogen, which can produce porosity and hydrogen-assisted cracking in the weld. Flux condition does not change electrode classification.

  11. Question 11Welding Fundamentals and Processes (Part A)

    In the GTAW tungsten electrode designation EWTh-2, the 'Th' and '2' indicate:

    1. 2 percent thoria added to the tungsten Correct answer.
    2. Thoriated coating and 2 percent nickel
    3. Tungsten hardness grade 2
    4. 2 percent thorium and a 2-inch length

    Explanation

    EWTh-2 is a tungsten electrode containing approximately 2 percent thorium oxide (thoria), which improves electron emission and arc starting. The digits denote alloy content, not length or hardness.

  12. Question 12Welding Fundamentals and Processes (Part A)

    Self-shielded flux-cored arc welding differs from gas-shielded FCAW mainly because it:

    1. Relies on flux core protection, not external gas Correct answer.
    2. Uses a solid electrode wire instead of a tubular wire
    3. Requires a larger shielding gas flow rate
    4. Cannot be used in outdoor windy conditions

    Explanation

    Self-shielded FCAW generates its own protective atmosphere from the flux core, so no external shielding gas is supplied. Gas-shielded FCAW uses a separate shielding gas and is more sensitive to wind.

  13. Question 13Welding Fundamentals and Processes (Part A)

    Given 25 volts, 200 amps, and a travel speed of 10 in/min, what is the heat input in joules per inch?

    1. 3,000 J/in
    2. 50,000 J/in
    3. 30,000 J/in Correct answer.
    4. 500 J/in

    Explanation

    Heat input equals voltage times amperage times 60 divided by travel speed in inches per minute: (25 x 200 x 60) / 10 = 30,000 J/in. Omitting the 60 gives 500, and other values arise from arithmetic errors.

  14. Question 14Welding Fundamentals and Processes (Part A)

    Which condition is most likely to produce porosity in a GMAW weld?

    1. Using a slightly larger contact tip
    2. High travel speed with proper gas flow
    3. Welding with a clean, dry base metal
    4. Loss of shielding gas coverage at the pool Correct answer.

    Explanation

    Porosity results when gas is trapped in the solidifying weld, commonly from lost or disturbed shielding, drafts, or contaminated surfaces. Contact tip size and clean base metal do not introduce porosity.

  15. Question 15Welding Fundamentals and Processes (Part A)

    Which technique helps control angular distortion in a long butt weld?

    1. Increasing the root gap progressively
    2. Increasing the welding current to maximum
    3. Welding continuously from one end
    4. Using a balanced backstep sequence Correct answer.

    Explanation

    Backstep and balanced sequences distribute heat and shrinkage so distortion is offset or reduced. Continuous welding from one end concentrates shrinkage and worsens distortion.

  16. Question 16Welding Fundamentals and Processes (Part A)

    Using CE = C + Mn/6 + (Cr+Mo+V)/5 + (Ni+Cu)/15, a steel with C 0.20, Mn 1.20, and no other alloys has a carbon equivalent of about:

    1. 1.20
    2. 0.40 Correct answer.
    3. 0.20
    4. 0.24

    Explanation

    Only carbon and manganese contribute here: 0.20 + 1.20/6 = 0.20 + 0.20 = 0.40. Higher values would raise hardenability and cracking risk.

  17. Question 17Welding Fundamentals and Processes (Part A)

    As carbon content of plain carbon steel increases, weldability generally:

    1. Increases because the steel becomes softer
    2. Improves because preheat requirements drop
    3. Decreases as hardenability and cracking risk rise Correct answer.
    4. Remains unchanged up to 0.60 percent carbon content

    Explanation

    Higher carbon raises hardenability, so welds and heat-affected zones can form hard martensite and crack without preheat or controlled cooling. Weldability therefore decreases as carbon increases.

  18. Question 18Welding Fundamentals and Processes (Part A)

    For GTAW on carbon steel, direct current electrode negative (DCEN) is preferred because it:

    1. Allows the use of a smaller gas nozzle
    2. Prevents tungsten contamination
    3. Concentrates heat in the workpiece for penetration Correct answer.
    4. Cleans the oxide layer from the surface

    Explanation

    With DCEN, electrons flow from the tungsten to the work, depositing more heat in the workpiece and giving deeper penetration while limiting tungsten erosion. Oxide cleaning is characteristic of DCEP or AC.

  19. Question 19Welding Fundamentals and Processes (Part A)

    How should covered low-hydrogen electrodes such as E7018 be stored before use?

    1. In a freezer to prevent oxidation
    2. In a heated holding oven at elevated temperature Correct answer.
    3. In water to keep the coating pliable
    4. In an open rack at room temperature

    Explanation

    Low-hydrogen electrodes absorb moisture unless held in heated holding ovens, typically around 250 to 300 F, to keep the coating dry. Room storage allows moisture pickup and hydrogen cracking risk.

  20. Question 20Welding Fundamentals and Processes (Part A)

    What is the likely result of setting shielding gas flow too high in GMAW?

    1. Deeper penetration and improved sidewall fusion quality
    2. Reduced spatter and a smoother bead
    3. Lower gas consumption and cost
    4. Turbulence that draws in air and causes porosity Correct answer.

    Explanation

    Excessive flow creates turbulence that draws ambient air into the shielding envelope, leading to porosity and an unstable arc. Adequate but not excessive flow gives laminar coverage.

  21. Question 21Welding Fundamentals and Processes (Part A)

    Sensitization of austenitic stainless steel occurs when:

    1. Molybdenum is added to improve pitting resistance
    2. The steel is quenched rapidly from the annealing temperature
    3. Chromium carbides precipitate at grain boundaries Correct answer.
    4. Ferrite content exceeds 50 percent in the weld

    Explanation

    In the 800 to 1500 F range, carbon combines with chromium to form grain-boundary carbides, depleting adjacent metal of chromium and reducing corrosion resistance. Rapid cooling through that range or using low-carbon grades prevents it.

  22. Question 22Welding Fundamentals and Processes (Part A)

    Which combination is most appropriate for GTAW of aluminum?

    1. DCEN with helium shielding
    2. DCEP with carbon dioxide shielding
    3. DCEN with a thoriated tungsten electrode only
    4. AC with argon shielding and high-frequency start Correct answer.

    Explanation

    Alternating current alternates cleaning (DCEP) and penetration (DCEN) half-cycles, which suits aluminum's tenacious oxide, and argon is the standard shielding gas. CO2 is not used for GTAW and DCEN alone provides little oxide cleaning.

  23. Question 23Welding Fundamentals and Processes (Part A)

    The oxyfuel cutting process removes metal primarily by:

    1. Oxidizing the iron, then blowing away the oxide Correct answer.
    2. Mechanical blowing of molten metal by the oxygen jet
    3. Melting the metal with the preheat flame alone
    4. Vaporizing the metal at the kerf

    Explanation

    The preheat flame brings steel to ignition temperature, and the cutting oxygen stream oxidizes the iron; the high-velocity jet then removes the molten oxide and metal. Pure melting or vaporization is not the cutting mechanism.

  24. Question 24Welding Fundamentals and Processes (Part A)

    A welding procedure specification (WPS) is supported by a procedure qualification record (PQR) that documents:

    1. The visual inspection acceptance criteria
    2. Only the welder's certification test results
    3. The cost of consumables used on the project
    4. The variables used and test coupon results Correct answer.

    Explanation

    The PQR records the essential variables actually used to weld the qualification test coupon and the results of mechanical testing, and it supports the WPS. Welder performance is qualified separately.

  25. Question 25Welding Fundamentals and Processes (Part A)

    Residual stress in a weldment is primarily caused by:

    1. Excessive shielding gas flow during welding
    2. The presence of a backing strip
    3. Use of direct current instead of alternating current
    4. Restraint of contraction as the weld cools Correct answer.

    Explanation

    As weld metal and the heat-affected zone cool, thermal contraction is resisted by surrounding cooler, rigid material, generating internal stress. Gas flow and current type do not create the primary residual stress pattern.

  26. Question 26Welding Fundamentals and Processes (Part A)

    In shielded metal arc welding, the cellulosic coating on an E6010 electrode decomposes to produce a shielding atmosphere composed mainly of:

    1. carbon dioxide and hydrogen Correct answer.
    2. argon and helium
    3. nitrogen and chlorine
    4. pure oxygen

    Explanation

    Cellulose in the coating decomposes in the arc to form carbon monoxide and hydrogen, which create the shielding atmosphere. These gases also help stabilize the arc.

  27. Question 27Welding Fundamentals and Processes (Part A)

    Which shielding gas mixture is most commonly used for short-circuiting transfer GMAW on carbon steel?

    1. 100% argon
    2. 100% helium
    3. 75% argon and 25% carbon dioxide Correct answer.
    4. 50% argon and 50% oxygen

    Explanation

    A 75% argon/25% CO2 mixture is the common short-circuiting gas for carbon steel because it balances arc stability, spatter control, and penetration.

  28. Question 28Welding Fundamentals and Processes (Part A)

    A neutral oxyacetylene flame is used when welding steel because it:

    1. adds carbon to the weld
    2. produces an oxidizing slag
    3. removes carbon from the weld
    4. neither adds nor removes carbon Correct answer.

    Explanation

    A neutral flame has an approximately one-to-one oxygen-to-acetylene ratio, so it is neither carburizing nor oxidizing. This makes it suitable for welding steel without altering carbon content.

  29. Question 29Welding Fundamentals and Processes (Part A)

    In submerged arc welding, the welding arc is:

    1. struck in a vacuum chamber
    2. buried beneath a layer of granular flux Correct answer.
    3. visible above a shielding gas cloud
    4. used only with a nonconsumable electrode

    Explanation

    The SAW arc is covered by a layer of granular flux that melts to shield the arc and weld pool. The arc is not visible during normal operation.

  30. Question 30Welding Fundamentals and Processes (Part A)

    The main function of the flux in a flux-cored arc welding wire is to:

    1. cool the weld puddle rapidly
    2. form shielding gas and slag Correct answer.
    3. conduct current to the workpiece
    4. increase carbon in the weld

    Explanation

    The flux core decomposes in the arc to generate shielding gas and form a slag layer over the weld. The slag protects the solidifying metal from contamination.

  31. Question 31Welding Fundamentals and Processes (Part A)

    For GTAW of carbon steel with direct current electrode negative, the tungsten electrode is normally prepared with a:

    1. spherical balled tip
    2. wide chisel edge
    3. flat square end
    4. sharp pointed tip Correct answer.

    Explanation

    DCEN concentrates heat at the workpiece and allows a pointed tungsten tip to stabilize the arc. A pointed tip is standard for carbon steel GTAW with DCEN.

  32. Question 32Welding Fundamentals and Processes (Part A)

    Under AWS position designations, a groove weld made in the flat position is identified as:

    1. 4G
    2. 1G Correct answer.
    3. 3G
    4. 2G

    Explanation

    The AWS position number 1 designates flat, 2 designates horizontal, 3 designates vertical, and 4 designates overhead. Therefore, a flat groove weld is 1G.

  33. Question 33Welding Fundamentals and Processes (Part A)

    Which welding process is a solid-state process that joins materials without melting the base metal?

    1. submerged arc welding
    2. shielded metal arc welding
    3. gas metal arc welding
    4. friction stir welding Correct answer.

    Explanation

    Friction stir welding joins materials by stirring and forging them in a plasticized state below the melting point. The other listed processes are fusion welding processes.

  34. Question 34Welding Fundamentals and Processes (Part A)

    In the SMAW electrode classification E7018, the digit 1 indicates that the electrode:

    1. requires direct current electrode positive
    2. has a minimum tensile strength of 70,000 psi
    3. is designed only for flat position
    4. can be used in all welding positions Correct answer.

    Explanation

    In E7018, E means electrode, 70 is the minimum tensile strength in ksi, 1 means all positions, and 8 indicates a low-hydrogen coating with specific current requirements.

  35. Question 35Welding Fundamentals and Processes (Part A)

    In short-circuiting GMAW transfer, metal is transferred to the weld pool when the:

    1. the electrode touches the puddle Correct answer.
    2. arc sprays fine droplets across the gap
    3. shielding gas ionizes into a plasma jet
    4. wire retracts without touching the puddle

    Explanation

    In short-circuiting transfer, the electrode contacts the weld pool and the arc extinguishes briefly. The wire then pinches off a droplet and the arc restarts.

  36. Question 36Welding Fundamentals and Processes (Part A)

    If all other variables are held constant, increasing the travel speed in a welding operation will:

    1. increase heat input per inch
    2. double the deposition efficiency
    3. decrease heat input per inch Correct answer.
    4. have no effect on heat input

    Explanation

    Heat input per unit length is proportional to voltage times current divided by travel speed. Increasing travel speed spreads the same energy over more distance and lowers heat input per inch.

  37. Question 37Welding Fundamentals and Processes (Part A)

    When welding the root pass of austenitic stainless steel pipe, a backing or purge gas is used mainly to:

    1. reduce the need for interpass cleaning
    2. increase the travel speed
    3. add carbon to the weld metal
    4. prevent oxidation of the root Correct answer.

    Explanation

    Austenitic stainless steel root passes oxidize readily when oxygen is present. An inert purge excludes oxygen and prevents oxidation, often called sugaring, on the inside surface.

  38. Question 38Welding Fundamentals and Processes (Part A)

    Porosity in aluminum GMAW or GTAW welds is most commonly caused by:

    1. too little travel speed
    2. copper inclusions from the filler wire
    3. hydrogen dissolved in the weld pool Correct answer.
    4. excess argon in the shielding gas

    Explanation

    Aluminum readily absorbs hydrogen in the molten weld pool, and the hydrogen forms porosity as the metal solidifies. Cleanliness and proper shielding are critical to reducing hydrogen pickup.

  39. Question 39Welding Fundamentals and Processes (Part A)

    Backstep welding is used primarily to:

    1. reduce distortion Correct answer.
    2. eliminate the need for preheat
    3. produce a wider heat-affected zone
    4. increase penetration on thick plate

    Explanation

    Backstep welding makes short beads in a direction opposite the general progression so that shrinkage is distributed and balanced. This helps reduce distortion in long joints.

  40. Question 40Welding Fundamentals and Processes (Part A)

    Undercut in a completed weld is most often associated with:

    1. travel speed that is too slow
    2. excessive current or a long arc Correct answer.
    3. electrode angle of 90 degrees
    4. insufficient shielding gas flow

    Explanation

    Excessive current or an excessively long arc can gouge the base metal at the weld toes before the molten metal fills the groove. The result is a concave undercut along the weld edge.

  41. Question 41Welding Fundamentals and Processes (Part A)

    Hydrogen-induced cracking in high-strength steel welds is promoted by:

    1. low restraint and dry electrodes
    2. excess argon in the shielding gas
    3. high preheat and slow cooling
    4. moisture in the arc environment Correct answer.

    Explanation

    Hydrogen from moisture, dirt, or other sources can diffuse into the weld metal and cause cracking when the microstructure is hard and restraint is high. Dry electrodes and proper preheat help reduce this risk.

  42. Question 42Welding Fundamentals and Processes (Part A)

    The main advantage of pulsed GMAW compared with continuous GMAW is that it:

    1. can weld only in the flat position
    2. eliminates the need for any shielding gas
    3. requires no wire feed system
    4. gives better heat and spatter control Correct answer.

    Explanation

    Pulsed GMAW alternates between peak and background current to control droplet transfer. This provides better control of heat input and reduces spatter compared with continuous GMAW.

  43. Question 43Welding Fundamentals and Processes (Part A)

    In FCAW with constant voltage, increasing the wire feed speed while holding voltage constant generally:

    1. has no effect on current
    2. shortens the arc and raises current Correct answer.
    3. lengthens the arc and lowers current
    4. changes the shielding gas composition

    Explanation

    Higher wire feed speed increases burnoff and welding current, so the arc self-regulates to a shorter length. The voltage setting remains the primary control of arc length.

  44. Question 44Welding Fundamentals and Processes (Part A)

    A welding arc that is too long in SMAW most often produces:

    1. automatic arc blow correction
    2. a smoother bead with less spatter
    3. more spatter and less penetration Correct answer.
    4. deeper penetration and narrower bead

    Explanation

    A long arc spreads heat over a wider area and reduces penetration while increasing spatter and arc instability. Maintaining a short arc improves penetration and control.

  45. Question 45Welding Fundamentals and Processes (Part A)

    An oxyacetylene flame with a distinct feathery inner cone and excess acetylene is called a:

    1. cutting flame
    2. oxidizing flame
    3. carburizing flame Correct answer.
    4. neutral flame

    Explanation

    A carburizing flame has excess acetylene and shows a feathery secondary cone around the inner cone. It can add carbon to steel and is used for specific applications such as certain hardfacing alloys.

  46. Question 46Welding Fundamentals and Processes (Part A)

    In austenitic stainless steel, sigma phase is most likely to form after prolonged exposure to what temperature range?

    1. 1000°C to 1200°C (1830°F to 2190°F)
    2. Below 0°C (32°F)
    3. 150°C to 300°C (300°F to 570°F)
    4. 600°C to 900°C (1100°F to 1650°F) Correct answer.

    Explanation

    Sigma phase is a brittle intermetallic that forms in austenitic stainless steels during prolonged exposure to roughly 600°C to 900°C. It reduces toughness and corrosion resistance.

  47. Question 47Welding Fundamentals and Processes (Part A)

    Arc blow during DC welding is most commonly caused by:

    1. excessive travel speed
    2. insufficient shielding gas
    3. wrong electrode coating color
    4. magnetic forces around the arc Correct answer.

    Explanation

    Arc blow results from magnetic forces that deflect the arc, especially in DC welding of ferromagnetic materials or when the ground connection is poorly placed. Adjusting ground location and using short arcs can reduce it.

  48. Question 48Welding Fundamentals and Processes (Part A)

    In FCAW, increasing the electrode extension while keeping other variables constant will generally:

    1. have no effect on the weld
    2. increase current and penetration
    3. lower current and penetration Correct answer.
    4. change the flux composition

    Explanation

    A longer electrode extension increases resistance heating in the wire, which raises burnoff and lowers welding current. Lower current generally reduces penetration.

  49. Question 49Welding Fundamentals and Processes (Part A)

    In submerged arc welding, which polarity generally produces the deepest penetration?

    1. Alternating current
    2. Direct current electrode negative
    3. Direct current electrode positive Correct answer.
    4. Direct current with a pulsed arc

    Explanation

    DCEP concentrates more heat at the workpiece, which generally produces deeper penetration in SAW. DCEN concentrates heat at the electrode and gives higher deposition with less penetration.

  50. Question 50Welding Fundamentals and Processes (Part A)

    Lamellar tearing is most likely to occur in:

    1. thin sheet welded with low heat input
    2. rolled plate with through-thickness strain Correct answer.
    3. austenitic stainless steel with low restraint
    4. wrought aluminum with a clean surface

    Explanation

    Lamellar tearing occurs when nonmetallic inclusions in rolled plate align in planes parallel to the surface and the weld applies through-thickness strain. The inclusions separate and tear under that stress.

  51. Question 51Welding Fundamentals and Processes (Part A)

    Alternating current is used for gas tungsten arc welding of aluminum primarily because the electrode-positive half-cycle provides:

    1. deeper penetration than direct current electrode negative
    2. a narrower heat-affected zone than pulsed current
    3. oxide cleaning action on the aluminum surface Correct answer.
    4. automatic control of filler wire feed

    Explanation

    In AC GTAW, the electrode-positive portion of the cycle breaks up and removes the refractory aluminum oxide, while the electrode-negative portion limits heating of the tungsten. This cleaning action is the main reason AC is selected for aluminum.

  52. Question 52Welding Fundamentals and Processes (Part A)

    Brazing is defined as a joining process in which the filler metal melts at a temperature:

    1. at any temperature, provided a suitable flux is used
    2. exactly at the melting temperature of the base metal
    3. below 450 °C (840 °F), and the base metal is also melted during joining
    4. above 450 °C (840 °F) but below the base-metal melting point Correct answer.

    Explanation

    Brazing uses a filler that melts above 450 °C (840 °F) while the base metal remains solid; soldering uses a filler below that temperature. The base metal must not melt for either process.

  53. Question 53Welding Fundamentals and Processes (Part A)

    Slag inclusions in a multipass shielded metal arc weld are most effectively prevented by:

    1. increasing travel speed on each pass
    2. using a longer arc length
    3. using a larger diameter electrode
    4. cleaning slag between passes Correct answer.

    Explanation

    Slag trapped between passes causes inclusions, so each bead must be cleaned before the next is deposited. Long arcs and high travel speed can increase the chance of trapping slag rather than prevent it.

  54. Question 54Welding Fundamentals and Processes (Part A)

    An SMAW power source rated at 200 A with a 60 percent duty cycle can be operated at 200 A for:

    1. 2 minutes out of each 10-minute period
    2. 6 minutes out of each 10-minute period Correct answer.
    3. 10 minutes out of each 6-minute period
    4. 60 minutes continuously

    Explanation

    A 60 percent duty cycle means the power source can operate at rated current for 60 percent of a 10-minute period, or 6 minutes, followed by 4 minutes of cooling. This rating applies at the specified current.

  55. Question 55Welding Fundamentals and Processes (Part A)

    In oxyfuel gas cutting, the metal is severed mainly by:

    1. high-frequency electrical arcing
    2. mechanical shearing by the cutting tip
    3. melting the metal with the preheat flame alone
    4. oxidation of iron by the oxygen jet Correct answer.

    Explanation

    The preheat flame brings the steel to its ignition temperature, and the cutting oxygen jet then oxidizes the iron; the oxide slag is blown from the kerf. The preheat flame alone does not sever the metal.

  56. Question 56Welding Fundamentals and Processes (Part A)

    Spray transfer in gas metal arc welding is most readily achieved with:

    1. argon-rich gas and current above transition Correct answer.
    2. 100% CO2 shielding and low welding current
    3. short-circuiting current and a long electrode extension
    4. helium shielding and globular current

    Explanation

    Spray transfer requires an argon-rich gas and sufficient current to form a fine, axial droplet stream. CO2-rich gases and low currents tend to produce short-circuiting or globular transfer instead.

  57. Question 57Welding Fundamentals and Processes (Part A)

    In submerged arc welding, the granular flux covering the arc primarily serves to:

    1. provide mechanical support for the weld pool
    2. shield the arc and weld metal Correct answer.
    3. cool the electrode wire before it melts
    4. conduct welding current to the workpiece

    Explanation

    Granular flux melts to form a slag blanket that shields the arc and weld metal from air and helps stabilize the arc. It may also add alloying elements, but it is not the current path or a support.

  58. Question 58Welding Fundamentals and Processes (Part A)

    Self-shielded flux-cored arc welding differs from gas-shielded FCAW in that self-shielded FCAW:

    1. cannot be used outdoors
    2. relies on the flux core for arc shielding Correct answer.
    3. uses only direct current electrode negative
    4. requires a separate argon-helium gas mixture

    Explanation

    Self-shielded FCAW generates its own shielding from ingredients in the flux core, so no external shielding gas is supplied. This makes it more portable and wind resistant than gas-shielded FCAW.

  59. Question 59Welding Fundamentals and Processes (Part A)

    If voltage and travel speed are held constant, increasing welding current will:

    1. increase heat input and widen the bead Correct answer.
    2. decrease penetration while increasing travel speed
    3. decrease heat input and narrow the weld bead
    4. have no effect on heat input if voltage is constant

    Explanation

    Heat input is proportional to arc voltage times current divided by travel speed, so raising current at constant voltage and speed increases heat input. More heat usually produces a wider bead and greater penetration.

  60. Question 60Welding Fundamentals and Processes (Part A)

    The primary effect of preheating a thick carbon steel joint before welding is to:

    1. slow cooling and limit hard microstructures Correct answer.
    2. increase the carbon content of the weld metal
    3. increase the cooling rate after welding
    4. eliminate the need for a root gap or backing

    Explanation

    Preheating raises the base metal temperature so heat is conducted away more slowly after welding. This lowers the cooling rate, reducing the risk of hard martensite and hydrogen cracking in susceptible steels.

  61. Question 61Welding Fundamentals and Processes (Part A)

    Solidification cracking in carbon steel weld metal is most likely when the weld contains:

    1. high manganese with low carbon
    2. low sulfur and low phosphorus contents
    3. a fine equiaxed grain structure
    4. high sulfur, phosphorus, and restraint Correct answer.

    Explanation

    Sulfur and phosphorus segregate during solidification and can form low-melting films along grain boundaries, making the weld susceptible to cracking. High joint restraint increases the strain on those boundaries.

  62. Question 62Welding Fundamentals and Processes (Part A)

    Why is alternating current often chosen over direct current for shielded metal arc welding on large steel structures?

    1. It produces a more stable arc than direct current
    2. It reduces arc blow caused by magnetic effects Correct answer.
    3. It requires no electrode coating
    4. It gives deeper penetration than direct current electrode positive

    Explanation

    With AC the polarity reverses each half-cycle, which helps cancel the magnetic forces that deflect the arc. DC welding is more susceptible to arc blow, especially near heavy steel masses or poor ground connections.

  63. Question 63Welding Fundamentals and Processes (Part A)

    In resistance spot welding, the heat generated at the faying surface is proportional to:

    1. voltage divided by current
    2. current squared × resistance × time Correct answer.
    3. arc length times shielding gas flow
    4. electrode force times travel speed

    Explanation

    Resistance welding heat follows H = I²Rt, where I is current, R is resistance at the faying surface, and t is time. Current has the strongest effect because it is squared.

  64. Question 64Welding Fundamentals and Processes (Part A)

    Carbon equivalent formulas are used in welding primarily to estimate:

    1. the shielding gas flow rate required
    2. the travel speed for a given joint
    3. steel weldability and hardenability Correct answer.
    4. the electrode deposition efficiency

    Explanation

    Carbon equivalent combines carbon with other alloying elements to express their combined effect on hardenability. Higher CE generally means a steel is more crack-sensitive and may require preheat or higher heat input.

  65. Question 65Welding Fundamentals and Processes (Part A)

    Austenitic stainless steel becomes sensitized to intergranular corrosion after prolonged exposure to approximately:

    1. 800-1500 °F (427-816 °C) Correct answer.
    2. 400-800 °F (204-427 °C)
    3. 200-400 °F (93-204 °C)
    4. 1600-2000 °F (871-1093 °C)

    Explanation

    In the 800-1500 °F range, chromium carbides precipitate at grain boundaries and deplete the adjacent metal in chromium. That depleted zone becomes susceptible to intergranular corrosion.

  66. Question 66Welding Fundamentals and Processes (Part A)

    In gas metal arc welding, the transition current from globular to spray transfer depends primarily on:

    1. electrode force and backing type
    2. gas composition and wire diameter Correct answer.
    3. joint thickness only
    4. travel speed only

    Explanation

    The current at which globular transfer changes to spray transfer depends mainly on the shielding gas and the wire diameter and composition. Argon-rich mixtures and smaller wires lower the transition current.

  67. Question 67Practical Inspection and Nondestructive Examination (Part B)

    Which nondestructive examination method relies on capillary action to reveal surface-breaking discontinuities?

    1. Ultrasonic testing
    2. Radiographic testing
    3. Liquid penetrant testing Correct answer.
    4. Magnetic particle testing

    Explanation

    Liquid penetrant testing applies a low-surface-tension liquid that is drawn by capillary action into openings that break the surface, then blotted out by a developer. The method detects only discontinuities that are open to the examined surface.

  68. Question 68Practical Inspection and Nondestructive Examination (Part B)

    Magnetic particle examination can be applied directly to which of the following base metals?

    1. Aluminum alloy
    2. Titanium alloy
    3. Austenitic stainless steel
    4. Carbon steel Correct answer.

    Explanation

    Magnetic particle testing requires a ferromagnetic material that will support a substantial flux density and produce leakage fields at discontinuities. Carbon steel is ferromagnetic, so it can be magnetized and examined.

  69. Question 69Practical Inspection and Nondestructive Examination (Part B)

    A fillet weld gauge is used to measure which of the following?

    1. fillet weld leg size Correct answer.
    2. root gap and land
    3. the height of weld reinforcement
    4. undercut depth

    Explanation

    Fillet weld gauges are fitted against the weld face so that the legs of the gauge contact the plate and the weld toe, allowing the leg size (and, with the appropriate gauge, the throat) to be read. They are not designed for root gap, undercut, or cap height.

  70. Question 70Practical Inspection and Nondestructive Examination (Part B)

    An inspector's visual examination of a weld is normally performed at what point in the work?

    1. only when another examination method has failed
    2. before, during, and after welding Correct answer.
    3. only before the first pass is deposited
    4. only after the weld has been completed and cleaned

    Explanation

    Visual examination is the most-used method and is applied to fit-up and joint preparation, to each pass as it is deposited, and to the finished weld. Many conditions, such as poor fit-up, slag between passes, and insufficient cleaning, can only be caught if the weld is seen at those stages.

  71. Question 71Practical Inspection and Nondestructive Examination (Part B)

    Radiographic examination of welds uses which form of energy?

    1. High-voltage electric current
    2. Magnetic fields
    3. Infrared radiation
    4. X-rays or gamma rays Correct answer.

    Explanation

    Radiography passes penetrating X-rays (from a tube) or gamma rays (from a radioactive isotope) through the part and records differences in absorption on film or a digital detector. Density differences in the beam path produce contrast on the image.

  72. Question 72Practical Inspection and Nondestructive Examination (Part B)

    Ultrasonic examination detects internal discontinuities by interpreting changes in which of the following?

    1. high-frequency sound waves Correct answer.
    2. capillary action within a crack
    3. visible light reflected from the weld
    4. magnetic flux leakage at the surface

    Explanation

    Ultrasonic testing introduces high-frequency sound into the part and evaluates the reflected or transmitted energy. A discontinuity with a different acoustic impedance reflects part of the beam, giving an indication on the display.

  73. Question 73Practical Inspection and Nondestructive Examination (Part B)

    Before liquid penetrant or magnetic particle examination, the weld surface must be in what condition?

    1. heated to at least 400 F
    2. painted white for contrast
    3. clean and dry Correct answer.
    4. coated with a light oil for lubrication

    Explanation

    Penetrant must be able to enter surface openings and magnetic particles must be free to migrate to leakage fields, so the surface has to be clean, dry, and free of scale, slag, oil, and paint. Contaminants can also produce false indications.

  74. Question 74Practical Inspection and Nondestructive Examination (Part B)

    A hi-lo gauge is used to measure which of the following?

    1. fillet weld throat thickness
    2. weld reinforcement height
    3. root gap between abutting members
    4. internal pipe misalignment Correct answer.

    Explanation

    A hi-lo gauge measures the internal offset, or mismatch, between the bores of two abutting pipe ends. Excessive hi-lo creates a stress concentration and can also cause incomplete fusion at the root.

  75. Question 75Practical Inspection and Nondestructive Examination (Part B)

    In liquid penetrant testing, what is the function of the developer?

    1. It draws penetrant out of discontinuities onto a contrasting background Correct answer.
    2. It magnetizes the part so particles are attracted to the indication
    3. It raises the surface tension of the penetrant so it stays in the crack
    4. It removes excess surface penetrant by emulsification and rinsing

    Explanation

    Developer is a thin, uniform layer of powder or coating that blots penetrant back out of surface openings and provides a light background so the indication stands out. It is applied after excess penetrant has been removed and the surface dried.

  76. Question 76Practical Inspection and Nondestructive Examination (Part B)

    Which type of magnetization current is most effective for finding discontinuities located slightly below the surface?

    1. Alternating current at high amperage
    2. Direct or rectified current Correct answer.
    3. Alternating current
    4. A very short capacitor-discharge impulse

    Explanation

    Direct and rectified currents produce a magnetic field that extends below the surface, so they can reveal discontinuities that are not open to the surface. Alternating current concentrates its field at the surface.

  77. Question 77Practical Inspection and Nondestructive Examination (Part B)

    Before use, an AC electromagnetic yoke is checked by confirming that it will lift which of the following?

    1. 2 lb at minimum pole spacing
    2. 10 lb at maximum pole spacing Correct answer.
    3. 25 lb at minimum pole spacing
    4. 50 lb with the poles in contact

    Explanation

    A standard performance check is that the AC yoke lift at least 10 lb (4.5 kg) with the poles at their maximum spacing. This confirms adequate field strength for the examinations to follow.

  78. Question 78Practical Inspection and Nondestructive Examination (Part B)

    When fluorescent penetrant is used, the black light intensity at the examination surface should be at least which value?

    1. 1000 microwatts per square centimeter Correct answer.
    2. 120 microwatts per square centimeter
    3. 500 microwatts per square centimeter
    4. 300 microwatts per square centimeter

    Explanation

    The standard minimum for fluorescent penetrant examination is about 1000 microwatts per square centimeter measured at the surface being examined, with the light warmed up and the ambient white light kept low. Lower intensity can cause faint indications to be missed.

  79. Question 79Practical Inspection and Nondestructive Examination (Part B)

    The purpose of an image quality indicator on a radiograph is to do which of the following?

    1. verify the source-to-film distance used for the shot
    2. measure the optical density of the processed film in the weld area
    3. demonstrate the image quality of the technique Correct answer.
    4. establish the exposure time required for the source

    Explanation

    The image quality indicator, or penetrameter, is placed on the source side of the part so that its image shows whether the technique achieves the required sensitivity. If the required penetrameter hole or wire is not visible, the technique is unacceptable regardless of how the weld looks.

  80. Question 80Practical Inspection and Nondestructive Examination (Part B)

    Geometric unsharpness on a radiograph is reduced by which of the following changes?

    1. decreasing the source-to-film distance
    2. using a larger focal spot
    3. increasing the source-to-object distance Correct answer.
    4. using a faster film with larger grain

    Explanation

    Geometric unsharpness is proportional to focal spot size and object-to-film distance and inversely proportional to source-to-object distance. Moving the source farther from the part therefore sharpens the image.

  81. Question 81Practical Inspection and Nondestructive Examination (Part B)

    What is the purpose of a couplant in ultrasonic testing?

    1. increase the frequency of the transducer
    2. provide a contrasting background for the display
    3. clean the surface of the part before scanning
    4. couple sound from the transducer into the part Correct answer.

    Explanation

    An air gap between the transducer and the part reflects nearly all the sound, so a liquid or grease couplant is used to bridge the gap and transmit the beam. Coupling must be uniform, because varying couplant thickness changes signal amplitude.

  82. Question 82Practical Inspection and Nondestructive Examination (Part B)

    Which method is most effective for detecting fine surface-breaking cracks in a ferromagnetic weld?

    1. Wet fluorescent magnetic particle Correct answer.
    2. Ultrasonic testing
    3. Radiography
    4. Visual examination with a magnifier

    Explanation

    Wet fluorescent magnetic particle testing combines high particle mobility with fluorescent contrast, making it very sensitive to tight surface cracks in ferromagnetic material. The fine particles are drawn to the leakage field and fluoresce strongly under black light.

  83. Question 83Practical Inspection and Nondestructive Examination (Part B)

    After a liquid penetrant examination of a weld has been completed and accepted, what should be done with the part?

    1. re-examine the part with radiography
    2. leave the developer on the surface as a protective coating
    3. weld over the developer without further cleaning
    4. remove all penetrant and developer residues Correct answer.

    Explanation

    Penetrant and developer residues must be removed because they can hold moisture, mask later examinations, and contaminate subsequent welding. Cleaning also protects against corrosion of the part in service.

  84. Question 84Practical Inspection and Nondestructive Examination (Part B)

    In magnetic particle testing, particles build up at a discontinuity because of which of the following?

    1. capillary action draws the particles into the opening
    2. a flux leakage field forms at the discontinuity Correct answer.
    3. the part is heated above the Curie temperature
    4. the particles are electrostatically attracted to the metal

    Explanation

    When the part is magnetized, a discontinuity that interrupts the flux path causes flux to leak out at the surface. Particles are attracted to this leakage field and gather there, forming the visible indication.

  85. Question 85Practical Inspection and Nondestructive Examination (Part B)

    A penetrant indication appears at a location where the surface is roughened and mechanically torn, not at a true discontinuity. This is best described as which type of indication?

    1. a rounded indication
    2. a relevant indication
    3. a false indication Correct answer.
    4. a linear indication

    Explanation

    A false indication is produced by surface conditions such as roughness, machining marks, or smeared metal that trap penetrant and mimic a discontinuity. The inspector must recognize it and re-examine rather than evaluate it as a defect.

  86. Question 86Practical Inspection and Nondestructive Examination (Part B)

    Which method is most appropriate for detecting internal porosity in a thick aluminum weld?

    1. Visual examination
    2. Radiography Correct answer.
    3. Liquid penetrant testing
    4. Magnetic particle testing

    Explanation

    Porosity is a volumetric discontinuity located below the surface, which radiography can show as a change in absorption through the weld. Aluminum is also nonmagnetic, ruling out magnetic particle testing.

  87. Question 87Practical Inspection and Nondestructive Examination (Part B)

    In weld radiography, the film density in the area of interest is typically required to fall within which range?

    1. 0.5 to 1.0
    2. 4.5 to 6.0
    3. 1.0 to 1.5
    4. 1.8 to 4.0 Correct answer.

    Explanation

    Radiographs are normally required to have a density between about 1.8 and 4.0 in the weld area, with the exact minimum depending on the source used. Too low a density gives insufficient contrast; too high a density makes the image difficult to interpret.

  88. Question 88Practical Inspection and Nondestructive Examination (Part B)

    In the expression used to calculate geometric unsharpness, the symbol F represents which quantity?

    1. the thickness of the part
    2. the object-to-film distance
    3. effective focal spot size Correct answer.
    4. the source-to-film distance

    Explanation

    Geometric unsharpness equals F times t divided by D, where F is the effective focal spot size, t is the distance from the source side of the object to the film, and D is the source-to-object distance. Reducing F or t, or increasing D, sharpens the image.

  89. Question 89Practical Inspection and Nondestructive Examination (Part B)

    A part examined by magnetic particle testing must be demagnetized under which circumstance?

    1. when residual magnetism could cause arc blow Correct answer.
    2. when a dry powder method was used for the examination
    3. when the part is to be painted immediately after testing
    4. when the part will be stored outdoors before shipment

    Explanation

    Residual magnetism can deflect a welding arc, attract chips during machining, and interfere with instruments or later magnetic examinations. When such effects matter, the part is demagnetized after the test.

  90. Question 90Practical Inspection and Nondestructive Examination (Part B)

    What is the purpose of a distance-amplitude correction curve in ultrasonic testing?

    1. select the transducer frequency for the material
    2. correct for differences in echo amplitude with distance Correct answer.
    3. establish the couplant viscosity required for the examination
    4. calculate the geometric unsharpness of the setup

    Explanation

    Echo amplitude from the same size reflector falls as sound path length grows, so a reference curve is built from known reflectors at several depths. Indications at different depths can then be compared on a common basis and evaluated against the acceptance criteria.

  91. Question 91Practical Inspection and Nondestructive Examination (Part B)

    An inspector must find tight, planar lack of fusion in a 50 mm thick carbon steel groove weld. Which technique is best suited to this task?

    1. Angle-beam shear wave ultrasonics Correct answer.
    2. AC magnetic particle testing with a yoke
    3. Fluorescent penetrant after grinding the cap flush
    4. Gamma radiography with a small source

    Explanation

    Angle-beam shear waves can be directed across the weld so that a planar discontinuity oriented roughly perpendicular to the surface returns a strong echo, and the technique is not limited by section thickness. Tight lack of fusion produces little change in absorption, so radiography is unreliable for it.

  92. Question 92Practical Inspection and Nondestructive Examination (Part B)

    Which gauge is used to determine the height of weld reinforcement above the base metal surface?

    1. Fillet weld gauge
    2. Undercut gauge
    3. Root gap gauge
    4. Weld reinforcement gauge Correct answer.

    Explanation

    A reinforcement gauge measures the height of the weld cap above the adjacent base metal surface. Fillet gauges check fillet leg or throat size, undercut gauges measure undercut depth, and root gap gauges measure joint opening.

  93. Question 93Practical Inspection and Nondestructive Examination (Part B)

    A fillet weld gauge is primarily used to check which feature of a finished fillet weld?

    1. Groove angle
    2. Leg size Correct answer.
    3. Root opening
    4. Joint misalignment

    Explanation

    Fillet weld gauges compare the weld leg length, and often the throat dimension, with the specified fillet size. Groove angle and root opening are checked during joint preparation and fit-up, while misalignment is checked with straightedges or alignment gauges.

  94. Question 94Practical Inspection and Nondestructive Examination (Part B)

    Before welding starts, visual inspection of the joint should confirm that which of the following is within the welding procedure?

    1. Developer coat thickness
    2. Radiographic film density
    3. Final weld hardness
    4. Fit-up and cleanliness Correct answer.

    Explanation

    Pre-weld visual inspection verifies joint fit-up, root opening, bevel condition, and freedom from contaminants such as oil, rust, and moisture. Hardness and radiography are post-weld checks, and developer is used in penetrant testing.

  95. Question 95Practical Inspection and Nondestructive Examination (Part B)

    Which tool is commonly used to verify that a specified preheat temperature has been reached on a carbon steel joint?

    1. Magnetic yoke
    2. Black light
    3. Fillet weld gauge
    4. Temperature-indicating crayon Correct answer.

    Explanation

    Temperature-indicating crayons melt at a designated temperature and confirm when the part has reached the required preheat. Gauges measure geometry, black lights are used for fluorescent penetrant, and a yoke is used for magnetic particle testing.

  96. Question 96Practical Inspection and Nondestructive Examination (Part B)

    Wet magnetic particle testing uses particles that are suspended in which medium?

    1. An inert gas
    2. A dry developer powder
    3. A liquid vehicle Correct answer.
    4. Dry compressed air

    Explanation

    Wet magnetic particles are suspended in a liquid vehicle such as water or oil so they can flow over the part and migrate to leakage fields. Dry particles are applied by air dispersion rather than in a liquid suspension.

  97. Question 97Practical Inspection and Nondestructive Examination (Part B)

    In liquid penetrant testing, dwell time is the period during which the penetrant is:

    1. Mixed with developer before application
    2. Washed off under ultraviolet light
    3. Allowed to dwell on the surface Correct answer.
    4. Baked on to increase sensitivity

    Explanation

    Dwell time allows penetrant to seep into surface-breaking discontinuities before excess penetrant is removed. It is specified by the procedure and begins after penetrant application.

  98. Question 98Practical Inspection and Nondestructive Examination (Part B)

    An angle beam ultrasonic search unit introduces sound into a weld at an angle by using which component?

    1. Yoke
    2. Image quality indicator
    3. Couplant
    4. Wedge Correct answer.

    Explanation

    The wedge, or prism, refracts the ultrasonic wave into the test material at a chosen angle. Couplant transmits sound between the probe and part, a yoke is for magnetic particle testing, and image quality indicators are used in radiography.

  99. Question 99Practical Inspection and Nondestructive Examination (Part B)

    Radiographic film is loaded into cassettes in a darkroom primarily to prevent which condition?

    1. Light fogging Correct answer.
    2. Screen contact
    3. Static marks
    4. Backscatter

    Explanation

    Exposure of unprocessed film to white light causes fogging that reduces image contrast. Static marks come from handling, screen contact is intentional in cassette loading, and backscatter originates from scattered radiation.

  100. Question 100Practical Inspection and Nondestructive Examination (Part B)

    In magnetic particle testing, a surface crack is most readily detected when the magnetic flux lines are oriented how relative to the crack?

    1. At 30 degrees to the crack
    2. Parallel to the crack
    3. Perpendicular to the crack Correct answer.
    4. At 45 degrees to the crack

    Explanation

    Maximum leakage occurs when flux lines cross a discontinuity at right angles to its long axis. A field parallel to the crack produces little leakage and therefore a weak indication.

  101. Question 101Practical Inspection and Nondestructive Examination (Part B)

    What is the function of the emulsifier in post-emulsification penetrant testing?

    1. It increases the viscosity of the penetrant
    2. It develops the indication into a visible image
    3. It makes excess surface penetrant water-washable Correct answer.
    4. It makes the penetrant fluorescent

    Explanation

    In post-emulsification testing, an emulsifier is applied after the penetrant dwell so excess surface penetrant becomes removable by water. Fluorescence comes from dyes in the penetrant, and the developer forms the visible indication.

  102. Question 102Practical Inspection and Nondestructive Examination (Part B)

    An ultrasonic reference block is used during examination to provide which of the following?

    1. A magnetic field of known strength
    2. Known reflectors for calibration Correct answer.
    3. A source of ionizing radiation
    4. A controlled penetrant dwell time

    Explanation

    Reference blocks contain known geometric reflectors used to set the time base, sensitivity, and distance-amplitude corrections. They do not produce magnetic fields, radiation, or penetrant timing.

  103. Question 103Practical Inspection and Nondestructive Examination (Part B)

    If the image of a lead letter B appears on a radiograph, it indicates that which condition occurred?

    1. The film was underdeveloped
    2. The exposure time was too short
    3. The IQI was placed on the source side
    4. Backscatter radiation reached the film Correct answer.

    Explanation

    A lead letter B is placed on the back of the cassette; if its image appears, radiation scattered from behind the film has exposed the film. Additional lead shielding is then required.

  104. Question 104Practical Inspection and Nondestructive Examination (Part B)

    An undercut gauge is used to measure which weld feature?

    1. Leg size of a fillet weld
    2. Height of weld reinforcement
    3. Depth of undercut Correct answer.
    4. Root opening before welding

    Explanation

    An undercut gauge has a pointed reference that measures the depth of undercut relative to the base metal surface. Fillet leg, root opening, and reinforcement are measured with other gauges.

  105. Question 105Practical Inspection and Nondestructive Examination (Part B)

    When water-washable penetrant is used, excess penetrant should be removed in what manner?

    1. With a solvent-soaked rag only
    2. With a water spray while wet Correct answer.
    3. After the developer has dried completely
    4. By sanding until the color disappears

    Explanation

    Water-washable penetrant is removed with a controlled water rinse before it dries, so excess penetrant does not become difficult to remove. Over-washing must be avoided to prevent removal of penetrant from discontinuities.

  106. Question 106Practical Inspection and Nondestructive Examination (Part B)

    Before welding a thick steel plate, a straight beam ultrasonic examination is often performed to detect which condition?

    1. Surface-breaking cracks
    2. Lack of fusion in the root
    3. Porosity in the weld cap
    4. Laminations in the plate Correct answer.

    Explanation

    A straight beam scan through the plate thickness detects planar internal reflectors parallel to the surface, such as laminations. Weld discontinuities are examined after welding, usually with angle beam techniques.

  107. Question 107Practical Inspection and Nondestructive Examination (Part B)

    Dry magnetic particle testing is commonly selected for which situation?

    1. A part that must remain wet
    2. Very tight fatigue cracks
    3. A smooth machined surface with fine cracks
    4. A rough weld surface at elevated temperature Correct answer.

    Explanation

    Dry particles are well suited to rough surfaces and higher temperatures where wet suspensions may not be practical. Wet fluorescent methods generally provide better sensitivity for fine surface cracks.

  108. Question 108Practical Inspection and Nondestructive Examination (Part B)

    Film density on a radiograph is measured with which device?

    1. Black light meter
    2. Densitometer Correct answer.
    3. Gaussmeter
    4. Ultrasonic thickness gauge

    Explanation

    A densitometer measures the optical density of processed radiographic film. Black light meters are used for fluorescent penetrant, gaussmeters for magnetic fields, and thickness gauges for ultrasonic measurements.

  109. Question 109Practical Inspection and Nondestructive Examination (Part B)

    In solvent-removable penetrant testing, excess penetrant is removed by which sequence?

    1. Dry wipe first, then solvent-dampened wipe Correct answer.
    2. Apply developer before wiping
    3. Rinse with water, then apply solvent
    4. Spray solvent, then wipe with a dry cloth

    Explanation

    The initial dry wipe removes most excess penetrant; a solvent-dampened cloth then removes the remaining film without flushing penetrant from discontinuities. Direct solvent spray can wash out indications.

  110. Question 110Practical Inspection and Nondestructive Examination (Part B)

    In the continuous magnetic particle method, the particles are applied at what time?

    1. Before the magnetizing current is applied
    2. While the magnetizing current is flowing Correct answer.
    3. Only after demagnetization is complete
    4. After the part has cooled for one hour

    Explanation

    The continuous method applies particles while the magnetizing current is on, allowing particles to migrate to leakage fields during magnetization. The residual method applies particles after the current is removed.

  111. Question 111Practical Inspection and Nondestructive Examination (Part B)

    A developer is applied to a penetrant-tested surface in what condition?

    1. As a thin, uniform coating over a dried surface Correct answer.
    2. As a heavy, thick coat
    3. While the part is still flooded with water
    4. Before excess penetrant is removed

    Explanation

    Developer is applied as a thin uniform layer after excess penetrant removal and surface drying; it draws penetrant from discontinuities to form indications. A heavy coat can mask indications.

  112. Question 112Practical Inspection and Nondestructive Examination (Part B)

    On a radiograph, a series of small, rounded, dark indications aligned along the weld centerline most likely represents which condition?

    1. Undercut
    2. Lack of fusion
    3. Gas porosity Correct answer.
    4. Slag inclusions

    Explanation

    Gas porosity appears as rounded dark spots, often in groups or aligned along the weld. Slag is typically irregular and elongated, lack of fusion is linear, and undercut appears at the weld toe.

  113. Question 113Practical Inspection and Nondestructive Examination (Part B)

    Time-of-flight diffraction (TOFD) is particularly effective for which weld inspection task?

    1. Detecting and sizing planar discontinuities Correct answer.
    2. Measuring surface roughness
    3. Determining penetrant dwell time
    4. Verifying preheat temperature

    Explanation

    TOFD uses diffracted signals from crack tips to detect and size planar defects such as lack of fusion, with good through-thickness coverage. It does not measure temperature, roughness, or penetrant time.

  114. Question 114Practical Inspection and Nondestructive Examination (Part B)

    A phased array ultrasonic examination offers which advantage for weld inspection?

    1. It eliminates the need for a couplant
    2. It can steer the beam electronically Correct answer.
    3. It produces a radiograph of the weld
    4. It magnetizes the weld for particle testing

    Explanation

    Phased array probes use multiple elements with time delays to steer and focus the beam, allowing multiple angles and sectorial scans from one position. Couplant is still needed, and the method produces ultrasonic data rather than radiographs.

  115. Question 115Practical Inspection and Nondestructive Examination (Part B)

    Ultrasonic examination of thick austenitic stainless steel welds is difficult primarily because of which characteristic?

    1. Low melting temperature
    2. Coarse grain structure that scatters sound Correct answer.
    3. Strong radiation emission
    4. High magnetic permeability

    Explanation

    Coarse austenitic grains scatter and attenuate the ultrasonic beam, reducing signal-to-noise ratio. Special low-frequency, dual-element, or phased array techniques may be needed.

  116. Question 116Practical Inspection and Nondestructive Examination (Part B)

    For a single-V groove weld examined with angle beam ultrasonics, why should the weld be scanned from both sides where accessible?

    1. To detect defects with different orientations Correct answer.
    2. To check the magnetic field direction
    3. To measure the weld cap height
    4. To verify the couplant is dry

    Explanation

    A planar discontinuity gives a strong reflection when the beam strikes it near perpendicular; scanning from both sides improves detection of defects with different orientations. It is not related to couplant, cap height, or magnetic fields.

  117. Question 117Practical Inspection and Nondestructive Examination (Part B)

    A fillet weld gauge set is used primarily to measure which weld feature?

    1. Joint misalignment
    2. Root opening and groove angle
    3. Weld reinforcement height
    4. Leg and throat size Correct answer.

    Explanation

    Fillet weld gauges have blades shaped to fit against the weld face so the leg and throat dimensions can be compared with the specified size. They are dimensional tools for fillet profile, not for joint fit-up or alignment.

  118. Question 118Practical Inspection and Nondestructive Examination (Part B)

    When standard solvent-removable penetrants are used, the part surface temperature during examination should generally be kept within which range?

    1. 60 °C to 90 °C (140 °F to 195 °F)
    2. 0 °C to 10 °C (32 °F to 50 °F)
    3. 10 °C to 52 °C (50 °F to 125 °F) Correct answer.
    4. Any temperature above freezing

    Explanation

    Standard penetrant materials are formulated to perform within a moderate range of about 10 °C to 52 °C (50 °F to 125 °F). Below that range the penetrant becomes sluggish, and above it the penetrant may dry out or degrade, both of which change sensitivity.

  119. Question 119Practical Inspection and Nondestructive Examination (Part B)

    Magnetization by the prod method produces which magnetic field orientation in the part?

    1. A circular field around each prod Correct answer.
    2. No measurable field between the prods
    3. A field confined to the electrode contact points
    4. A longitudinal field parallel to the current path

    Explanation

    Current passing through the part between the prods creates a circular field around the path of current flow. Discontinuities lying roughly perpendicular to that circular field are the ones most strongly detected.

  120. Question 120Practical Inspection and Nondestructive Examination (Part B)

    What is the function of the couplant in ultrasonic examination?

    1. To transmit sound across the gap Correct answer.
    2. To cool the search unit during long examinations
    3. To protect the part from corrosion
    4. To clean the transducer face between scans

    Explanation

    A thin couplant layer displaces air between the search unit and the part so ultrasonic energy can pass into the material. Without it, the large acoustic impedance mismatch at an air gap reflects nearly all the sound.

  121. Question 121Practical Inspection and Nondestructive Examination (Part B)

    Which change will reduce geometric unsharpness on a radiograph?

    1. Increasing the source focal spot size
    2. Decreasing the source-to-film distance
    3. Increasing source-to-object distance Correct answer.
    4. Increasing the object-to-film distance

    Explanation

    Geometric unsharpness is proportional to focal spot size and object-to-film distance and inversely proportional to source-to-object distance. Moving the source farther from the object therefore sharpens the image edge.

  122. Question 122Practical Inspection and Nondestructive Examination (Part B)

    A hi-lo gauge is used to measure which condition in pipe welding?

    1. The pipe wall thickness at the bevel
    2. The weld cap height after welding
    3. The root gap before welding
    4. Internal misalignment of the bore Correct answer.

    Explanation

    The hi-lo gauge compares the inside surfaces of two pipe ends to quantify internal misalignment, often called hi-lo. Excessive mismatch must be corrected because it affects root quality and inspection.

  123. Question 123Practical Inspection and Nondestructive Examination (Part B)

    A vacuum box test is most commonly used to locate leaks in which location?

    1. Tank-bottom lap welds Correct answer.
    2. The weld metal of a completed butt joint
    3. A heat-affected zone
    4. Small pressure vessels

    Explanation

    A vacuum box is sealed over a lap weld and the space is evacuated while a soap solution is applied, so bubbles reveal through-leaks. This technique suits lap joints on tank bottoms and shells that cannot be pressurized.

  124. Question 124Practical Inspection and Nondestructive Examination (Part B)

    Before portable hardness testing on a weld, the surface must be prepared in which way?

    1. Left as-welded to preserve the original condition
    2. Heated to a dull red color
    3. Coated with a thin layer of oil
    4. Ground smooth and free of scale Correct answer.

    Explanation

    Portable hardness methods require a smooth, clean surface because the indenter or rebound device must contact sound metal. Scale, spatter, or roughness produce unreliable readings.

  125. Question 125Practical Inspection and Nondestructive Examination (Part B)

    Ferrite content is measured in austenitic stainless steel welds primarily to help prevent which problem?

    1. Solidification cracking Correct answer.
    2. Hydrogen blistering
    3. Lamellar tearing
    4. Excessive hardness

    Explanation

    A controlled amount of delta ferrite in the weld metal helps resist solidification, or hot, cracking. It also improves resistance to certain forms of corrosion, but excess ferrite can reduce toughness.

  126. Question 126Practical Inspection and Nondestructive Examination (Part B)

    Positive material identification (PMI) is performed on alloy piping primarily for which reason?

    1. To confirm the alloy matches the specification Correct answer.
    2. To detect subsurface cracks in the weld
    3. To measure the wall thickness of the pipe
    4. To verify postweld heat treatment was applied

    Explanation

    PMI uses techniques such as X-ray fluorescence or optical emission to determine alloy composition and confirm the installed material matches the specified grade. This guards against mix-ups of similar-looking alloys.

  127. Question 127Practical Inspection and Nondestructive Examination (Part B)

    An AC electromagnetic yoke used for magnetic particle testing should be capable of lifting at least how much weight at its maximum pole spacing?

    1. 10 lb (4.5 kg) Correct answer.
    2. 5 lb (2.3 kg)
    3. 1 lb (0.45 kg)
    4. 50 lb (23 kg)

    Explanation

    A properly functioning AC yoke must lift a 10 lb (4.5 kg) weight at its maximum rated pole spacing. This check confirms the yoke produces adequate flux density for the examination.

  128. Question 128Practical Inspection and Nondestructive Examination (Part B)

    Excessive washing during removal of a water-washable penetrant will most likely produce which result?

    1. A heavy fluorescent background
    2. Increased bleed-out from deep defects
    3. A false indication from the developer
    4. Missed shallow defects Correct answer.

    Explanation

    Penetrant trapped in shallow or tight discontinuities is easily flushed away if washing is prolonged. The result is reduced sensitivity and discontinuities that may go undetected.

  129. Question 129Practical Inspection and Nondestructive Examination (Part B)

    On a radiograph, a dark, straight line running along the toe of a weld and parallel to its edge most likely indicates which condition?

    1. Slag inclusion
    2. Undercut Correct answer.
    3. Lack of penetration
    4. Porosity

    Explanation

    Undercut appears as a dark line at the weld toe where base metal has been grooved away. Its straight, edge-following appearance helps distinguish it from rounded gas porosity or irregular slag.

  130. Question 130Practical Inspection and Nondestructive Examination (Part B)

    During fluorescent penetrant examination, the UV-A intensity at the part surface should be at least which value?

    1. 1,000 µW/cm² Correct answer.
    2. 20,000 µW/cm²
    3. 100 µW/cm²
    4. 5,000 µW/cm²

    Explanation

    Fluorescent penetrant inspection requires a minimum UV-A intensity of about 1,000 µW/cm² at the surface being examined. Adequate intensity, together with dark adaptation, is needed for reliable indication detection.

  131. Question 131Practical Inspection and Nondestructive Examination (Part B)

    Increasing the frequency of an ultrasonic search unit from 2.25 MHz to 5 MHz will produce which change?

    1. Greater penetration and lower resolution
    2. Better resolution and less penetration Correct answer.
    3. Better penetration and better resolution
    4. No change in resolution or penetration

    Explanation

    Higher frequency means a shorter wavelength, which improves resolution but increases attenuation, reducing penetration. Lower frequency behaves in the opposite way.

  132. Question 132Practical Inspection and Nondestructive Examination (Part B)

    A hydrostatic test on a completed pressure vessel is performed mainly to demonstrate which of the following?

    1. That the material hardness is acceptable
    2. That the vessel is leak-tight Correct answer.
    3. That the radiographs were properly exposed
    4. That the weld surfaces are clean

    Explanation

    A hydrostatic test pressurizes the vessel with water to demonstrate structural integrity and leak tightness. It complements, but does not replace, the NDE required by the construction code.

  133. Question 133Codes, Standards, and Acceptance Criteria (Part C)

    A visual inspection reveals a crack in a production fillet weld. Under AWS D1.1 acceptance criteria, the weld is:

    1. acceptable if the crack is shorter than 1/4 in.
    2. acceptable if the crack is peened closed before inspection
    3. rejectable regardless of the size or location of the crack Correct answer.
    4. acceptable if the crack is confined to the weld crater

    Explanation

    D1.1 visual acceptance criteria state that any crack, regardless of size or location, is a rejectable discontinuity. Cracks act as sharp stress raisers and can propagate under load. The defective weld metal must be removed and the joint rewelded.

  134. Question 134Codes, Standards, and Acceptance Criteria (Part C)

    A fillet weld shows overlap at the toe, where weld metal has rolled onto the base metal without fusing. The correct disposition is to:

    1. accept the weld after the welder blends the toe with a grinder
    2. reject the weld, because overlap is an unfused discontinuity that is not permitted Correct answer.
    3. accept the weld if the overlap is less than 1/16 in. wide
    4. accept the weld, because overlap does not reduce the throat

    Explanation

    Overlap is unfused weld metal lying on the base metal surface and creates a notch at the weld toe. D1.1 requires welds to be free of overlap, so the condition is rejectable. Grinding simply removes the evidence rather than repairing the lack of fusion.

  135. Question 135Codes, Standards, and Acceptance Criteria (Part C)

    Under AWS D1.1, the responsibility for performing the inspection of welds during fabrication and erection rests with:

    1. the engineer of record
    2. the owner's third-party inspector
    3. the filler metal manufacturer
    4. the contractor performing the fabrication and erection Correct answer.

    Explanation

    D1.1 assigns the duty of inspection to the contractor, who must provide the inspectors and the inspection program. The owner's representative verifies that the contractor's inspection is being performed. The engineer of record and the filler metal manufacturer have no inspection duty under the code.

  136. Question 136Codes, Standards, and Acceptance Criteria (Part C)

    Visual inspection of welded joints in accordance with AWS D1.1 shall be performed:

    1. before welding, during welding, and after welding Correct answer.
    2. only when specifically requested by the engineer
    3. only after the completed weld has cooled to ambient temperature
    4. only after the final pass has been completed

    Explanation

    D1.1 requires visual inspection at three stages: before welding to verify fit-up, joint preparation, and cleanliness; during welding to observe technique and interpass conditions; and after welding to judge the finished weld against the acceptance criteria. Inspecting only the finished weld misses conditions that can no longer be seen.

  137. Question 137Codes, Standards, and Acceptance Criteria (Part C)

    The minimum size of a fillet weld, as tabulated in AWS D1.1, is determined by:

    1. the tensile strength of the electrode used
    2. the thickness of the thicker part joined Correct answer.
    3. the overall length of the weld
    4. the thickness of the thinner part joined

    Explanation

    The D1.1 minimum fillet weld size table is keyed to the thickness of the thicker part joined, because that part controls how rapidly heat is extracted and therefore the risk of cracking and lack of fusion. The minimum size increases as the thicker part becomes thicker.

  138. Question 138Codes, Standards, and Acceptance Criteria (Part C)

    A 3/8 in. thick plate is joined with fillet welds and the joint is statically loaded. Undercut measured at the weld toe is acceptable up to a depth of:

    1. 1/32 in. Correct answer.
    2. 1/16 in.
    3. 1/8 in.
    4. 3/32 in.

    Explanation

    For statically loaded material less than 1 in. thick, D1.1 limits undercut to 1/32 in. in depth. The 1/16 in. limit applies only when the material is 1 in. or thicker. Undercut deeper than the applicable limit must be repaired.

  139. Question 139Codes, Standards, and Acceptance Criteria (Part C)

    Production welding under AWS D1.1 shall be performed in accordance with:

    1. a welding procedure specification qualified as required by the code Correct answer.
    2. verbal instructions from the engineer recorded in the daily report
    3. the individual welder's preferred technique
    4. the filler metal manufacturer's published data sheet

    Explanation

    D1.1 requires all production welding to follow a welding procedure specification that is either prequalified under Clause 3 or qualified by testing under Clause 4. Welding to an unqualified procedure is a code violation regardless of the welder's skill.

  140. Question 140Codes, Standards, and Acceptance Criteria (Part C)

    For statically loaded material 1 in. or thicker, the maximum permitted depth of undercut under AWS D1.1 is:

    1. 1/8 in.
    2. 3/32 in.
    3. 1/32 in.
    4. 1/16 in. Correct answer.

    Explanation

    D1.1 permits undercut up to 1/16 in. deep when the material is 1 in. thick or greater and the structure is statically loaded. The larger allowance reflects the greater section available to carry the load in heavy material. Anything deeper is rejectable.

  141. Question 141Codes, Standards, and Acceptance Criteria (Part C)

    The face reinforcement on a groove weld in plate shall not exceed:

    1. 3/16 in.
    2. 1/16 in.
    3. 1/4 in.
    4. 1/8 in. Correct answer.

    Explanation

    D1.1 visual acceptance criteria limit groove weld face reinforcement to 1/8 in. Excessive reinforcement creates a severe notch at the weld toe and does not increase the strength of the joint. Reinforcement above the limit must be removed.

  142. Question 142Codes, Standards, and Acceptance Criteria (Part C)

    A specified 5/16 in. fillet weld is measured and found to be undersized. Under D1.1 visual acceptance criteria, the maximum permitted undersize is:

    1. 1/8 in.
    2. 3/32 in.
    3. 1/32 in.
    4. 1/16 in. Correct answer.

    Explanation

    D1.1 permits fillet welds to be undersized by no more than 1/16 in., provided the weld still satisfies the minimum size requirement for the material thickness. A weld undersized by more than that amount is rejectable.

  143. Question 143Codes, Standards, and Acceptance Criteria (Part C)

    A 1/2 in. thick plate carries a fillet weld along its edge. Unless the drawings specify a larger size, the maximum permitted fillet weld size is:

    1. 1/4 in.
    2. 1/2 in.
    3. 3/8 in.
    4. 7/16 in. Correct answer.

    Explanation

    For material 1/4 in. and thicker, the maximum fillet weld size that may be deposited along an edge is the plate thickness minus 1/16 in., here 7/16 in. This prevents the arc from washing away the plate edge and leaving an undercut or melted edge.

  144. Question 144Codes, Standards, and Acceptance Criteria (Part C)

    When nondestructive testing of complete joint penetration groove welds is required by the contract, AWS D1.1 provides acceptance criteria for:

    1. radiographic and ultrasonic testing Correct answer.
    2. liquid penetrant testing only
    3. magnetic particle testing only
    4. visual inspection only

    Explanation

    D1.1 sets acceptance criteria for volumetric examination of groove welds by radiography and ultrasonography, in addition to the visual criteria that always apply. Magnetic particle and penetrant testing are surface methods and are used mainly to detect surface and near-surface discontinuities.

  145. Question 145Codes, Standards, and Acceptance Criteria (Part C)

    AWS D1.1 covers carbon and low-alloy steel structures in which the specified minimum yield strength does not exceed:

    1. 50 ksi
    2. 100 ksi Correct answer.
    3. 150 ksi
    4. 70 ksi

    Explanation

    The scope of D1.1 extends to steels with a specified minimum yield strength of 100 ksi or less. Steels with higher yield strengths fall outside the code and require other qualification and design provisions.

  146. Question 146Codes, Standards, and Acceptance Criteria (Part C)

    A 1/4 in. fillet weld is specified. Based on the D1.1 minimum length rule, the shortest acceptable weld length is:

    1. 2 in.
    2. 4 in.
    3. 1/2 in.
    4. 1 in. Correct answer.

    Explanation

    D1.1 requires that a fillet weld be at least four times its nominal size in length, so a 1/4 in. fillet must be at least 1 in. long. Shorter welds are not considered effective because the start and stop craters dominate the weld.

  147. Question 147Codes, Standards, and Acceptance Criteria (Part C)

    After a rejectable discontinuity has been removed and the joint rewelded, the repair shall be:

    1. examined by the same method and to the same acceptance criteria as the original weld Correct answer.
    2. accepted without further examination
    3. examined only if the owner's representative asks for it
    4. examined by radiography regardless of the original examination method

    Explanation

    D1.1 requires repaired welds to be re-examined using the same inspection method and acceptance criteria that applied to the original weld. A repair is not automatically acceptable simply because weld metal was added. The repair itself must also be made under a qualified WPS.

  148. Question 148Codes, Standards, and Acceptance Criteria (Part C)

    Visual inspection finds porosity open to the surface of a completed fillet weld. This condition is:

    1. acceptable if the joint is statically loaded
    2. acceptable if the pores cover less than 1% of the weld face
    3. unacceptable and requires repair Correct answer.
    4. acceptable if the individual pores are smaller than 1/16 in.

    Explanation

    Surface porosity is a rejectable discontinuity under D1.1 visual acceptance criteria; it reduces the effective throat and provides initiation sites for cracking. The affected weld metal must be removed and rewelded. No percentage or pore-size allowance appears in the visual criteria.

  149. Question 149Codes, Standards, and Acceptance Criteria (Part C)

    Under AWS D1.1, welding shall not be performed when the ambient temperature is below:

    1. 40 °F
    2. 0 °F Correct answer.
    3. 32 °F
    4. 70 °F

    Explanation

    D1.1 prohibits welding when the ambient temperature falls below 0 °F. At ambient temperatures between 0 °F and 32 °F, the base metal adjacent to the joint must be preheated to at least 70 °F and maintained at that temperature during welding.

  150. Question 150Codes, Standards, and Acceptance Criteria (Part C)

    Before the final visual inspection of a completed weld is performed, the weld and adjacent base metal shall be:

    1. left in the as-welded condition so the original profile is preserved
    2. wetted with a liquid penetrant to highlight surface cracks
    3. cleaned of slag and foreign matter so the weld surface is fully visible Correct answer.
    4. coated with a protective primer

    Explanation

    D1.1 requires welds to be cleaned before examination so that slag, spatter, and other foreign material do not hide discontinuities. An inspector cannot judge a weld profile that is obscured. Penetrant testing is a separate examination method, not a cleaning step.

  151. Question 151Codes, Standards, and Acceptance Criteria (Part C)

    A 45° fillet weld has equal legs measuring 3/8 in. Its effective throat is approximately:

    1. 3/8 in.
    2. 0.265 in. Correct answer.
    3. 3/16 in.
    4. 1/4 in.

    Explanation

    The effective throat of a 45° fillet weld with equal legs is 0.707 times the leg size, so 0.707 times 3/8 in. equals about 0.265 in. The effective throat, not the leg, is the dimension used in strength calculations.

  152. Question 152Codes, Standards, and Acceptance Criteria (Part C)

    The size of a completed fillet weld is normally verified in the field using:

    1. a fillet weld gauge Correct answer.
    2. a micrometer caliper
    3. a magnetic particle yoke
    4. a straight edge and feeler gauges

    Explanation

    A fillet weld gauge is designed with blades that compare the actual leg lengths and throat against the specified size. It is the standard field tool for checking fillet weld size and convexity. Micrometers, straight edges, and magnetic yokes do not measure fillet leg dimensions.

  153. Question 153Codes, Standards, and Acceptance Criteria (Part C)

    For a joint to be prequalified under AWS D1.1 without procedure qualification testing, which condition must be satisfied?

    1. The base metal and filler metal must be listed in the code's prequalified tables, and the joint detail and welding variables must fall within the prequalified limits Correct answer.
    2. The welder must hold a certification for the 6G position
    3. The welding procedure must have been qualified by destructive testing of a test coupon
    4. The engineer of record must approve the joint detail in writing before welding begins

    Explanation

    Prequalification is granted by the code when the base metal, filler metal, joint geometry, and essential variables all remain within the limits of Clause 3. Under those conditions no procedure qualification test is needed. Once any variable moves outside those limits, the procedure must be qualified by testing.

  154. Question 154Codes, Standards, and Acceptance Criteria (Part C)

    A fabricator is welding the shell of a carbon steel pressure vessel. The welding should conform to:

    1. AWS D1.1
    2. AWS D1.2
    3. ASME Boiler and Pressure Vessel Code, Section VIII Correct answer.
    4. AWS D1.3

    Explanation

    AWS D1.1 expressly excludes pressure vessels from its scope. Pressure vessels are governed by Section VIII of the ASME Boiler and Pressure Vessel Code, which contains its own welding, qualification, and examination requirements.

  155. Question 155Codes, Standards, and Acceptance Criteria (Part C)

    A fillet weld is to be made on 3/4 in. thick plate. The minimum fillet weld size permitted by AWS D1.1 is:

    1. 5/16 in.
    2. 3/16 in.
    3. 1/8 in.
    4. 1/4 in. Correct answer.

    Explanation

    The D1.1 minimum fillet size table assigns 1/4 in. to material over 1/2 in. through 3/4 in. thick. Sizes of 1/8 in. and 3/16 in. apply to thinner material, and 5/16 in. applies only above 3/4 in.

  156. Question 156Codes, Standards, and Acceptance Criteria (Part C)

    Radiography of a complete joint penetration groove weld shows incomplete fusion between the weld metal and the base metal. Under AWS D1.1 the weld is:

    1. acceptable after the area is ground and blended from the surface
    2. acceptable if the unfused area is shorter than 1 in.
    3. rejectable and must be repaired and re-examined Correct answer.
    4. acceptable if the joint is in a statically loaded member

    Explanation

    Incomplete fusion is a rejectable discontinuity because it directly reduces the load-carrying section and acts as a crack initiator. D1.1 radiographic acceptance criteria do not allow fusion defects at any length. The weld must be excavated, repaired under a qualified WPS, and re-examined.

  157. Question 157Codes, Standards, and Acceptance Criteria (Part C)

    Personnel performing ultrasonic examination of D1.1 welds shall be qualified in accordance with:

    1. AWS D1.1 Clause 4
    2. ASME Section IX
    3. AWS A5.1
    4. ASNT SNT-TC-1A Correct answer.

    Explanation

    D1.1 requires nondestructive testing personnel to be qualified under a recognized program such as ASNT SNT-TC-1A, with certification in the applicable method and level. Clause 4 governs welding procedure qualification, and ASME Section IX governs procedure and performance qualification for welding, not NDT personnel.

  158. Question 158Codes, Standards, and Acceptance Criteria (Part C)

    Carbon steel covered electrodes for shielded metal arc welding used under AWS D1.1 must conform to which AWS filler metal specification?

    1. AWS A5.14
    2. AWS A5.1 Correct answer.
    3. AWS A5.18
    4. AWS A5.20

    Explanation

    D1.1 requires filler metals to conform to the applicable AWS filler metal specification. Carbon steel covered electrodes for SMAW are covered by AWS A5.1. Solid wires and rods for GMAW are A5.18, flux cored electrodes are A5.20, and nickel-alloy electrodes are A5.14.

  159. Question 159Codes, Standards, and Acceptance Criteria (Part C)

    Between passes in a multi-pass weld, the welder must:

    1. Clean the weld only if the WPS lists cleaning as essential
    2. Leave the slag in place so the passes cool slowly
    3. Remove slag, scale, and spatter before the next pass Correct answer.
    4. Clean only the final pass, since only it is inspected

    Explanation

    D1.1 requires each pass to be cleaned of slag, scale, and spatter before the next pass is deposited. Cleaning before inspection is likewise required so that discontinuities are not hidden. Buried slag produces slag inclusions and lack of fusion.

  160. Question 160Codes, Standards, and Acceptance Criteria (Part C)

    Under AWS D1.1, welding shall not be performed when:

    1. Wind speed at the site exceeds 5 mph
    2. Ambient temperature is below 70 °F
    3. Relative humidity at the site exceeds 50%
    4. The base metal surface is wet from rain or snow Correct answer.

    Explanation

    Welding on wet surfaces, or where rain or snow is falling on the joint, is prohibited because hydrogen pickup and porosity result. The code also bars welding below 0 °F, but it does not set a 70 °F minimum, a humidity limit, or a fixed wind limit.

  161. Question 161Codes, Standards, and Acceptance Criteria (Part C)

    Craters at the end of a weld shall be:

    1. Ground out completely after welding is finished
    2. Left unfilled so residual stress can relieve
    3. Filled only when the weld will be radiographed
    4. Filled to the full cross section of the weld Correct answer.

    Explanation

    D1.1 requires craters to be filled to the full cross section of the weld. An unfilled crater is a shrinkage-stress concentration and a common origin of crater cracks. Filling the crater is required regardless of the NDT that will follow.

  162. Question 162Codes, Standards, and Acceptance Criteria (Part C)

    Visual inspection reveals a crack in a completed fillet weld. The proper disposition is:

    1. Accept the weld if the crack is shorter than 1/8 in.
    2. Accept the weld after the surface is ground flush
    3. Reject the weld, remove the crack, and rewelding the joint Correct answer.
    4. Accept the weld if the crack does not reach the root

    Explanation

    Cracks are unacceptable in any amount under D1.1; there is no size tolerance. The crack, plus any cracked metal, must be removed and the joint rewelded and reexamined. Grinding the crown flush does not eliminate a crack that extends below the surface.

  163. Question 163Codes, Standards, and Acceptance Criteria (Part C)

    Overlap at the toe of a completed fillet weld is:

    1. Acceptable if it does not exceed 1/16 in.
    2. Acceptable only in the flat welding position
    3. Rejectable and shall be removed Correct answer.
    4. Acceptable when the remainder of the weld is sound

    Explanation

    Overlap is a cold lap where weld metal rolled onto the base metal without fusing, so it acts as a notch. D1.1 visual criteria do not permit it, and it must be removed.

  164. Question 164Codes, Standards, and Acceptance Criteria (Part C)

    A welder who has passed a groove weld performance qualification test is also qualified to:

    1. Make only fillet welds, in any size
    2. Make fillet welds only in the flat position
    3. Make fillet welds within the qualified ranges Correct answer.
    4. Weld with any process the shop uses

    Explanation

    D1.1 provides that qualification on a groove weld test also qualifies the welder for fillet welds within the ranges established by that test. A fillet-only test, by contrast, does not qualify the welder for groove welds.

  165. Question 165Codes, Standards, and Acceptance Criteria (Part C)

    E7018 electrodes are designed primarily to be operated with:

    1. Direct current, electrode positive Correct answer.
    2. Direct current, electrode negative
    3. Direct current, electrode negative, or AC
    4. Alternating current at reduced amperage

    Explanation

    E7018 is a low-hydrogen, iron powder electrode intended primarily for DCEP operation, although many classifications also permit AC. DCEN is not a normal operating condition for this classification.

  166. Question 166Codes, Standards, and Acceptance Criteria (Part C)

    Low-hydrogen electrodes that are not in immediate use shall be stored:

    1. Immersed in oil to exclude moisture
    2. In unopened cartons on the shop floor
    3. In a holding oven held near 250 °F Correct answer.
    4. In a freezer to prevent oxidation

    Explanation

    D1.1 requires low-hydrogen electrodes to be kept in a holding oven maintained at approximately 250 °F (250 ± 25 °F) after the container is opened. This keeps the coating dry and limits hydrogen pickup. Electrodes that do pick up moisture must be redried per the manufacturer's instructions.

  167. Question 167Codes, Standards, and Acceptance Criteria (Part C)

    An arc strike made on base metal outside the weld joint shall be:

    1. Left in place if it is outside the heat-affected zone
    2. Covered with a small weld pass and dressed smooth
    3. Accepted if it is less than 1/16 in. deep
    4. Ground out and the area examined for cracks Correct answer.

    Explanation

    Arc strikes create hard, crack-susceptible zones and are not permitted on the finished work. D1.1 requires them to be removed, typically by grinding, and the area examined for cracking. Covering them with weld metal only buries the problem.

  168. Question 168Codes, Standards, and Acceptance Criteria (Part C)

    According to AWS D1.1, peening is:

    1. Required on every pass to control distortion
    2. Prohibited on the root pass and the final pass Correct answer.
    3. Permitted on all passes when the plate exceeds 1 in.
    4. Permitted only on the root pass

    Explanation

    Peening may be used to control distortion, but D1.1 prohibits it on the root pass and on the final pass. Peening the root can mask or initiate cracking, and peening the finished surface hides defects from inspection.

  169. Question 169Codes, Standards, and Acceptance Criteria (Part C)

    Which change to a qualified welding procedure requires requalification?

    1. Using a different lot of E7018 from the same maker
    2. Changing the electrode from E7018 to E6010 Correct answer.
    3. Switching brands of E7018 within the same classification
    4. Increasing preheat above the minimum in the WPS

    Explanation

    A change in filler metal classification is an essential variable because it changes the filler metal grouping, hydrogen level, and operating characteristics. Requalification is therefore required. Preheat increases above the minimum and brand or lot changes within the same classification are not essential.

  170. Question 170Codes, Standards, and Acceptance Criteria (Part C)

    Under AWS D1.1, the inspector is authorized to:

    1. Reject work that does not conform to the code Correct answer.
    2. Direct the welders and supervise their technique
    3. Waive contract NDT requirements for qualified welders
    4. Approve WPS changes in the field without the engineer

    Explanation

    The inspector acts for the owner and has the authority to reject work that does not comply with the code and contract documents. The inspector does not design, supervise the welding crew, or waive specified requirements.

  171. Question 171Codes, Standards, and Acceptance Criteria (Part C)

    Before welding the second side of a double-V groove weld, the first side shall be backgouged:

    1. Only when radiography is required
    2. Just enough to expose the root bead
    3. To sound metal Correct answer.
    4. To one-half the plate thickness

    Explanation

    Backgouging must continue until sound weld metal and base metal are reached so that the second side fuses into clean metal. Stopping at the visible root bead leaves slag or unfused metal at the joint root. The depth required is whatever sound metal dictates.

  172. Question 172Codes, Standards, and Acceptance Criteria (Part C)

    A procedure qualification bend specimen is unacceptable when the convex surface shows a discontinuity that:

    1. Shows on the concave side of the bend
    2. Appears anywhere on the bend
    3. Exceeds 1/8 in. in any direction Correct answer.
    4. Exceeds 1/16 in. in the weld metal

    Explanation

    D1.1 bend test acceptance allows no single discontinuity exceeding 1/8 in. measured in any direction on the convex surface of the bent specimen. Cracks that originate at the edges of the specimen are generally not cause for rejection.

  173. Question 173Codes, Standards, and Acceptance Criteria (Part C)

    Where members of different thickness are butt welded and a tapered transition is required, the transition shall not be steeper than:

    1. 1:2
    2. 1:1
    3. 1:2.5 Correct answer.
    4. 1:4

    Explanation

    D1.1 limits the slope of a transition between parts of unequal thickness to 1:2.5, roughly 22 degrees. A steeper transition creates a stress concentration at the weld toe, which is especially severe under cyclic loading. The taper is made in the thicker part.

  174. Question 174Codes, Standards, and Acceptance Criteria (Part C)

    The required quality of a radiograph is demonstrated by:

    1. Image quality indicators of the required sensitivity Correct answer.
    2. The film manufacturer's certificate of speed
    3. Densitometer readings taken at the weld root
    4. A step wedge placed on the base metal

    Explanation

    Radiographic image quality is verified with image quality indicators (penetrameters), and the required essential wire or hole must be visible. This demonstrates that the technique can reveal discontinuities of the required size. Densitometer readings confirm density only, not sensitivity.

  175. Question 175Codes, Standards, and Acceptance Criteria (Part C)

    Tack welds that will become part of the finished weld shall be:

    1. Removed only if they exceed 2 in. in length
    2. Made with any electrode the welder prefers
    3. Made by a qualified welder under a qualified WPS and cleaned Correct answer.
    4. Left heavily oxidized to improve penetration

    Explanation

    Tack welds that are incorporated into the final weld are production welds: they must be made by a qualified welder using a qualified WPS, and they must be cleaned before welding over them. Otherwise slag or unsound metal is buried in the joint.

  176. Question 176Codes, Standards, and Acceptance Criteria (Part C)

    Under AWS D1.1, the extent of visual inspection of production welds shall be:

    1. A random 10% sample of the welds
    2. Only welds scheduled for radiography
    3. The first 5 ft of each weld
    4. 100% of the weld length Correct answer.

    Explanation

    All production welds are to be visually inspected over their full length before the work is accepted. Visual inspection is the first and most basic acceptance gate and is not a sampling operation. Other NDT methods may then be applied in the extent specified.

  177. Question 177Codes, Standards, and Acceptance Criteria (Part C)

    The inspector confirms that structural base metals conform to the contract by:

    1. Checking the color coding of the painted surface
    2. Reviewing the welder qualification records
    3. Measuring the members with a fillet weld gauge
    4. Reviewing mill test reports and heat identification Correct answer.

    Explanation

    Conformance of base metal is verified from mill test reports together with the heat number or other identification on the material, supplemented by testing when documentation is missing. Welder records and dimensional gauges speak to other requirements.

  178. Question 178Codes, Standards, and Acceptance Criteria (Part C)

    Responsibility for selecting a welding sequence that minimizes distortion rests with:

    1. The inspector assigned to the project
    2. The fabricator, unless the contract says otherwise Correct answer.
    3. The engineer in every case
    4. The welding supply vendor

    Explanation

    Unless the contract documents prescribe a sequence, the fabricator selects the welding sequence and techniques that control distortion. The inspector verifies compliance with the documents but does not direct production methods.

  179. Question 179Codes, Standards, and Acceptance Criteria (Part C)

    For a member designated as fracture critical, AWS D1.1 requires:

    1. No requirements beyond non-critical work
    2. Ten percent sampling by magnetic particle
    3. CVN toughness testing and 100% NDT Correct answer.
    4. Visual inspection only

    Explanation

    Fracture critical members must use weld metal with demonstrated Charpy V-notch toughness, and their complete joint penetration groove welds are examined by ultrasonic or radiographic testing over the full length. The added toughness and volumetric examination address the consequence of a brittle failure.

  180. Question 180Codes, Standards, and Acceptance Criteria (Part C)

    Radiographic acceptance criteria for cyclically loaded structures, compared with statically loaded structures, are:

    1. Dependent only on welder qualification
    2. Less restrictive
    3. Identical in every respect
    4. More restrictive Correct answer.

    Explanation

    D1.1 provides separate acceptance limits, and the limits applied to cyclically loaded structures are tighter because small discontinuities can initiate fatigue cracks. Static loading tolerates somewhat larger indications. Welder qualification has no bearing on acceptance limits.

  181. Question 181Codes, Standards, and Acceptance Criteria (Part C)

    A welder passes a groove weld qualification test in the vertical (3G) position. The qualification covers:

    1. All positions, including overhead
    2. Vertical and overhead only
    3. The vertical position only
    4. Flat, horizontal, and vertical Correct answer.

    Explanation

    Qualification in the vertical position extends to the flat, horizontal, and vertical positions, but it does not cover overhead. Each position must otherwise be qualified separately.

  182. Question 182Codes, Standards, and Acceptance Criteria (Part C)

    Low-hydrogen electrodes that have absorbed moisture shall be:

    1. Dipped in water to restore the coating
    2. Dried in accordance with the manufacturer's instructions Correct answer.
    3. Used as-is when the coating looks intact
    4. Returned to the supplier for reclassification

    Explanation

    Electrodes exposed to moisture must be redried following the manufacturer's recommended baking time and temperature before use. Using them wet reintroduces the hydrogen that the low-hydrogen classification is meant to exclude. Coatings that are damaged or that cannot be restored are discarded.

  183. Question 183Codes, Standards, and Acceptance Criteria (Part C)

    In the electrode classification E70T-1, the letter T indicates that the electrode is:

    1. A tubular flux-cored electrode Correct answer.
    2. A tungsten-electrode classification
    3. A titania-coated covered electrode
    4. A tempered low-hydrogen electrode

    Explanation

    In the AWS filler metal classification system, E designates an electrode, the two digits give the minimum tensile strength in ksi, T identifies a tubular flux-cored electrode, and the suffix indicates usability and shielding.

  184. Question 184Codes, Standards, and Acceptance Criteria (Part C)

    In a welding symbol, the tail is used to:

    1. Cite a process specification or supplementary information Correct answer.
    2. Give the number of weld passes
    3. Show the weld length and pitch
    4. Specify the weld size

    Explanation

    The tail is the optional part at the far end of the reference line and is used to cite a process specification, procedure, or other reference information.

  185. Question 185Codes, Standards, and Acceptance Criteria (Part C)

    AWS D1.1 requires each welder to:

    1. Keep a personal log of every electrode used
    2. Apply a distinctive identification mark to the work Correct answer.
    3. Carry a personal copy of the WPS at all times
    4. Submit payment records for each weld

    Explanation

    AWS D1.1 requires each welder to apply a distinctive identification mark to the welds made so the inspector can trace the work to the qualified welder.

  186. Question 186Codes, Standards, and Acceptance Criteria (Part C)

    AWS D1.1 requires nondestructive testing personnel to be qualified in accordance with:

    1. AWS A5.20
    2. ASNT SNT-TC-1A or an equivalent standard Correct answer.
    3. OSHA 1910.147
    4. ASME Section IX

    Explanation

    AWS D1.1 requires NDT personnel to be qualified and certified in accordance with ASNT SNT-TC-1A or an equivalent nationally recognized program.

  187. Question 187Codes, Standards, and Acceptance Criteria (Part C)

    Before depositing the next weld pass, the welder shall:

    1. Remove slag from the previous pass Correct answer.
    2. Allow the slag to remain and cool
    3. Wire-brush only the final pass
    4. Paint the completed pass to protect it

    Explanation

    AWS D1.1 requires slag and other discontinuities to be removed from each weld pass before the next pass is deposited, and welds must be cleaned before inspection.

  188. Question 188Codes, Standards, and Acceptance Criteria (Part C)

    A fillet weld joins two plates that are each 1/2 in. thick. The minimum permitted fillet weld size is:

    1. 5/16 in.
    2. 1/8 in.
    3. 3/16 in. Correct answer.
    4. 1/4 in.

    Explanation

    AWS D1.1 sets minimum fillet weld sizes by the thickness of the thinner part joined. For thickness over 1/4 in. through 1/2 in., the minimum is 3/16 in.

  189. Question 189Codes, Standards, and Acceptance Criteria (Part C)

    The maximum size of a single-pass fillet weld is:

    1. 5/16 in. Correct answer.
    2. 1/4 in.
    3. 3/8 in.
    4. 1/2 in.

    Explanation

    AWS D1.1 limits a single-pass fillet weld to 5/16 in. leg size; larger fillet welds must be made with multiple passes.

  190. Question 190Codes, Standards, and Acceptance Criteria (Part C)

    The minimum length of a fillet weld shall be:

    1. Equal to the plate thickness
    2. One inch
    3. Four times the weld size Correct answer.
    4. Two times the weld size

    Explanation

    AWS D1.1 requires a fillet weld to be at least four times its nominal size in length before it is considered effective.

  191. Question 191Codes, Standards, and Acceptance Criteria (Part C)

    The minimum length of an intermittent fillet weld segment is:

    1. 2 in.
    2. 1-1/2 in. Correct answer.
    3. 1 in.
    4. 3 in.

    Explanation

    For intermittent fillet welds, AWS D1.1 requires each weld segment to be at least 1-1/2 in. long.

  192. Question 192Codes, Standards, and Acceptance Criteria (Part C)

    The size of a fillet weld is determined by the:

    1. Throat measured perpendicular to the root
    2. Leg of the largest inscribed right triangle Correct answer.
    3. Shortest leg of the weld
    4. Average of the two leg lengths

    Explanation

    Fillet weld size is defined by the leg of the largest right triangle that can be inscribed in the weld cross section, not by the throat or an average of the legs.

  193. Question 193Codes, Standards, and Acceptance Criteria (Part C)

    Before production welding begins, the inspector should confirm that:

    1. A current WPS is available at the work site Correct answer.
    2. The welder has purchased the electrodes
    3. The welding machine is new
    4. The base metal has been painted

    Explanation

    AWS D1.1 requires that a WPS be available at the point of use, and the inspector verifies this before production welding begins.

  194. Question 194Codes, Standards, and Acceptance Criteria (Part C)

    When the contract documents conflict with each other, the inspector should:

    1. Refer the conflict to the engineer for resolution Correct answer.
    2. Stop all work permanently
    3. Follow the drawings because they always govern
    4. Choose the least expensive requirement

    Explanation

    The contract documents govern the work, but when they conflict the inspector should not choose arbitrarily; the conflict is referred to the engineer for resolution.

  195. Question 195Codes, Standards, and Acceptance Criteria (Part C)

    A welder who is qualified under ASME Section IX is:

    1. Qualified only for fillet welds under D1.1
    2. Required to retake the ASME test
    3. Qualified for all AWS D1.1 work
    4. Not automatically qualified under AWS D1.1 Correct answer.

    Explanation

    Qualification under one code is not transferable to another. A welder must be qualified under AWS D1.1 to perform D1.1 work, even if qualified under ASME Section IX.

  196. Question 196Codes, Standards, and Acceptance Criteria (Part C)

    AWS D1.1 permits a WPS to be used without procedure qualification testing when:

    1. The welder has ten years of experience
    2. The base metal is unknown
    3. All prequalified joint requirements are met Correct answer.
    4. The joint is not covered by D1.1

    Explanation

    D1.1 allows prequalified WPSs to be used without procedure qualification testing only when the joint detail, base metal, filler metal, and other conditions meet the prequalified requirements of the code.

  197. Question 197Codes, Standards, and Acceptance Criteria (Part C)

    In procedure qualification testing, the groove weld tensile specimen shall:

    1. Be tested at 0 deg F
    2. Have a tensile strength not less than the base metal minimum Correct answer.
    3. Have an elongation of at least 50 percent
    4. Fail in the weld metal

    Explanation

    The groove weld tensile specimen must develop a tensile strength at least equal to the minimum specified tensile strength of the base metal; failure in the base metal is acceptable if that strength is reached.

  198. Question 198Codes, Standards, and Acceptance Criteria (Part C)

    AWS D1.1 requires welding inspectors to be qualified in accordance with:

    1. AWS A5.20
    2. OSHA 1910.147
    3. AWS QC1 or an equivalent program Correct answer.
    4. ASME Section IX

    Explanation

    D1.1 requires welding inspectors to be qualified under AWS QC1, the Certified Welding Inspector program, or an equivalent program acceptable to the engineer.

  199. Question 199Codes, Standards, and Acceptance Criteria (Part C)

    A weld rejected by nondestructive testing shall be repaired by:

    1. Peening the surface of the defect
    2. Adding a cover pass without removing the defect
    3. Painting over the rejected area
    4. Removing the defect, rewelding, and re-inspecting Correct answer.

    Explanation

    Rejected welds must have the defect removed, be repaired with a qualified WPS and qualified welder, and be re-inspected by the same method that revealed the defect.

  200. Question 200Codes, Standards, and Acceptance Criteria (Part C)

    The minimum fillet weld size determined from the code table need not exceed:

    1. 1/4 in. in all cases
    2. The length of the weld
    3. The thickness of the thicker part joined
    4. The thickness of the thinner part joined Correct answer.

    Explanation

    The minimum fillet weld size from the table need not exceed the thickness of the thinner part joined, because a fillet weld cannot be larger than that part.

CWI flashcards

32 cards. Read the term and the definition here. The deck at the top of this page is optional.

SMAW electrode E7018
Low-hydrogen, iron-powder covered electrode rated 70,000 psi minimum tensile strength, usable in all positions on AC or DC; the coating must be kept dry to prevent hydrogen-assisted cracking.
E6010 electrode characteristics
Cellulosic sodium-coated electrode producing a forceful arc and deep penetration; operates on DC electrode positive only and is widely used for root passes and pipe welding.
GMAW spray transfer
Requires high current and argon-rich shielding gas to produce a fine axial spray of droplets, giving high deposition and deep penetration; generally limited to flat and horizontal positions.
GTAW AC for aluminum
Alternating current alternates a cleaning half-cycle that breaks up the aluminum oxide film with a penetration half-cycle; used for aluminum and magnesium because the oxide must be removed.
Heat input formula
Heat input in joules per inch equals 60 multiplied by the arc voltage multiplied by the amperage, divided by the travel speed expressed in inches per minute.
Carbon equivalent purpose
An empirical number calculated from steel chemistry that estimates hardenability and weldability; higher values signal a greater need for preheat and hydrogen control.
FCAW self-shielded
Uses a flux-cored wire whose core supplies shielding and slag, so no external gas is needed; the process tolerates wind and is therefore common on outdoor field work.
SAW process features
Submerged arc welding buries the arc under a blanket of granular flux with a continuously fed wire, producing high deposition and deep penetration in flat or horizontal positions.
Fillet weld throat
The shortest distance from the joint root to the face of the fillet weld; for an equal-legged 45 degree fillet, the throat equals 0.707 times the leg.
Common groove weld types
Square, single-V, double-V, single-bevel, single-U and single-J grooves; the shape is chosen based on material thickness, joint access, and cost.
Welding position 3G
A groove weld made with the plates vertical and the weld axis vertical, progressing upward or downward; it is a standard skill test for all-position welders.
Visual inspection illumination
AWS D1.1 requires a minimum of 1000 lux, roughly 100 foot-candles, at the surface being examined, along with adequate access and unobstructed line of sight.
Penetrant testing limitation
Detects only discontinuities that are open to the surface of nonporous materials; subsurface flaws cannot be found, and the surface must be clean and dry.
Magnetic particle testing scope
Applies only to ferromagnetic materials and reveals surface and near-surface discontinuities; alternating current favors surface sensitivity while direct current reaches deeper.
Ultrasonic testing principle
High-frequency sound is transmitted into the part and echoes from reflectors are displayed; the method is best at planar flaws oriented perpendicular to the beam.
Radiographic testing principle
Radiation passes through the part and exposes film or a detector; differences in density reveal internal volumetric flaws, while planar flaws parallel to the beam may be missed.
Hi-lo gauge use
Measures internal misalignment of abutting pipe or plate surfaces; excessive high-low misalignment promotes lack of fusion and incomplete penetration at the root.
Fillet weld gauge
A gauge used to measure the leg size, and on some designs the throat, of a fillet weld so the measured size can be compared to the specified size.
Undercut gauge
A gauge with pointed or stepped blades that measures the depth of undercut at the weld toe so the reading can be compared against the code limit.
NDE personnel qualification
ASNT SNT-TC-1A is a recommended practice for employer-written qualification programs; Levels I, II and III define increasing responsibility, and the employer issues certification.
Discontinuity versus defect
A discontinuity is any interruption in the material; it is called a defect only after it exceeds the acceptance criteria of the applicable code.
Weld inspection stages
Inspection occurs before welding (materials, fit-up, procedure, qualifications), during welding (root pass, interpass), and after welding (final visual examination followed by NDE).
AWS D1.1 scope
Structural Welding Code - Steel; it covers design, procedure and personnel qualification, fabrication, and inspection of welded steel structures and is the most common CWI reference.
Prequalified WPS
A welding procedure that uses only joints and essential variables listed in AWS D1.1 Clause 3; it needs no mechanical testing but must still be written and followed.
WPS essential variable
A condition such as welding process, position, thickness range, filler metal classification, preheat, or current type whose change requires requalification of the welding procedure specification.
D1.1 butt weld reinforcement
Weld reinforcement on a butt joint shall not exceed 1/8 in (3 mm); reinforcement within that limit does not have to be removed.
D1.1 undercut limit
Undercut shall not exceed 1/32 in (1 mm) in depth; deeper undercut up to 1/16 in is permitted only in limited cumulative lengths within any 12 in.
Minimum fillet weld size
Based on thinner part thickness: up to 1/4 in requires 1/8 in; over 1/4 to 1/2 in requires 3/16 in; over 1/2 to 3/4 in requires 1/4 in.
Minimum fillet weld length
A fillet weld must be at least four times its nominal size in length; if it is shorter, the effective size is taken as the length divided by four.
ASME Section IX
Covers qualification of welding procedures, welders, and operators for ASME pressure equipment through the WPS, the PQR, and performance qualification; it is not a construction code.
API 1104 scope
Standard for welding pipelines and related facilities; it sets requirements for procedure and welder qualification and for acceptance of girth welds in transmission pipelines.
Inspector authority source
An inspector's authority comes from the contract documents and the referenced code, so each acceptance or rejection decision should cite a specific code clause or drawing requirement.

CWI study guide

Welding Fundamentals and Processes (Part A)

Process families you must be able to compare

SMAW (stick): covered electrode, slag shielding, wide alloy range, low deposition rate, tolerant of wind. FCAW: continuous tubular wire with a flux core; self-shielded (no external gas) versus gas-shielded (usually CO2). GMAW: solid wire plus external shielding gas, with transfer modes - short-circuit (low current, thin material), globular, spray (argon-rich mixtures, high current, flat and horizontal), and pulsed spray. SAW: arc buried under granular flux, highest deposition, mechanized, flat position. GTAW: non-consumable tungsten electrode, inert gas, precise, used for thin material and root passes.

Electrode classification

The digits are where candidates lose points. In E7018: E = electrode, 70 = 70,000 psi minimum tensile strength, 1 = usable in all positions, 8 = low-hydrogen coating with iron powder, usable on AC or DCEP. The third digit is position and the fourth is coating/current type; neither describes strength. ER70S-6: ER = electrode or rod for GMAW/GTAW, 70 = tensile, S = solid, 6 = chemistry (more deoxidizers than S-2).

Heat input and metallurgy

Heat input drives cooling rate, and cooling rate drives toughness and cracking risk:

HI (J/in) = (volts × amps × 60) ÷ travel speed (in/min)

Worked example: 25 V, 200 A, 8 in/min gives (25 × 200 × 60) ÷ 8 = 300,000 J/in, or 300 kJ/in - a hot, slow pass. Doubling travel speed halves heat input.

Preheat and interpass limits are essential variables. Preheat slows cooling on thick or high-carbon-equivalent steel; excessive interpass temperature can degrade toughness. Carbon equivalent (CE = C + Mn/6 + (Cr+Mo+V)/5 + (Ni+Cu)/15) flags steel that needs preheat before an arc is struck.

Practical Inspection and Nondestructive Examination (Part B)

Visual examination comes first

Visual inspection (VT) applies to essentially every weld and happens in three stages: before welding (joint preparation, fit-up, cleanliness, consumable condition), during welding (root condition, interpass cleaning, preheat/interpass checks), and after welding (final size, profile, and surface discontinuities). Typical tools: fillet weld gauge, undercut gauge, V-WAC-type gauge, taper gauge, magnifier, flashlight, mirror, borescope, tape, and straightedge.

Verify lighting rather than assuming it. A commonly cited minimum for weld inspection is about 100 foot-candles (roughly 1,000 lux) at the inspection surface, but the governing procedure controls; use a meter.

Choosing an NDE method

PT: surface-breaking discontinuities only, on nonporous materials; requires proper cleaning, dwell time, and developer. MT: surface and near-surface discontinuities, ferromagnetic materials only; AC magnetization is biased to the surface, DC reaches deeper. UT: volumetric and internal; angle-beam search units (45°, 60°, 70°) are used on welds; requires couplant and reference blocks; strong on planar defects such as lack of fusion. RT: volumetric; relies on density differences, so it reliably reveals porosity, slag, and inclusions but can miss tight planar defects oriented parallel to the beam; radiation safety controls the area.

Measurement rule of thumb

For a 90° fillet, theoretical throat = 0.707 × leg. A 1/4 in (6 mm) leg therefore gives about 0.177 in (4.5 mm) of throat.

Worked example: a gauge shows a 5/16 in leg with a visibly concave face. Record the leg and the profile; concavity reduces effective throat, so compare both against the WPS and acceptance criteria instead of accepting on leg alone.

Common traps: swapping PT and MT capabilities, treating RT as a universal detector, calling an indication a defect, and ignoring weld profile while measuring size.

Codes, Standards, and Acceptance Criteria (Part C)

Finding the governing requirement

Read the hierarchy before answering. Contract documents (drawings and specifications) normally govern where they conflict with the code, and the code governs where it conflicts with a referenced standard; always confirm the precedence clause in the edition you are testing against. A code sets minimum requirements - a specification may be stricter, and the stricter requirement then applies.

Prequalified versus qualified procedures

In AWS D1.1, Clause 3 lists prequalified joints: specified base metal groups, thickness ranges, groove details, processes, positions, and preheat conditions. If a WPS stays wholly inside those limits, no qualification testing is needed - but the WPS must still exist, be written, and be followed. If anything falls outside (process, thickness, joint detail, position, base metal), the WPS must be qualified by test under Clause 4 with a PQR supported by mechanical tests such as reduced-section tension, guided bends, and Charpy impact testing when required.

Essential variables

Process, filler metal classification (F-number and A-number), current type and polarity, position, preheat and interpass range, thickness range, joint detail, and significant technique changes. Change one outside its qualified range and the procedure is no longer supported.

Welder performance qualification is separate from procedure qualification: it records the individual welder's ability within position and thickness ranges, and continuity requirements must be tracked.

Acceptance criteria

Acceptance tables group requirements by category: cracks (rejected outright), fusion, crater fill, undercut, porosity, weld profile, weld size, and arc strikes. Criteria often differ for statically versus cyclically loaded structure, and much NDT is required only when the contract documents demand it - though the code itself mandates specific testing for certain applications.

Worked example: given a 3/8 in groove weld in a base metal outside the prequalified list, stop and require a qualified WPS rather than applying engineering judgment.

CWI cheat sheet

Quick reference

Welding Fundamentals and Processes (Part A)

  • AWS filler metal classification EXXYZ: E = electrode; first two digits = minimum tensile strength in ksi (E70 = 70,000 psi); third digit = position (1 = all positions, 2 = flat and horizontal); fourth digit = coating and current type.

  • E6010 is a cellulosic electrode that runs on DC electrode positive only and gives deep penetration; E7018 is low-hydrogen, runs on AC or DC, and must be held dry (typically 250-300 F holding oven).

  • Heat input (J/in) = 60 x volts x amps / travel speed (in/min). Increasing heat input slows the cooling rate and lowers hardness, but increases distortion and shrinks the HAZ toughness.

  • Carbon equivalent: CE = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15. Steels with CE above roughly 0.40 generally require preheat and hydrogen control to avoid delayed cracking.

  • GMAW transfer modes: short-circuiting for thin sheet and out-of-position work; globular is unstable and avoided; spray requires high current plus argon-rich shielding and is limited to flat and horizontal positions.

  • GTAW uses a non-consumable tungsten electrode with separately added filler. DCEN concentrates heat for deep penetration in steel; AC is used on aluminum because the electrode-positive half-cycle breaks up the oxide film.

  • SAW blankets a continuously fed wire under granular flux, giving high deposition and deep penetration; it is normally restricted to flat and horizontal positions because the flux must support the arc.

  • Fillet weld throat = 0.707 x leg for an equal-leg 45 degree fillet; effective throat, not leg or face width, governs the strength of the weld.

  • Distortion control methods include balanced (backstep) welding, presetting the parts, restricting heat input, welding from the center outward, and using fixtures or strongbacks.

Quick reference

Practical Inspection and Nondestructive Examination (Part B)

  • Inspection takes place in three stages: before welding (materials, fit-up, WPS, welder qualification), during welding (root pass, interpass cleaning), and after welding (final visual, then NDE).

  • AWS D1.1 requires a minimum illumination of 1000 lux (about 100 foot-candles) on the surface being examined, along with adequate access and line of sight for the inspector.

  • A discontinuity is any interruption in the material; it becomes a defect only when it exceeds the acceptance criteria of the governing code.

  • PT detects only surface-breaking discontinuities in nonporous materials. MT detects surface and near-surface discontinuities but works only on ferromagnetic materials (AC for surface sensitivity, DC for deeper flux fields).

  • UT is strongest on planar reflectors oriented perpendicular to the sound beam; RT is stronger on volumetric flaws but needs access from both sides and cannot reveal laminations parallel to the beam.

  • Common weld gauges: undercut gauge, V-WAC combination gauge, fillet leg gauge, bridge-cam gauge, taper gauge, and hi-lo gauge for internal misalignment of abutting members.

  • NDE personnel are qualified to ASNT SNT-TC-1A Level I, II, or III under the employer's written practice; certification is issued by the employer, not by ASNT.

  • Fillet weld size is measured by leg length, not face width; for an equal-leg 45 degree fillet the theoretical throat is 0.707 times the leg.

  • Visual discontinuities to identify: undercut, overlap, surface porosity, spatter, arc strikes, crater cracks, incomplete fusion or penetration, and joint misalignment.

Quick reference

Codes, Standards, and Acceptance Criteria (Part C)

  • AWS code family: D1.1 structural steel, D1.2 aluminum, D1.3 sheet steel, D1.5 steel bridges, D1.6 stainless steel, D9 aluminum structures.

  • A WPS is prequalified under D1.1 Clause 3 only when the joint detail and every essential variable fall inside the prequalified limits; otherwise the procedure must be qualified by test under Clause 4.

  • Essential variables include welding process, position, thickness range, filler metal classification, preheat, and current type; changing any one of them requires requalification of the WPS.

  • D1.1 acceptance limits: butt weld reinforcement shall not exceed 1/8 in (3 mm); undercut shall not exceed 1/32 in (1 mm) except for limited cumulative lengths where 1/16 in is permitted.

  • Minimum fillet weld size based on thickness of the thinner part: up to 1/4 in = 1/8 in; over 1/4 to 1/2 in = 3/16 in; over 1/2 to 3/4 in = 1/4 in; over 3/4 in = 5/16 in.

  • A fillet weld must be at least four times its nominal size in length; if shorter, the effective size is taken as the length divided by four.

  • ASME Section IX qualifies procedures and personnel for pressure equipment through the WPS, the PQR, and welder performance qualification; it is not a construction code.

  • API 1104 governs the welding of transmission pipelines and related facilities, including girth weld qualification and acceptance criteria.

  • The inspector's authority derives from the contract documents and the referenced code; every rejection or acceptance should cite the specific code clause or drawing requirement.

CWI key terms

Shielded Metal Arc Welding (SMAW)

An arc welding process in which a covered consumable electrode supplies both filler metal and shielding. The flux coating produces gas and slag that protect the molten weld, and slag must be chipped between passes.

Related: Electrode Classification (E7018), Heat Input
Gas Metal Arc Welding (GMAW)

An arc welding process using a continuous solid wire electrode fed through a gun, with shielding supplied by an external gas. It produces no slag and is common for production welding of steel, aluminum, and stainless.

Related: Polarity, Heat Input
Flux Cored Arc Welding (FCAW)

An arc welding process using a continuous tubular wire containing flux. The flux generates shielding gas and slag, and the process gives high deposition rates, especially in flat and horizontal positions.

Related: Electrode Classification (E7018), Heat Input
Gas Tungsten Arc Welding (GTAW)

An arc welding process using a nonconsumable tungsten electrode and a separately fed filler rod under inert gas shielding. It gives precise control and clean welds, especially on thin material and root passes.

Related: Polarity, Heat Input
Submerged Arc Welding (SAW)

An arc welding process in which the arc is struck beneath a layer of granular flux, hiding the arc from view. It is normally mechanized, uses high currents, and achieves high deposition on flat work.

Related: Heat Input, Distortion
Electrode Classification (E7018)

A standard designation system for covered electrodes. In E7018, E means electrode, 70 is minimum tensile strength in ksi, 1 is usable position, and 8 indicates a low-hydrogen coating and the current type.

Related: Shielded Metal Arc Welding (SMAW), Electrode Holding Oven
Polarity

The electrical relationship between electrode and workpiece in direct current welding. Electrode negative concentrates heat in the work for deeper penetration; electrode positive concentrates heat at the electrode and suits lighter gauge work.

Related: Gas Metal Arc Welding (GMAW), Arc Blow
Heat Input

The energy delivered per unit length of weld, calculated as amperage times voltage times sixty divided by travel speed. High heat input slows cooling, widens the heat-affected zone, and changes mechanical properties.

Related: Heat-Affected Zone (HAZ), Preheat
Preheat

Heating the base metal to a specified temperature before welding begins. Preheat slows cooling, helps remove moisture and hydrogen, and reduces the risk of cracking in thick or hardenable steel.

Related: Interpass Temperature, Carbon Equivalent
Interpass Temperature

The temperature of the weld and surrounding base metal just before the next pass is deposited. Codes set a maximum to control cooling rate and toughness, and sometimes a minimum to avoid cracking.

Related: Preheat, Heat Input
Carbon Equivalent

A calculated value combining the percentages of carbon and other alloying elements to indicate how readily a steel hardens. Higher values mean greater susceptibility to cracking and usually require preheat.

Related: Preheat, Heat-Affected Zone (HAZ)
Heat-Affected Zone (HAZ)

The base metal next to the weld that is not melted but is changed by welding heat. It can harden, soften, or grow grains, and it is often where cracks and failures begin.

Related: Heat Input, Carbon Equivalent
Arc Blow

Deflection of the welding arc away from the intended path by magnetic forces, common in direct current welding near joint ends or with poor ground placement. It causes spatter and incomplete fusion.

Related: Polarity, Shielded Metal Arc Welding (SMAW)
Effective Throat

The shortest distance from the root of a fillet weld to its face, excluding any convexity. It is the dimension used to calculate the design strength of the weld.

Related: Fillet Weld Gauge
Distortion

Unwanted change in the shape or dimensions of a welded assembly caused by uneven heating and shrinkage. It can be controlled by proper sequencing, balanced welding, restraint, and backstep techniques.

Related: Heat Input, Preheat
Visual Inspection (VT)

Examination of welds and components by eye, aided by lights, magnifiers, and gauges. It is performed before, during, and after welding and is the most widely used examination method.

Related: Fillet Weld Gauge, Discontinuity
Liquid Penetrant Testing (PT)

A surface examination method in which a liquid penetrant enters surface-breaking openings and is then drawn out by a developer for visual detection. It works on nonporous materials including aluminum and stainless steel.

Related: Indication, Discontinuity
Magnetic Particle Testing (MT)

A surface and near-surface examination method for ferromagnetic materials. Magnetizing the part causes particles to gather at discontinuities that interrupt the magnetic field, forming a visible indication.

Related: Indication, Discontinuity
Ultrasonic Testing (UT)

A volumetric examination method that sends high-frequency sound waves into the material and interprets reflected echoes. It detects internal flaws and measures thickness, and requires a trained operator and couplant.

Related: Couplant, Indication
Radiographic Testing (RT)

A volumetric examination method that passes X-rays or gamma rays through the weld onto film or a digital detector. Differences in density reveal internal discontinuities, and radiation safety controls are essential.

Related: Image Quality Indicator (IQI), Indication
Image Quality Indicator (IQI)

A small device, also called a penetrameter, placed on the part during radiography to show whether the exposure achieved the required sensitivity. Its image must meet the code before a radiograph is accepted.

Related: Radiographic Testing (RT)
Couplant

A substance such as oil, grease, or water applied between an ultrasonic transducer and the part surface. It removes the air gap so sound energy can pass into the material.

Related: Ultrasonic Testing (UT)
Fillet Weld Gauge

A hand tool with several blades used to check the leg size, throat thickness, and convexity or concavity of fillet welds. It gives an approximate field measurement rather than a precise dimension.

Related: Visual Inspection (VT), Effective Throat
Indication

A response from a nondestructive test that may or may not come from a real discontinuity. Indications must be evaluated against the acceptance criteria before being judged acceptable or rejected.

Related: Discontinuity, Acceptance Criteria
Discontinuity

An interruption in the normal structure of a weld or base metal, such as porosity, slag, or a crack. A discontinuity is not necessarily a defect; it becomes one only when it exceeds code limits.

Related: Indication, Acceptance Criteria
Material Test Report (MTR)

A document supplied by the material producer listing the chemical composition and mechanical properties of a heat or lot. Inspectors compare it with code and specification requirements before accepting material.

Related: Welding Procedure Specification (WPS)
Electrode Holding Oven

A heated cabinet that stores low-hydrogen electrodes at a controlled temperature after the original container is opened. Proper holding keeps the coating dry and helps prevent hydrogen cracking in the finished weld.

Related: Electrode Classification (E7018), Preheat
Welding Procedure Specification (WPS)

A written document giving the welding variables, materials, joint details, and ranges a welder must follow to produce welds meeting the code. It must be supported by a qualified procedure qualification record.

Related: Procedure Qualification Record (PQR), Essential Variable
Procedure Qualification Record (PQR)

A record of the actual welding and testing performed to qualify a welding procedure. It documents the variables used and the results of mechanical tests such as bend and tensile tests.

Related: Welding Procedure Specification (WPS), Essential Variable
Welder Performance Qualification (WPQ)

A test demonstrating a welder's ability to deposit sound welds to a given procedure and code. It is documented by a record and is usually limited in position, thickness, and process.

Related: Welding Procedure Specification (WPS), Essential Variable
Essential Variable

A welding condition in a procedure that, if changed beyond code limits, requires requalification. Examples include filler metal classification, preheat, current type, and base metal thickness or group.

Related: Procedure Qualification Record (PQR), Welding Procedure Specification (WPS)
Nonessential Variable

A welding condition that may be changed in a procedure without requalification but must still be updated on the WPS. Examples include travel speed, nozzle size, and some cleaning methods.

Related: Essential Variable, Welding Procedure Specification (WPS)
AWS D1.1

The American Welding Society structural welding code for steel. It covers design, qualification, fabrication, inspection, and acceptance criteria for statically and cyclically loaded steel structures.

Related: Acceptance Criteria, Welding Procedure Specification (WPS)
ASME Section IX

The section of the ASME Boiler and Pressure Vessel Code that governs qualification of welding procedures and welders. It sets essential variables and testing requirements but does not give acceptance criteria for production welds.

Related: Essential Variable, Welder Performance Qualification (WPQ)
API 1104

The American Petroleum Institute standard for welding pipelines and related facilities. It covers procedure and welder qualification, inspection, and acceptance criteria for transmission pipeline girth welds.

Related: Acceptance Criteria, Procedure Qualification Record (PQR)
Acceptance Criteria

The limits stated by the applicable code or specification that define whether a weld is acceptable. Inspectors compare measured indications and dimensions with these limits rather than with personal judgment.

Related: Discontinuity, Indication
Hold Point

A stage in fabrication where work may not continue until an authorized inspector has reviewed and approved it. Hold points are agreed in the inspection plan and enforced by the quality program.

Related: Visual Inspection (VT), Acceptance Criteria
Repair Rate

The percentage of welds or joints requiring repair compared with the number completed. Tracking repair rate shows trends in workmanship and can trigger retraining or additional examination.

Related: Acceptance Criteria, Discontinuity

CWI study plan

8 weeks · About 7 hours per week

Week 1

Welding Fundamentals and Processes (Part A) & Codes, Standards, and Acceptance Criteria (Part C)

  • Define the five primary arc welding processes (SMAW, GMAW, FCAW, SAW, GTAW) and list the essential variables that control each

  • Identify and sketch the five joint types and the standard weld types performed on each

  • Label weld cross-section terminology (root, face, toe, throat, leg, reinforcement) on hand-drawn diagrams

  • Decode AWS filler metal classification numbers for at least six common electrodes and rods

  • Build a tabbed index of the codebook by clause number and title

Your checkpoint

A one-page weld and joint terminology sheet with 10 labeled hand sketches, plus a self-quiz scored at 90% or better

Week 2

Welding Fundamentals and Processes (Part A) & Codes, Standards, and Acceptance Criteria (Part C)

  • Calculate heat input, amperage-travel speed relationships, and deposition rates for 10 parameter sets

  • Explain how preheat, interpass temperature, and cooling rate affect microstructure and cracking

  • Differentiate essential, supplementary essential, and nonessential variables on a WPS/PQR

  • Trace the qualification path from procedure qualification through welder performance qualification

  • Map the clause structure of the structural welding code so any topic can be located in under 60 seconds

Your checkpoint

A worked problem set of 10 heat-input and travel-speed calculations plus a one-page WPS/PQR variable checklist

Week 3

Welding Fundamentals and Processes (Part A) & Codes, Standards, and Acceptance Criteria (Part C)

  • Distinguish discontinuities from defects and explain why the distinction is acceptance-criteria dependent

  • Classify porosity, slag inclusion, incomplete fusion, incomplete penetration, and undercut by cause and morphology

  • Identify distortion types and select corrective and preventive techniques for each

  • Match base metal groups and filler metal selections for common structural steels

  • Explain the purpose and content of a WPS, PQR, and welder qualification record

Your checkpoint

A discontinuity cause-and-prevention table with at least 15 entries, each naming the process, cause, and control measure

Week 4

Practical Inspection and Nondestructive Examination (Part B)

  • Describe the inspector's responsibilities before, during, and after welding

  • Sequence a complete visual inspection from fit-up through final acceptance

  • Identify visual inspection tools (filters, magnifiers, undercut gauge, fillet weld gauge, HI-LO gauge) and state when each is used

  • Explain the physical principles, capabilities, and limitations of PT, MT, UT, and RT

  • Select an appropriate NDE method for a given discontinuity type and location

Your checkpoint

A mock visual inspection report covering five described weld scenarios, documenting observed conditions and required actions

Week 5

Practical Inspection and Nondestructive Examination (Part B)

  • Measure fillet weld leg, throat, convexity, and concavity using gauge readings and compute effective throat

  • Convert measured groove weld reinforcement and misalignment values into acceptance comparisons

  • Interpret welding symbols and NDE symbols on fabrication drawings

  • Explain weld mapping, joint tracking, and documentation of inspection hold points

  • Describe how surface condition and accessibility constrain NDE method selection

Your checkpoint

A 10-problem gauge-reading and weld-size calculation worksheet with a self-check answer key

Week 6

Practical Inspection and Nondestructive Examination (Part B) & Codes, Standards, and Acceptance Criteria (Part C)

  • Apply code acceptance criteria to 20 written discontinuity scenarios and issue accept or reject determinations

  • Cite the specific clause supporting each determination

  • Explain qualification and certification requirements for inspection personnel

  • Compare visual and volumetric NDE results and justify repair, retest, or acceptance decisions

  • Describe repair procedure requirements and re-inspection steps

Your checkpoint

A 20-scenario accept/reject log with a clause citation recorded for every decision

Week 7

Codes, Standards, and Acceptance Criteria (Part C) & Welding Fundamentals and Processes (Part A)

  • Tabulate the most frequently applied code clauses covering workmanship, fit-up, tolerances, and acceptance

  • Apply prequalified joint detail limits, including thickness and process ranges

  • Review welding symbol fundamentals and construct symbols for six given joints

  • Explain stud welding and tubular connection requirements at a familiarization level

  • Reconcile any conflicts between drawing notes, the WPS, and the governing code

Your checkpoint

A tabbed codebook with at least 40 marked and annotated clauses plus a completed six-item welding symbol worksheet

Week 8

Welding Fundamentals and Processes (Part A) & Practical Inspection and Nondestructive Examination (Part B) & Codes, Standards, and Acceptance Criteria (Part C)

  • Complete two full-length timed practice exams under exam-day conditions

  • Analyze every missed item and assign it to a domain and a root cause

  • Re-drill the three weakest subtopics until the error log is fully resolved

  • Assemble an exam-day checklist covering references, calculator, and time allocation

  • Verify that all three domains receive balanced final review

Your checkpoint

An error log with 100% of missed items resolved and two timed exams scored at 85% or higher

Milestones

Week 2: Score 80% or better on a self-made 30-question quiz covering process fundamentals and heat input calculations, and locate any named code clause within one minute

Week 4: Score 80% or better on a 40-question mixed quiz spanning fundamentals and code application, and submit a completed mock inspection report

Week 6: Achieve 17 of 20 correct accept/reject determinations with a correct clause citation on at least 15 of them

Week 8: Score 85% or higher on two separate full-length timed practice exams, with every missed item logged and re-worked to a correct answer

CWI exam day

Your checklist

Government-issued photo ID with signature

The name on the ID must match the name on your exam registration exactly. Bring the original; photocopies are not accepted. Confirm with the provider which ID forms are accepted if your ID is from another country.

Exam admission or confirmation letter/email

Printed or on paper (do not rely on your phone, since phones are typically not permitted in the testing room). Confirm with the provider whether a printed copy is required.

Silent non-programmable calculator

Bring one you already know how to use, plus spare batteries. Programmable, graphing, or wireless-capable calculators are usually prohibited. Confirm with the provider whether any calculator models are restricted.

Pencils, eraser, and pens

Several sharpened No. 2 pencils, a good eraser, and a pen for the practical recording section. Confirm with the provider whether scratch paper is supplied or prohibited.

Your own code book(s) for the open-book portion

Bring the exact code and edition specified for your exam (for example AWS D1.1, API 1104, or ASME Section IX as applicable). Confirm with the provider which edition is used before the exam date.

Practical inspection tools, if you must supply them

Typical kit: fillet weld gauge, undercut/V-WAC gauge, hi-lo gauge, weld reinforcement gauge, magnifier, flashlight, 6-inch rule, tape measure, dividers. Confirm with the provider exactly which tools are supplied at the station and which you must bring; do not assume.

Small tool pouch or container

Keeps gauges and scales together and easy to find under time pressure. Confirm with the provider whether containers must be clear or are subject to inspection.

Reading glasses or loupes if you use them

Fine measurement work on the practical portion is unforgiving; bring whatever magnification you normally use in the shop.

A non-smart watch

Useful for pacing the practical section. Confirm with the provider whether a clock is visible in the room and whether watches are permitted.

Travel, parking, and arrival plan

Know the testing location, parking or transit, and building/room number in advance. Plan to arrive well before the start time; late arrivals may be refused entry per provider policy.

Water and a snack for breaks

The exam is long and often runs through part of the day. Confirm with the provider what food and drink are allowed in the room and whether breaks are scheduled.

Nothing on this list: phones, smart watches, notes, or loose papers

Leave them in your vehicle or locker. Bringing prohibited items into the testing room can result in removal from the exam; confirm the provider's policy on secure storage.

Plan the day

72 hours before

Re-read the provider's candidate handbook and your admission letter end to end. Verify the test center address, reporting time, ID requirements, calculator policy, and which code editions and tools are permitted. Resolve any ambiguity by contacting the provider.

72 hours before

Confirm which exam parts you are sitting for and in what order (typically a fundamentals portion, a practical hands-on portion, and an open-book code portion). Adjust your preparation time to match.

72 hours before

Do a timed run-through of the practical measurements using your own gauges on scrap welds: fillet leg and throat, undercut, misalignment, reinforcement height, and pipe/plate dimensions. Practice recording each reading the same way every time.

72 hours before

Practice navigating your code book by index and table under time pressure. If you plan to tab or highlight, confirm with the provider what annotations are allowed in the testing room before you do it.

24 hours before

Pack the bag: ID, admission letter, calculator and spare batteries, pencils/eraser/pen, code book, tools, glasses, watch, snack. Check gauge zero points and that your scale markings are readable.

24 hours before

Light review only: formula sheet you write from memory, common definition and symbol recall, and the document structure of your code. Do not start new material the night before.

24 hours before

Set two alarms, lay out clothes, confirm the route and travel time, and get a full night of sleep. Fatigue costs more points on measurement questions than one more hour of study gains.

Morning of

Eat a real meal and hydrate. Arrive earlier than you think you need to; allow buffer for traffic, parking, and security screening.

Morning of

At the door: turn off and stow your phone, present your ID and admission letter, and listen carefully to the proctor's instructions on timing, breaks, and materials. Ask the proctor, not another candidate, if anything is unclear.

During the test

Work the closed-book portion first-pass on questions you know, flag the rest, and return to them. Watch the clock against the number of questions remaining rather than against your feelings.

During the test

On the practical portion, measure every dimension twice with the correct gauge, hold the gauge square to the surface, and write the reading immediately. Do not round or estimate unless the question directs you to.

During the test

On the open-book portion, use the code's table of contents and index rather than reading chapters. Verify the edition and the clause number before you commit to an answer.

During the test

Before each portion ends, confirm you have transferred every answer to the required format and that no question is blank; unanswered items cost the same as wrong ones.

Rules to check

  • Bring government-issued photo ID matching your registration name; you will likely be refused admission without it. If your documents are unusual (name change, foreign ID), confirm acceptability with the provider in advance.

  • Electronic devices, including phones, smart watches, and programmable calculators, are typically prohibited in the testing room. Confirm the provider's exact policy on calculators and secure storage before exam day.

  • The open-book privilege is usually limited to the code documents specified for the exam. Loose notes, sticky notes with writing, and unbound pages are commonly disallowed; confirm with the provider what tabs and highlighting are acceptable.

  • Breaks are generally at the proctor's discretion and may not stop the clock. Confirm with the provider whether scheduled breaks exist and whether exam time is paused.

  • Scoring is per part, and a candidate typically must meet the minimum score on each part of the exam rather than on the average. Confirm the current passing standard and retake policy with the provider, as these change.

  • Follow all proctor instructions on timing, materials, and conduct. Talking, sharing tools or references, or leaving the room without permission can result in invalidation of your exam.

  • Report any defective gauge, damaged specimen, or misprinted question to the proctor immediately rather than guessing; document the issue as instructed.

  • Use only your own materials at your own station. Sharing a code book, calculator, or gauges during the exam is generally treated as misconduct.

CWI FAQ

How many CWI practice questions are available?

The practice set has 200 CWI questions. Each one includes the choices, the correct answer, and an explanation, and the set is free to read with no signup.

How many CWI flashcards are available?

The flashcard set has 32 CWI cards. Each card shows the term and its definition.

Which topics does the CWI study material cover?

The CWI study material covers Welding Fundamentals and Processes (Part A), Practical Inspection and Nondestructive Examination (Part B), and Codes, Standards, and Acceptance Criteria (Part C).

What format facts does the catalog list for the CWI exam?